# US 2023/0227361 A1 · High-toughness geopolymer grouting material modified by ultra-high weight fibers and emulsified asphalt, preparation and application

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0227361 A1
- Document ID: US20230227361A1
- Status: Published application
- Kind: A1
- Application number: 17/915,490
- Filed: 2021-01-25
- Published: 2023-07-20
- Earliest claimed: 2020-11-16
- Assignees: Tongji University
- Applicants: Tongji University
- Inventors: Xingyi ZHU; Yafeng PANG; Yuchuan DU
- Web page: https://patentgrep.com/patent/US20230227361A1

## CPC

- C04B 28/003: {containing hybrid binders other than those of the polycarboxylate type}
- C04B 28/006: {containing mineral polymers, e.g. geopolymers of the Davidovits type}
- E01C 7/147: {Repairing concrete pavings, e.g. joining cracked road sections by dowels, applying a new concrete covering (applying thin surface layers with other binder E01C7/35; repairing pavings in general E01C11/005; roughening by means of tools E01C11/24)}
- E01C 23/10: for raising or levelling sunken paving; for filling voids under paving; for introducing material into substructure (consolidating soil in general E02D3/12)
- C04B 2111/0075: {for road construction}
- C04B 2111/70: Grouts, e.g. injection mixtures for cables for prestressed concrete
- C04B 2201/50: for the mechanical strength
- Y02P 40/10: Production of cement, e.g. improving or optimising the production methods; Cement grinding
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- E01C: CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE; MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR (forming roads or like surfaces by compacting or grading snow or ice E01H)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention relates to a high-toughness geopolymer grouting material modified by ultra-high molecular weight fibers and emulsified asphalt, and a preparation method and application thereof, wherein the grouting material comprises the following components in parts by mass: 4-12 parts of emulsified asphalt, 80-100 parts of a geopolymer, 103-126 parts of an alkali-activated solution, 2-3 parts of ultra-high molecular weight fibers and 30-35 parts of water. Compared to the prior art, the grouting material modified by ultra-high molecular weight fibers and emulsified asphalt is simple to prepare, has good fluiditygood, and matches well with road substrate; the good toughness and crack control capability of the ultra-high molecular weight fibers enables this novel grouting material to overcome the problem in durability of common geopolymer-based materials. The material of the present invention can be applied in filling voids beneath a slab of a cement concrete pavement and in the technology of non-excavation road reinforcement of a road base course and a subgrade of a high-grade highway.

## Claims

### Claim 1

A high-toughness geopolymer grouting material modified by ultra-high molecular weight fibers and emulsified asphalt, comprising following components in parts by weight:
4-12 parts of the emulsified asphalt;
80-100 parts of a geopolymer;
103-126 parts of an alkali-activated solution;
2-3 parts of the ultra-high molecular weight fiber; and
30-35 parts of water,
wherein the geopolymer comprises a combination of one or more of metakaolin, kaolinite, fly ash and slag,
wherein the emulsified asphalt is cationic emulsified asphalt which is medium-breaking or slow-breaking, the cationic emulsified asphalt having a screen residue of less than or equal to 0.1% and 1-day room-temperature stability of less than or equal to 1%,
wherein the ultra-high molecular weight fiber is polyethylene fiber with a molecular weight of 1,000,000-5,000,000, an ultimate tensile strain of 3%-7%, a fiber length of 6-18 mm, a nominal strength of 2900-3800 MPa and an elastic modulus of 100-120 GPa,
wherein the alkali-activated solution consists of sodium silicate solution and sodium hydroxide particles, comprising following components in parts by mass: 11-15 parts of the sodium silicate solution, and 1-4 parts of the sodium hydroxide particles,
wherein a preparation method of the high-toughness geopolymer grouting material modified by ultra-high molecular weight fibers and emulsified asphalt comprises following steps:
step (1) weighing preset amounts of sodium silicate solution and sodium hydroxide according to the component requirement to prepare the alkali-activated solution, and allowing the prepared alkali-activated solution to stand for 18-36 h;
step (2) weighing each raw material according to the mass parts;
step (3) adding the geopolymer into a mixing pot of a cement paste mixer, turning on the mixer, and after mixing for 20-40 s, adding the alkali-activated solution into the mixing pot for a further mixing for 1-2 min;
step (4) adding the ultra-high molecular weight fibers into the mixing pot in 2-4 batches, and stirring quickly after the addition of all of the fibers until well-mixed to obtain a geopolymer-based slurry; and
step (5) adding the emulsified asphalt into the geopolymer-based slurry and mixing well to obtain the high-toughness geopolymer grouting material.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The high-toughness geopolymer grouting material modified by ultra-high molecular weight fibers and emulsified asphalt of claim 1, wherein the geopolymer has a density of 2.2-2.7 g·cm−3, an elastic modulus of 50-55 GPa, a tensile strength of 30-190 MPa, a compressive strength of 40-120 MPa and a fracture energy of 50-1500 J·cm−2.

### Claim 4

(canceled)

### Claim 5

(canceled)

### Claim 6

(canceled)

### Claim 7 (depends on 1)

A preparation method of the high-toughness geopolymer grouting material modified by ultra-high molecular weight fibers and emulsified asphalt of claim 1, comprising following steps:
step (1) weighing preset amounts of sodium silicate solution and sodium hydroxide according to the component requirement to prepare the alkali-activated solution, and allowing the prepared alkali-activated solution to stand for 18-36 h;
step (2) weighing each raw material according to the mass parts;
step (3) adding the geopolymer into a mixing pot of a cement paste mixer, turning on the mixer, and after mixing for 20-40 s, adding the alkali-activated solution into the mixing pot for a further mixing for 1-2 min;
step (4) adding the ultra-high molecular weight fibers into the mixing pot in 2-4 batches, and stirring quickly after the addition of all of the fibers until well-mixed to obtain a geopolymer-based slurry; and
step (5) adding the emulsified asphalt into the geopolymer-based slurry and mixing well to obtain the high-toughness geopolymer grouting material.

### Claim 8 (depends on 7)

The preparation method of claim 7 of the high-toughness geopolymer grouting material modified by ultra-high molecular weight fibers and emulsified asphalt, wherein in the step (4), the mixing is firstly conducted at ⅓ of a rated mixing speed, and then the ultra-high molecular weight fibers are added into the mixing pot in 2-4 batches, and after that, the mixing is conducted at the rated mixing speed.

### Claim 9 (depends on 7)

The preparation method of claim 7 of the high-toughness geopolymer grouting material modified by ultra-high molecular weight fibers and emulsified asphalt, wherein the high-toughness geopolymer grouting material obtained in the step (5) has a 28-day flexural strength of 12.8 MPa and a 28-day compressive strength of 37.03 MPa.

### Claim 10 (depends on 1)

An application of the high-toughness geopolymer grouting material modified by ultra-high molecular weight fibers and emulsified asphalt of claim 1 in filling voids beneath a slab of a cement concrete pavement, reinforcement of a road base course and a subgrade, and non-excavation road reinforcement.