# US 2023/0235475 A1 · Systems, devices, and methods for electroplated zinc negative electrodes for zinc metal cells and batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0235475 A1
- Document ID: US20230235475A1
- Status: Published application
- Kind: A1
- Application number: 18/168,104
- Filed: 2023-02-13
- Published: 2023-07-27
- Earliest claimed: 2018-11-06
- Assignees: Salient Energy Inc.
- Applicants: Salient Energy Inc.
- Inventors: Brian D. Adams; Marine B. Cuisinier; John Philip S. Lee
- Web page: https://patentgrep.com/patent/US20230235475A1

## CPC

- C25D 17/10: Electrodes {, e.g. composition, counter electrode}
- C25D 3/00: Electroplating: Baths therefor
- C25D 3/24: from cyanide baths
- C25D 5/18: Electroplating using modulated, pulsed or reversing current
- C25D 7/00: Electroplating characterised by the article coated
- H01M 4/045: {Electrochemical coating; Electrochemical impregnation}
- H01M 4/0452: {from solutions}
- H01M 4/06: Electrodes for primary cells
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/244: {Zinc electrodes}
- H01M 4/38: of elements or alloys
- H01M 6/04: Cells with aqueous electrolyte
- H01M 6/14: Cells with non-aqueous electrolyte
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01M 10/36: Accumulators not provided for in groups H01M10/05-H01M10/34
- H01M 12/08: composed of a half-cell of a fuel-cell type and a half-cell of the secondary-cell type
- Y02E 60/10: Energy storage using batteries
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of fabricating and using a zinc negative electrode and systems thereof are described. A zinc electroplated electrode including a layer of zinc metal bonded to a surface of an electrically conductive current collector is fabricated by an electroplating process using a zinc electroplating system. The zinc electroplating system includes: a zinc metal anode, a cathode including the current collector for plating zinc thereon, and an electrolyte bath comprising zinc ions. The electroplating process bonds the zinc metal to the surface of the current collector to create the electroplated zinc electrode. The electroplated zinc electrode is used as a negative electrode in a zinc metal cell. The zinc metal cell may be a primary cell or a secondary cell.

## Claims

### Claim at position 1

1-29. (canceled)

### Claim 30

A method of fabricating a zinc metal electrode for use in a zinc metal cell, the method comprising:
providing a zinc electroplating system comprising:
an anode comprising zinc metal;
a cathode comprising a current collector for electroplating a zinc metal layer thereon; and
an electrolyte bath comprising Zn2+ cations or [Zn(OH)4]2− ions;
applying a current or voltage between the anode and the cathode; and
depositing the zinc metal layer onto the current collector, wherein the deposited zinc metal layer is bonded to the current collector.

### Claim 31 (depends on 30)

The method of claim 30, wherein the zinc metal layer has a density greater than 5 g/cc.

### Claim 32 (depends on 30)

The method of claim 30, wherein the zinc metal layer has a density greater than 6 g/cc.

### Claim 33 (depends on 30)

The method of claim 30, wherein the zinc metal layer has a thickness between 0.05 μm to 50 mm.

### Claim 34 (depends on 30)

The method of claim 30, wherein the cathode is electroplated using a batch process wherein the batch process is one or more of rack electroplating and barrel electroplating.

### Claim 35 (depends on 30)

The method of claim 30, wherein the cathode is electroplated using a continuous process wherein the continuous process is one or more of roll-to-roll electroplating or reel-to-reel electroplating.

### Claim 36 (depends on 30)

The method of claim 30, wherein the zinc metal of the anode is in the form of one or more of balls, foil, rod, sheet, wire, plate, foam, sponge, mesh, and bar.

### Claim 37 (depends on 30)

The method of claim 30, wherein the anode comprises an anode basket or bag containing zinc metal and wherein the anode basket or bag is composed of one or more of titanium, stainless steel, tantalum, zirconium, or other corrosion resistant material.

### Claim 38 (depends on 31)

The method of claim 31, wherein the current collector comprises an electrically conductive surface.

### Claim 39 (depends on 30)

The method of claim 30, wherein the current collector comprises one or more of a foil, wire, sheet, plate, foam, sponge, mesh, rod, bar, can, and lid.

### Claim 40 (depends on 30)

The method of claim 30, wherein the electrolyte bath is an alkaline non-cyanide zinc bath.

### Claim 41 (depends on 40)

The method of claim 40, wherein the alkaline non-cyanide zinc bath contains an excess of hydroxide ions (OH—), an excess of zincate ions ([Zn(OH)4]2−), or an excess of hydroxide ions and an excess of zincate ions, and wherein the pH of the electrolyte bath is >7.

### Claim 42 (depends on 30)

The method of claim 30, wherein the electrolyte bath is a cyanide zinc bath and wherein the cyanide zinc bath contains dissolved zinc cyanide (Zn(CN)2).

### Claim 43 (depends on 30)

The method of claim 30, wherein the electrolyte bath is an acid sulfate zinc bath and wherein the acid sulfate zinc bath contains dissolved zinc sulfate (ZnSO4), and wherein the pH of the electrolyte bath is <7.

### Claim 44 (depends on 30)

The method of claim 30, wherein the electrolyte bath is an acid chloride zinc bath wherein the acid chloride zinc bath contains dissolved zinc chloride (ZnCl2), and wherein the pH of the electrolyte bath is <7.

### Claim 45 (depends on 30)

The method of claim 30, wherein the electrolyte bath is one of maintained at room temperature in the absence of a temperature controller for the electrolyte bath and heated and maintained at a constant temperature between 20° C. and 60° C.

### Claim 46 (depends on 30)

The method of claim 30, wherein the zinc metal from the anode is plated onto the current collector by applying a voltage difference between the anode and the cathode and wherein the voltage difference is applied using a constant voltage.

### Claim 47 (depends on 30)

The method of claim 30, wherein the zinc metal from the anode is plated onto the current collector by applying a voltage difference between the anode and the cathode and wherein the voltage difference is applied using a voltage pulse.

### Claim 48 (depends on 39)

The method of claim 39, wherein the zinc from the anode is plated onto the current collector by applying a current between the anode and the cathode and wherein the current is applied using a constant current.

### Claim 49 (depends on 39)

The method of claim 39, wherein the zinc from the anode is plated onto the current collector by applying a current between the anode and the cathode and wherein the current is applied using a current pulse.