# US 2023/0235098 A1 · Sphere-like super-macroporous mesoporous material and polyolefin catalyst containing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0235098 A1
- Document ID: US20230235098A1
- Status: Published application
- Kind: A1
- Application number: 18/000,716
- Filed: 2020-10-30
- Published: 2023-07-27
- Earliest claimed: 2020-06-05
- Assignees: China Petroleum & Chemical Corporation; Beijing Research Institute of Chemical Industry, China Petroleum & Chemical Corporation
- Applicants: China Petroleum & Chemical Corporation; Beijing Research Institute of Chemical Industry, China Petroleum & Chemical Corporation
- Inventors: Yu KANG; Xinping LYU; Dongbing LIU; Zifang GUO; Hongmei LIU; Bingyi LI; Ruen WANG
- Web page: https://patentgrep.com/patent/US20230235098A1

## CPC

- C08F 4/02: Carriers therefor
- C08F 110/02: Ethene
- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- B01J 21/08: Silica
- B01J 21/10: Magnesium; Oxides or hydroxides thereof
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 23/02: of the alkali- or alkaline earth metals or beryllium
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 35/51: Spheres
- B01J 35/615: {100-500 m2/g}
- B01J 35/647: {2-50 nm}
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/0045: {Drying a slurry, e.g. spray drying}
- B01J 37/0201: {Impregnation}
- B01J 37/088: {Decomposition of a metal salt}
- C01B 33/18: Preparation of finely divided silica neither in sol nor in gel form; After-treatment thereof (preparation of aerogels by dehydrating gels C01B33/158; treatment to enhance the pigmenting or filling properties C09C)
- C08F 4/605: Component covered by group C08F4/60 with a metal or compound covered by group C08F4/44, not provided for in a single group of groups C08F4/602 or C08F4/603 {(C08F4/60003 - C08F4/60196 take precedence)}
- C08F 2410/04: Dual catalyst, i.e. use of two different catalysts, where none of the catalysts is a metallocene
- C08F 2410/06: Catalyst characterized by its size
- C08F 2410/07: Catalyst support treated by an anion, e.g. Cl-, F-, SO42-
- Y02P 20/52: using catalysts, e.g. selective catalysts
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are a spherelike supermacroporous mesoporous material, a polyolefin catalyst, and a preparation method therefor and an olefin polymerization process. The spherelike supermacroporous mesoporous material has a twodimensional hexagonal ordered pore channel structures. The mesoporous material has an average pore size of 10 nm to 15 nm, a specific surface area of 300 m2/g to 400 m2/g, and an average particle size of 1 µm to 3 µm, based on the total mass of the mesoporous material. The mass content of water in the mesoporous material is < 1 ppm. The mass content of oxygen in the mesoporous material is < 1 ppm. When a polyolefin catalyst prepared with the mesoporous material as a carrier is used for an olefin polymerization reaction, the a polyolefin product with a narrow molecular weight distribution and a good melt index can be obtained.

## Claims

### Claim 1

A mesoporous material, characterized in that the mesoporous material has a two-dimensional hexagonal ordered channel structure, and the mesoporous material has an average pore diameter of from 10 nm to 15 nm, a specific surface area of from 300 m2/g to 400 m2/g, and an average particle size of from 1 µm to 3 µm; the mass content of water in the mesoporous material is less than 1 ppm, preferably less than 0.5 ppm, and more preferably less than 0.1 ppm, and the mass content of oxygen gas in the mesoporous material is less than 1 ppm, preferably less than 0.5 ppm, and more preferably less than 0.1 ppm, based on the total mass of the mesoporous material.

### Claim 2 (depends on 1)

The mesoporous material as claimed in claim 1, having at least one of the following features:
the mesoporous material has a water contact angle of 101° to 130°, preferably 115° to 125°, and more preferably 118° to 124°;
the mesoporous material has a crushing strength of 0.001 N/cm to 0.6 N/cm, preferably 0.01 N/cm to 0.55 N/cm, and more preferably 0.1 N/cmto 0.45 N/cm;
the mesoporous material has a pore volume of 1 mL/g to 2 mL/g, and preferably 1.5 mL/g to 1.9 mL/g; and
the mesoporous material has a particle size distribution of 0.01 to 3, and preferably 0.1 to 2.8.

### Claim 3 (depends on 1)

The mesoporous material as claimed in claim 1, wherein the mesoporous material is obtained by treatment with a chlorinecontaining silane;
preferably, the chlorinecontaining silane is at least one selected from the group consisting of dichlorodimethoxysilane, monochlorotrimethoxysilane, dichlorodiethoxysilane and monochlorotriethoxysilane.

### Claim 4 (depends on 1)

The mesoporous material as claimed in claim 1, wherein the mesoporous material has an average pore diameter of from 11 nm to 13 nm, a specific surface area of from 310 m2/g to 380 m2/g, and an average particle size of from 1.1 µm to 2.9 µm.

### Claim 5

A method for a mesoporous material, comprising:
(1) mixing and contacting a silicon source, an acid agent, ammonium fluoride and heptane in the presence of a template agent and water, and subjecting the mixture resulting from the mixing and contacting in sequence to crystallization, filtering and drying, to afford a raw powder of the mesoporous material;
(2) subjecting the raw powder of the mesoporous material in sequence to a template agentremoving treatment, a primary thermal activation treatment and a secondary thermal activation treatment, to afford the mesoporous material.

