# US 2023/0242806 A1 · Alkylaniline Polyether Benzenesulfonate and Process of Producing Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0242806 A1
- Document ID: US20230242806A1
- Status: Published application
- Kind: A1
- Application number: 18/003,395
- Filed: 2021-07-02
- Published: 2023-08-03
- Earliest claimed: 2020-07-02
- Assignees: Shanghai Research Institute of Petrochemical Technology, Sinopec
- Applicants: China Petroleum & Chemical Corporation
- Inventors: Yingcheng LI; Xinning BAO; Weidong ZHANG; Ou SHA; Xinyue WU; Jun JIN
- Web page: https://patentgrep.com/patent/US20230242806A1

## CPC

- C09K 8/584: characterised by the use of specific surfactants
- C08G 65/2627: {containing aromatic or arylaliphatic amine groups}
- C08G 65/326: containing sulfur
- C09K 8/035: Organic additives
- C09K 8/588: characterised by the use of specific polymers {(polymeric surfactants C09K8/584)}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

A process for the conversion of methanol to olefins includes the steps of passing a feedstock comprising methanol to a fluidized bed reactor in contact with a catalyst to produce an olefin product, wherein the process at least partially deactivates the catalyst to form an at least partially deactivated catalyst; and passing spent catalyst from said at least partially deactivated catalyst to a regenerator for regeneration thereby forming regenerated catalyst and returning activated catalyst from said regenerated catalyst to said reactor via a regenerated catalyst line. An oxygen volume content in the gas-phase component at the outlet of the regenerated catalyst pipeline is controlled to be less than 0.1 percent, preferably less than 0.05% and more preferably less than 0.01% on the regenerated catalyst pipeline.

## Claims

### Claim 1

An alkylaniline polyether benzenesulfonate, having a structure shown in a formula (I):
in formula (I):
R1 and R2 are independently selected from the group consisting of H, C1-C40 hydrocarbyl group or
and are not H at the same time;
R3 was independently selected at each occurrence from the group consisting of H, C1-C10 hydrocarbyl group, C1-C10 carbonyl group, C1-C10 alkylsulfonic group, C1-C10 alkylolsulfonic group, C1-C10 alkylcarboxylic group, and —SO3(M)n;
-(Polyoxyalkylene)1- is one or a combination of several of —(PO)x1—, -(EO)y1—, —(BO)z1—;
-(Polyoxyalkylene)2- is one or a combination of several of —(PO)x2—, -(EO)y2—, —(BO)z2—;
x1, x2, y1, y2, z1, and z2 are each independently selected from any integer between 0 and 50, and x1+x2=0-50, y1+y2=1-50, and z1+z2=0-50;
M is selected from alkali metals and alkaline earth metals, wherein n is 1 when M is an alkali metal, and n is 0.5 when M is an alkaline earth metal; and
wherein PO is propoxy, EO is ethoxy, and BO is butoxy.

### Claim 2 (depends on 1)

The alkylaniline polyether benzenesulfonate according to claim 1, characterized in that in formula (I), R1 is a C6-C30 hydrocarbyl group, preferably R1 is a C6-C30 alkyl or alkenyl group, R2 is H, a C1-C30 hydrocarbyl group or
R3 is independently at each occurrence H, —CH3, —CH2CH3, —CH2SO3(M)n, —CH2(CHOH)SO3(M)n, —CH2COO(M)n or —SO3(M)n, x1+x2=0-30, y1+y2=1-30, and z1+z2=0-30.

### Claim 3 (depends on 1)

The alkylaniline polyether benzenesulfonate according to claim 1, wherein in formula (I), R1 is a C6-C20 hydrocarbyl group, preferably R1 is a C6-C20 alkyl or alkenyl group; R2 is H or a C1-C30 hydrocarbyl group; R3 is independently selected at each occurrence from H, —CH3 and —CH2CH3; x1+x2=0-20, preferably x1+x2=1-10, or preferably x1+x2=2-10; y1+y2=1-20, preferably y1+y2=2-20; z1+z2=0-20, preferably z1+z2=1-10, or preferably z1+z2=2-10; M is selected from sodium ion, potassium ion, calcium ion and magnesium ion.

### Claim 4 (depends on 1)

The alkylaniline polyether benzenesulfonate according to claim 1, wherein in the formula (I), R1 or R2 is

### Claim 5 (depends on 1)

The alkylaniline polyether benzenesulfonate according to claim 1, wherein each occurrence of R3 is the same.

### Claim 6 (depends on 1)

The alkylaniline polyether benzenesulfonate according to claim 1, wherein R3 is —SO3(M)n, preferably each M occurring in the formula (I) is the same.

### Claim 7 (depends on 1)

A surfactant composition comprising one or more of the alkylaniline polyether benzenesulfonates according to claim 1.

