# US 2023/0243068 A1 · Method for forming silicon-phosphorous materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0243068 A1
- Document ID: US20230243068A1
- Status: Published application
- Kind: A1
- Application number: 18/131,255
- Filed: 2023-04-05
- Published: 2023-08-03
- Earliest claimed: 2019-06-20
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Errol Antonio C. SANCHEZ; Mark J. SALY; Schubert CHU; Abhishek DUBE; Srividya NATARAJAN
- Web page: https://patentgrep.com/patent/US20230243068A1

## CPC

- C30B 29/54: Organic compounds
- C01B 33/02: Silicon (forming single crystals or homogeneous polycrystalline material with defined structure C30B)
- C07F 9/06: without P—C bonds
- C07F 9/28: with one or more P—C bonds
- C07F 9/5009: {substituted by B, Si, P or a metal (C07F9/5027 takes precedence)}
- C30B 25/02: Epitaxial-layer growth
- H10D 62/149: {Source or drain regions of field-effect devices}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/3402: {characterised by the chemical composition}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3442: {N-type}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C07F: ACYCLIC, CARBOCYCLIC OR HETEROCYCLIC COMPOUNDS CONTAINING ELEMENTS OTHER THAN CARBON, HYDROGEN, HALOGEN, OXYGEN, NITROGEN, SULFUR, SELENIUM OR TELLURIUM (metal-containing porphyrins C07D487/22)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Embodiments generally relate to methods for depositing silicon-phosphorous materials, and more specifically, relate to using silicon-phosphorous compounds in vapor deposition processes (e.g., epitaxy, CVD, or ALD) to deposit silicon-phosphorous materials. In one or more embodiments, a method for forming a silicon-phosphorous material on a substrate is provided and includes exposing the substrate to a deposition gas containing one or more silicon-phosphorous compounds during a deposition process and depositing a film containing the silicon-phosphorous material on the substrate. The silicon-phosphorous compound has the chemical formula [(R3-vHvSi)—(R2-wHwSi)n]xPHyR′z, where each instance of R and each instance of R′ are independently an alkyl or a halogen, n is 0, 1, or 2; v is 0, 1, 2, or 3; w is 0, 1, or 2; x is 1, 2, or 3; y is 0, 1, or 2; z is 0, 1, or 2, and where x+y+z=3.

## Claims

### Claim 1

A method for forming a silicon-phosphorous material on a substrate, comprising:
exposing the substrate to a deposition gas comprising a silicon-phosphorous compound during a deposition process; and
depositing a film comprising the silicon-phosphorous material on the substrate,
wherein the silicon-phosphorous compound has the chemical formula:
(R3-vHvSi)xPHyR′z, and
wherein:
each instance of R is independently an alkyl or a halogen;
each instance of R′ is independently an alkyl or a halogen;
v is 0, 1, 2, or 3;
x is 1, 2, or 3;
y is 0, 1, or 2; and
z is 0, 1, or 2;
wherein x+y+z=3.

### Claim 2 (depends on 1)

The method of claim 1, wherein each instance of R and each instance of R′ are independently selected from the group consisting of methyl, ethyl, propyl, butyl, pentyl, fluoride, chloride, bromide, iodide, and an isomer thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein x is 3; y is 0; and z is 0.

### Claim 4 (depends on 3)

The method of claim 3, wherein each instance of R is independently selected from the group consisting of methyl, ethyl, propyl, butyl, and an isomer thereof.

### Claim 5 (depends on 4)

The method of claim 4, wherein v is 0.

### Claim 6 (depends on 4)

The method of claim 4, wherein v is 1.

### Claim 7 (depends on 4)

The method of claim 4, wherein v is 2.

### Claim 8 (depends on 3)

The method of claim 3, wherein v is 3.

### Claim 9 (depends on 3)

The method of claim 3, wherein each instance of R is methyl, and v is 1, 2, or 3.

### Claim 10 (depends on 3)

The method of claim 3, wherein each instance of R is butyl, and v is 1, 2, or 3.