### Claim 6 (depends on 5)

The method as claimed in claim 5, having at least one of the following features:
in step (2), the conditions for the primary thermal activation treatment include: in an inert atmosphere, a treatment temperature of from 250° C. to 900° C., preferably from 250° C. to 700° C., and more preferably from 250° C. to 650° C., and a treatment time of from 1 to 48 hours, preferably from 4 to 48 hours, and more preferably from 6 to 24 hours;
in step (2), the conditions for the secondary thermal activation treatment include: in an inert atmosphere, a treatment temperature of from 250° C. to 900° C., preferably from 250° C. to 700° C., and more preferably from 250° C. to 650° C., and a treatment time of from 1 to 48 hours, preferably from 4 to 48 hours, and more preferably from 6 to 24 hours; and
in step (2), the conditions for the primary thermal activation treatment are the same as the conditions for the secondary thermal activation treatment.

### Claim 7 (depends on 5)

The method as claimed in claim 5, having at least one of the following features:
in step (1), the mixing and contacting are carried out as follows: the silicon source, the acid agent, the ammonium fluoride and the heptane are stirred in the presence of the template agent and water at a temperature of 25° C. to 60° C. for a period of time of 4 minutes or more, and then the resulting mixture is left stand still for 1 hour or more;
in step (1), the acid agent is at least one of hydrochloric acid, sulfuric acid, nitric acid and hydrobromic acid, preferably hydrochloric acid;
in step (1), the silicon source is at least one of ethyl orthosilicate, methyl orthosilicate, propyl orthosilicate, sodium orthosilicate and silica sol, and more preferably ethyl orthosilicate;
a molar ratio of the template agent to the silicon source to the acid agent to the ammonium fluoride to the heptane is 1 : 2 to 500 : 100 to 2000 : 0.7 to 200 : 20 to 1650;
the template agent is a triblock copolymer of polyoxyethylenepolyoxypropylene polyoxyethylene, EO20PO70EO20;
the conditions for the crystallization include a crystallization temperature of 90° C. to 180° C. and a crystallization time of 10h to 40h;
in step (2), the template agentremoving treatment includes washing the raw powder of the mesoporous material with an alcohol at 90 to 120° C. for 10 to 40 hours.

### Claim 8 (depends on 5)

The method as claimed in claim 5, wherein the method further comprises mixing via stirring the thermally activated mesoporous material and a chlorinecontaining silane;
preferably, the chlorinecontaining silane is at least one selected from the group consisting of dichlorodimethoxysilane, monochlorotrimethoxysilane, dichlorodiethoxysilane and monochlorotriethoxysilane.

### Claim 9 (depends on 5)

The method as claimed in claim 5, wherein the method does not comprise a grinding step after the thermal activation treatment.

### Claim 10 (depends on 1)

A polyolefin catalyst comprising a carrier and, supported on the carrier, a magnesium component, a titanium component and an optional electron donor component, wherein the carrier is the mesoporous material as claimed in claim 1.

### Claim 11 (depends on 10)

The polyolefin catalyst as claimed in claim 10, having at least one of the following features:
the content of the carrier is from 20 wt.% to 90 wt.%, preferably from 30 wt.% to 70 wt.%, based on the total weight of the polyolefin catalyst;
the content of the magnesium component in terms of magnesium element is from 1 wt.% to 50 wt.%, preferably from 1 wt.% to 30 wt.%, based on the total weight of the polyolefin catalyst;
the content of the titanium component in terms of titanium element is from 1 wt.% to 50 wt.%, preferably from 1 wt.% to 30 wt.%, based on the total weight of the polyolefin catalyst;
the polyolefin catalyst has a pore volume of from 0.5 mL/g to 1 mL/g;
the polyolefin catalyst has a specific surface area of from 120 m2/g to 300 m2/g;
the polyolefin catalyst has a most probable pore diameter of from 7 nm to 12 nm;
the polyolefin catalyst has an average particle size of from 3 µm to 25 µm; and
the polyolefin catalyst has a particle size distribution value of from 0.85 to 0.95.

### Claim 12 (depends on 1, 2, 3, 4, 10)

A method for preparing the polyolefin catalyst as claimed in claim 10, comprising:
(i) under an inert atmosphere, (ia) conducting impregnation treatment of the mesoporous material of any one of claims 1 to 4 with a solution containing a magnesium component and then with a solution containing a titanium component, (ib) conducting impregnation treatment of the mesoporous material of any one of claims 1 to 4 with a solution containing a titanium component and then with a solution containing a magnesium component, or (ic) conducting coimpregnation treatment of the mesoporous material of any one of claims 1 to 4 with a solution containing both a titanium component and a magnesium component, to obtain a slurry; and
(ii) spray drying the slurry from step (i) to obtain the polyolefin catalyst.

### Claim 13 (depends on 10)

An olefin polymerization method, comprising: a) polymerizing olefin monomer(s) under polymerization conditions in the presence of the polyolefin catalyst of claim 10 and a cocatalyst, to provide a polyolefin; and b) recovering the polyolefin.