### Claim 8 (depends on 1)

A process for producing the alkylaniline polyether benzenesulfonate according to claim 1, comprising the steps of:
Step 1, reacting alkylaniline serving as an initiator with an epoxy compound, and optionally performing blocking treatment on the reaction product by using a blocking agent, to obtain alkylaniline polyether;
Step 2, sulfonating the alkylaniline polyether by using a sulfonating reagent, to obtain the alkylaniline polyether benzenesulfonate.

### Claim 9 (depends on 8)

The process according to claim 8, characterized in that the alkylaniline is of the formula: R1-Ph-NH2, wherein Ph represents phenyl and R1 is selected from the group consisting of H, C1-C40 hydrocarbyl group or
and are not H at the same time.

### Claim 10 (depends on 8)

The process according to claim 8, characterized in that step 1′ and step 1″ are carried out before step 1:
Step 1′, taking alkylbenzene as a raw material, and carrying out nitration treatment to obtain alkyl nitrobenzene;
Step 1″, carrying out hydrotreatment on the alkyl nitrobenzene to obtain the alkylaniline.

### Claim 11 (depends on 10)

The process according to claim 10, characterized in that in step 1′, the alkylbenzene is nitrated with a nitrating agent and optionally an activator, wherein the nitrating agent is selected from nitric acid and dinitrogen pentoxide, and the activator is selected from concentrated sulfuric acid, glacial acetic acid, acetic anhydride, and phosphorus pentoxide.

### Claim 12 (depends on 11)

The process according to claim 11, characterized in that
the molar ratio of the nitrating reagent to alkylbenzene is (1-5):1, preferably (1-3):1; and/or
the nitration treatment of step 1′ is carried out at 0-80° C., preferably 20-65° C. for 1-10 hours, preferably 2-8 hours.

### Claim 13 (depends on 10)

The process according to claim 10, characterized in that in step 1″, the hydrotreatment is carried out in the presence of a hydrogenation catalyst selected from palladium on carbon and Raney nickel; and/or
the hydrogenation catalyst is used in an amount of 0.1-10 wt %, and preferably 1.0-5.0 wt %, relative to the alkyl nitrobenzene; and/or
the hydrotreatment described in step 1″ is carried out at 20 to 150° C., preferably 50 to 110° C., under 0 to 5 MPa, preferably 0.5 to 4 MPa.

### Claim 14 (depends on 8)

The process according to claim 8, characterized in that
in step 1, the epoxy compound is selected from C2-C6 epoxy compounds, preferably from propylene oxide and ethylene oxide; and/or
in step 1, the molar ratio of the epoxy compound to the alkylaniline is (1-150):1, preferably (1-90):1, more preferably (1-60):1, and even more preferably (1-40):1 or (2-40):1; and/or
step 1 is carried out in the presence of a basic catalyst; preferably, the basic catalyst is selected from the group consisting of alkali metals, alkali metal hydroxides, alkaline earth metal hydroxides, alkali metal alcoholates and alkali metal oxides; more preferably, the basic catalyst is used in an amount of 0.1 wt % to 10 wt %, preferably 0.5 wt % to 5.0 wt % of the total weight of the reactants; and
in step 1, the reaction conditions comprise: a reaction temperature of 140-200° C., and a reaction pressure of 0-5 MPa.

### Claim 15 (depends on 8)

The process according to claim 8, characterized in that in step 1, the blocking agent is selected from R′3—X or R″3—X′—R″3, wherein R′3 is a C1-C10 hydrocarbyl group or C1-C10 carbonyl group, X is selected from halogens or hydroxyl, for which when X is hydroxyl, R′3 is a C1-C10 carbonyl group; R″3 is selected from C1-C10 carbonyls and X′ is selected from 0; preferably the halogen is F, Cl or Br, R′3 is a C1-C10 alkyl, alkenyl or phenylalkyl group; more preferably, the blocking agent is selected from methyl iodide, ethyl iodide, propyl iodide, vinyl iodide, toluene iodide, acetic acid, acetic anhydride, acetyl chloride, benzoyl chloride; and the molar ratio of the blocking agent to the alkylaniline is preferably (2-2.6):1, and preferably (2.04-2.4):1.

### Claim 16 (depends on 8)

The process according to claim 8, characterized in that
the sulfonating agent is selected from concentrated sulfuric acid, fuming sulfuric acid and sulfur trioxide.

### Claim 17 (depends on 8)

The process according to claim 8, characterized in that step 2 comprises the sub-steps of:
Step 2-1, mixing the alkylaniline polyether with a sulfonating agent, and carrying out sulfonation reaction at 20-80° C. for 0.5-10 hours;
Step 2-2, adjusting the pH value to 10-14, and performing hydrolysis reaction for 0.5-5 hours, to obtain the alkylaniline polyether benzenesulfonate.

### Claim 18 (depends on 1)

An enhanced oil recovery agent composition, comprising the alkylaniline polyether benzenesulfonate according to claim 1 as a surfactant and water, wherein the weight ratio of the surfactant to the water is 1:(50-2000), preferably 1:(80-500).