# US 2023/0234886 A1 · High-strength glass-ceramic-based lightweight aggregates and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0234886 A1
- Document ID: US20230234886A1
- Status: Published application
- Kind: A1
- Application number: 18/097,346
- Filed: 2023-01-16
- Published: 2023-07-27
- Earliest claimed: 2022-01-21
- Assignees: Wuhan University of Technology
- Applicants: Wuhan University of Technology
- Inventors: Yunpeng Liu; Wenhao Wan; Fazhou Wang; Shuguang Hu
- Web page: https://patentgrep.com/patent/US20230234886A1

## CPC

- C03C 12/00: Powdered glass (C03C8/02 takes precedence); Bead compositions
- C04B 33/132: Waste materials; Refuse {; Residues} (C04B33/16 takes precedence)
- C03B 19/108: {Forming porous, sintered or foamed beads (chemical aspects C03C11/00)}
- C03C 1/026: {Pelletisation or prereacting of powdered raw materials (apparatus or methods C03B1/02)}
- C03C 3/078: containing an oxide of a divalent metal, e.g. an oxide of zinc
- C03C 10/00: Devitrified glass ceramics, i.e. glass ceramics having a crystalline phase dispersed in a glassy phase and constituting at least 50% by weight of the total composition
- C04B 14/22: Glass {; Devitrified glass}
- C04B 18/023: {Fired or melted materials}
- C04B 18/027: {Lightweight materials}
- C04B 33/13: Compounding ingredients (C04B33/36, C04B35/71 take precedence {; pigments for ceramics C09C1/0009})
- C04B 33/131: {Inorganic additives}
- C03B 1/00: Preparing the batches (chemical compositions C03C)
- C03B 19/063: {by hot-pressing powders}
- C03C 1/002: {Use of waste materials, e.g. slags}
- C03C 10/0063: {containing waste materials, e.g. slags}
- C03C 10/16: Halogen containing crystalline phase
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C04B 38/009: {Porous or hollow ceramic granular materials, e.g. microballoons (C04B18/027, C04B20/002 take precedence)}
- C04B 2111/40: Porous or lightweight materials
- C04B 2201/50: for the mechanical strength
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3232: Titanium oxides or titanates, e.g. rutile or anatase
- C04B 2235/3241: Chromium oxides, chromates, or oxide-forming salts thereof
- C04B 2235/442: Carbonates
- C04B 2235/445: Fluoride containing anions, e.g. fluosilicate
- Y02P 40/60: Production of ceramic materials or ceramic elements, e.g. substitution of clay or shale by alternative raw materials, e.g. ashes
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention discloses high-strength glass-ceramic-based lightweight aggregates and the preparation method thereof. The mass ratio of raw material components is 50-70 parts of engineering muck, 20-40 parts of glass, 3-7 parts of calcium carbonate, 3-7 parts of magnesium oxide, and 2-10 parts of a nucleating agent; the nucleating agent is at least one of calcium fluoride, titanium dioxide, and chromium oxide. After crushing, mixing, and granulating, spherical particles with a particle size of 10-12 mm are formed; and then the product can be obtained after drying, sintering, and cooling. The obtained lightweight aggregate from the invention has a diopside matrix which provides high strength and a low water absorption rate at low densities. Moreover, waste glass and engineering muck could be utilized with high value.

## Claims

### Claim 1

High-strength glass-ceramic-based lightweight aggregates, containing the following components in parts by mass for sintering steps:
50-70 parts of engineering muck, 20-40 parts of waste glass, 3-7 parts of calcium carbonate, 3-7 parts of magnesium oxide, and 2-10 parts of a nucleating agent; wherein the nucleating agent is at least one of calcium fluoride, titanium dioxide, and chromium oxide;
wherein the sintering steps of the high-strength glass-ceramic-based lightweight aggregates are as follows:
a first heating stage that raises a temperature from room temperature to 800° C. at a heating rate of 5-10° C./min;
a nucleation phase that is maintained at 800° C. for 30-60 min;
a second heating stage that raises the temperature from 800° C. to 1100 -1180° C. at a heating rate of 10° C./min;
a sintering phase that maintains at 1120-1180° C. for 1 h and then cools down to the room temperature.

### Claim 2 (depends on 1)

The high-strength glass-ceramic-based lightweight aggregates according to claim 1, containing the following components in parts by mass: 50-70 parts of engineering muck, 20-40 parts of waste glass, 5 parts of calcium carbonate, 5 parts of magnesium oxide and 2-10 parts of a nucleating agent; wherein the nucleating agent is at least one of calcium fluoride, titanium dioxide, and chromium oxide.

### Claim 3 (depends on 2)

The high-strength glass-ceramic-based lightweight aggregates according to claim 2, wherein the engineering muck is brown muck produced in underground engineering development, which is crushed before use and then dried at 105° C. for 48 h.

### Claim 4 (depends on 2)

The high-strength glass-ceramic-based lightweight aggregates according to claim 2, wherein the calcium carbonate and the magnesium oxide are analytically pure; the waste glass is waste colorless transparent flat glass.

### Claim 5 (depends on 1)

The high-strength glass-ceramic-based lightweight aggregates according to claim 1 are used to prepare building materials.

### Claim 6 (depends on 1)

A preparation method of the high-strength glass-ceramic-based lightweight aggregates, comprising the following steps:
(1) separately crushing, ball milling, and sieving the engineering muck, the waste glass, the calcium carbonate, the magnesium oxide, and the nucleating agent to obtain powder thereof;
(2) mixing the powder in step (1) with water to obtain a mixture, and then granulating, drying, and sintering the mixture to obtain the high-strength glass-ceramic-based lightweight aggregates according to claim 1.

### Claim 7 (depends on 6)

The preparation method of the high-strength glass-ceramic-based lightweight aggregates according to claim 6, wherein an amount of the water added in step (2) accounts for 30-40% of a total mass of the powder.

### Claim 8 (depends on 7)

The preparation method of the high-strength glass-ceramic-based lightweight aggregates according to claim 7, wherein a process of the granulating in step (2) is as follows: preparing spherical particles with a particle size of 10-12 mm by a granulator.

### Claim 9 (depends on 7)

The preparation method of the high-strength glass-ceramic-based lightweight aggregates according to claim 7, wherein a temperature of the drying is 105° C. and a time of the drying is 2-4 h in step (2); and
the sieving in step (1) is 200 mesh sieve.