# US 2023/0235422 A1 · Motor core production method and heat treatment device used therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0235422 A1
- Document ID: US20230235422A1
- Status: Published application
- Kind: A1
- Application number: 18/097,936
- Filed: 2023-01-17
- Published: 2023-07-27
- Earliest claimed: 2022-01-21
- Assignees: Daido Steel Co., Ltd.
- Applicants: Daido Steel CO., Ltd.
- Inventors: Koichiro ASAI
- Web page: https://patentgrep.com/patent/US20230235422A1

## CPC

- C21D 9/0056: {Furnaces through which the charge is moved in a horizontal straight path (C21D9/0043 takes precedence)}
- C21D 1/26: Methods of annealing
- C21D 1/74: Methods of treatment in inert gas, controlled atmosphere, vacuum or pulverulent material
- C21D 1/76: Adjusting the composition of the atmosphere
- C21D 6/00: Heat treatment of ferrous alloys
- C21D 8/12: during manufacturing of articles with special electromagnetic properties
- C21D 8/1244: characterised by the heat treatment
- C21D 8/1272: {Final recrystallisation annealing}
- C21D 9/0062: {Heat-treating apparatus with a cooling or quenching zone}
- C21D 9/0068: {for particular articles not mentioned below}
- C21D 9/46: for sheet metals
- C21D 9/561: {with a controlled atmosphere or vacuum}
- C21D 9/563: {Rolls; Drums; Roll arrangements}
- C21D 9/573: with cooling
- C21D 9/67: adapted for treating the charge in vacuum or special atmosphere
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

The present invention relates to a motor core production method including: a preparation step of preparing a laminate of electromagnetic steel sheets each processed into a predetermined shape; a first heating step of heating the laminate at an atmospheric temperature of 500° C. to 800° C. in an atmospheric gas comprising at least one kind selected from the group consisting of a low oxidizing gas and a reducing gas, and having a dew point of −20° C. or lower; and a second heating step of soaking the laminate at 1,000° C. to 1,200° C. in a vacuum of 100 Pa or less after the first heating step, and a heat treatment device for performing the production method.

## Claims

### Claim 1

A motor core production method comprising:
a preparation step of preparing a laminate of electromagnetic steel sheets each processed into a predetermined shape;
a first heating step of heating the laminate at an atmospheric temperature of 500° C. to 800° C. in an atmospheric gas comprising at least one kind selected from the group consisting of a low oxidizing gas and a reducing gas, and having a dew point of −20° C. or lower; and
a second heating step of soaking the laminate at 1,400° C. to 1,200° C. in a vacuum of 100 Pa or less after the first heating step.

### Claim 2 (depends on 1)

The motor core production method according to claim 1, wherein the laminate is heat-treated in a state of being placed on a jig made of a C/C composite.

### Claim 3 (depends on 1)

The motor core production method according to claim 1, wherein the low oxidizing gas is nitrogen gas, and the reducing gas is at least one kind selected from the group consisting of hydrogen gas and carbon monoxide gas.

### Claim 4 (depends on 1)

The motor core production method according to claim 1, wherein each of the electromagnetic steel sheets before the first heating step has an average crystal grain size of less than 100 μm.

### Claim 5 (depends on 4)

The motor core production method according to claim 4, wherein the each of electromagnetic steel sheets after the second heating step has an average crystal grain size of 100 μm to 300 μm.

### Claim 6 (depends on 1)

A roller hearth type heat treatment device for performing the production method according to claim 1, the heat treatment device comprising:
a plurality of heat treatment chambers configured to heat the laminate; and
a roller disposed in each of the heat treatment chambers and configured to support and convey the laminate, wherein
the plurality of heat treatment chambers comprises a first heating chamber performing the first heating step, a second heating chamber performing the second heating step, and an annealing chamber annealing the laminate after the second heating step, and
the first heating chamber, the second heating chamber and the annealing chamber are disposed in series.

### Claim 7 (depends on 1)

A heat treatment device for performing the production method according to claim 1, the heat treatment device comprising:
a transport track;
a batch-type heating chamber disposed along the transport track and configured to perform at least one of the first heating step and the second heating step;
a batch-type cooling chamber disposed along the transport track and configured to anneal the laminate after the second heating step; and
a transport unit comprising a temperature-retaining chamber configured to house a target object and retain a temperature of the target object by a heater, and a transfer chamber configured to transfer the laminate between the heating chamber and the temperature-retaining chamber and between the cooling chamber and the temperature-retaining chamber.