### Claim 11 (depends on 1)

The method of claim 1, wherein the substrate is in a processing chamber during the deposition process, and wherein the silicon-phosphorous compound is produced in-situ the processing chamber prior to or during the deposition process.

### Claim 12 (depends on 1)

The method of claim 1, wherein the deposition gas further comprises one or more of a silicon source gas, a phosphorous source gas, an arsenic source gas, an antimony source gas, an etchant gas, a carrier gas, or any combination thereof.

### Claim 13 (depends on 12)

The method of claim 12, wherein:
the silicon source gas comprises silane, disilane, trisilane, tetrasilane, chlorosilane, dichlorosilane, trichlorosilane, tetrachlorosilane, hexachlorodisilane, tetraethyl orthosilicate (TEOS), or any combination thereof;
the phosphorous source gas comprises phosphine, trichlorophosphine, methylphosphine, ethylphosphine, propylphosphine, butylphosphine, dimethylphosphine, diethylphosphine, dipropylphosphine, dibutylphosphine, trimethylphosphine, triethylphosphine, tripropylphosphine, tributylphosphine, alkyl isomers thereof, adducts thereof, or any combination thereof;
the arsenic source gas comprises arsine, methylarsine, ethylarsine, propylarsine, butylarsine, dimethylarsine, diethylarsine, dipropylarsine, dibutylarsine, trimethylarsine, triethylarsine, tripropylarsine, tributylarsine, alkyl isomers thereof, adducts thereof, or any combination thereof;
the etchant gas comprises chlorine (Cl2), hydrogen chloride, an alkylchloride, or any combinations thereof; and
the carrier gas comprises hydrogen (H2), nitrogen (N2), forming gas, a mixture of hydrogen and nitrogen, argon, helium, or any combination thereof.

### Claim 14 (depends on 1)

The method of claim 1, wherein the deposition process is an epitaxial process, wherein the substrate is in a processing chamber during the epitaxial process, the substrate is heated to a temperature of about 400° C. to about 700° C. during the epitaxial process, and the processing chamber is maintained at a pressure of about 20 Torr to about 600 Torr during the epitaxial process.

### Claim 15 (depends on 1)

The method of claim 1, wherein the film comprising the silicon-phosphorous material is deposited on a feature disposed on the substrate, wherein the feature is a source-drain or a source-drain extension, and wherein the silicon-phosphorous material comprises a phosphorous concentration in a range from about 1×1020 atoms/cm3 to about 1×1022 atoms/cm 3.

### Claim 16

A method for forming a silicon-phosphorous material on a substrate, comprising:
exposing the substrate in a processing chamber to a deposition gas comprising a silicon-phosphorous compound during an epitaxial process; and
selectively depositing a film comprising the silicon-phosphorous material on the substrate,
wherein the substrate is heated to a temperature of about 400° C. to about 700° C.;
wherein the processing chamber is maintained at a pressure of about 20 Torr to about 600 Torr;
wherein the silicon-phosphorous compound has the chemical formula:
(R3-vHvSi)xPHyR′z, and
wherein:
each instance of R is independently an alkyl;
each instance of R′ is independently an alkyl;
v is 0, 1, 2, or 3;
x is 1, 2, or 3;
y is 0, 1, or 2; and
z is 0, 1, or 2;
wherein x+y+z=3.

### Claim 17

A method for forming a silicon-phosphorous material on a substrate, comprising:
exposing the substrate in a processing chamber to a deposition gas comprising a silicon-phosphorous compound during an epitaxial process; and
selectively depositing a film comprising the silicon-phosphorous material on the substrate,
wherein the silicon-phosphorous compound has the chemical formula:
(R3-vHvSi)3P, and
wherein:
each instance of R is independently selected from the group consisting of methyl, ethyl, propyl, butyl, and an isomer thereof;
v is 0, 1, 2, or 3.

### Claim 18 (depends on 17)

The method of claim 17, wherein v is 0.

### Claim 19 (depends on 17)

The method of claim 17, wherein each instance of R is methyl, and v is 1, 2, or 3.

### Claim 20 (depends on 17)

The method of claim 17, wherein each instance of R is butyl, and v is 1, 2, or 3.