# US 2023/0192529 A1 · Continuous sol-gel process for producing silicate-containing glasses or glass ceramics

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0192529 A1
- Document ID: US20230192529A1
- Status: Published application
- Kind: A1
- Application number: 18/168,731
- Filed: 2023-02-14
- Published: 2023-06-22
- Earliest claimed: 2016-08-12
- Assignees: D. Swarovski & Co.
- Applicants: D. Swarovski KG
- Inventors: Georg Czermak; Matthias Gander; Christina Streiter; Christian Gabl; Christian Lipp; Roy Layne Howell; Nina Stepanik
- Web page: https://patentgrep.com/patent/US20230192529A1

## CPC

- C03C 3/076: with 40% to 90% silica, by weight {(C03C3/045 takes precedence)}
- C03B 19/12: by liquid-phase reaction processes
- C03C 1/006: {to produce glass through wet route}
- C03B 2201/06: Doped silica-based glasses
- C03B 2201/40: doped with transition metals other than rare earth metals, e.g. Zr, Nb, Ta or Zn
- C03B 2201/42: doped with titanium
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A continuous sol-gel process for producing silicate-containing glasses and glass ceramics is proposed, comprising the following steps: (a) continuously feeding a silicon tetraalkoxide, a silicon alkoxide with at least one non-alcoholic functional group and an alcohol into a first reactor (R1), and at least partially hydrolyzing by the addition of a mineral acid to obtain a first product stream (A); (b) continuously providing a second product stream (B) in a second reactor (R2) by feeding a metal alkoxide component or continuously mixing an alcohol and a metal alkoxide component; (c) continuously mixing product streams (A) and (B) in a third reactor (R3) for producing a presol to obtain a third product stream (C); (d) continuously adding water or a diluted acid to the product stream (C) to obtain a sol (gelation); (e) continuously filling the emerging sol into molds to obtain an aquagel; (f) drying the aquagels to obtain xerogels; (g) sintering the xerogels to obtain silicate-containing glasses and glass ceramics.

## Claims

### Claim 1

A continuous sol-gel method for the production of silicate-containing glasses and glass-ceramics comprising the steps of:
(a) continuously feeding a mixture of tetraethyl orthosilicate and methyltriethoxysilane and alcohol into a first reactor R1, and at least partially hydrolyzing by adding a mineral acid to obtain a first product stream A;
the weight ratio of tetraethyl ortho-silicate to the methyltriethoxysilane is 5:1 to 15:1;
(b) continuously providing a second product stream B in a second reactor R2 by adding a metal alkoxide component or continuously mixing the alcohol and metal alkoxide components;
(c) continuous mixing of product streams A and B in a third reactor R3 to produce a pre-sol to obtain a third product stream C;
(d) continuously adding water or dilute acid to product stream C to obtain sol gelation;
(e) continuously filling the obtained sol into a mould to obtain a hydrogel;
(f) drying the hydrogel to obtain a xerogel;
(g) sintering the xerogel at 850 to 1200° C. to obtain a silicate-containing glass and glass-ceramic; wherein the metal oxide component is present in the silicate-containing glass or silicate-containing glass-ceramic in an amount of 20 wt.% to 55 wt.%.

### Claim 2 (depends on 1)

The method of claim 1, wherein nitric acid is used as the mineral acid in the step (a).

### Claim 3 (depends on 1)

The method according to claim 1, characterized in that in the step (a), 1 to 60% of the inorganic acid by weight of the silicon alkoxide is used.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the at least partial hydrolyzing of the silicon alkoxide in the step (a) is carried out at a temperature of 1-100° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein in the step (b), an alkyl orthotitanate is used as the metal alkoxide component.

### Claim 6 (depends on 1)

The method according to claim 1, wherein in the step (b), zirconium (IV) alkoxide is used as the metal alkoxide component.

### Claim 7 (depends on 1)

The method of claim 1, wherein the product streams (A) and (B) are mixed in a volume ratio of metal alkoxide to silica of 10:1 to 1:10.

### Claim 8 (depends on 1)

The method of claim 1, wherein the product streams (A) and (B) are mixed in a temperature range of 0-80° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein at least one of steps (a), (b) or (c) is carried out in a continuous reactor, which may have an upper agitator element.

### Claim 10 (depends on 9)

The method of claim 9, wherein the continuous reactor has a length of 1 cm to 1000 m and/or a cross-sectional width of 1 to 10 mm.

### Claim 11 (depends on 1)

The method of claim 1, wherein the gelation is carried out in a temperature range of 0 to 100° C.

### Claim 12 (depends on 1)

The method of claim 1, wherein the drying is carried out in a temperature range of 0-150° C.

### Claim 13

A silicate-containing glass or a silicate-containing glass-ceramic obtainable by a continuous sol-gel method comprising the steps of:
(a) continuously feeding a mixture of tetraethyl orthosilicate and methyltriethoxysilane and alcohol into the first reactor R1, and at least partially hydrolyzing by adding a mineral acid to obtain a first product stream A; the ortho-silicon The weight ratio of tetraethyl acid to the methyltriethoxysilane is 5:1 to 15:1;
(b) continuously providing a second product stream B in the second reactor R2 by adding the metal alkoxide component or continuously mixing the alcohol and metal alkoxide components;
(c) continuous mixing of product streams A and B in a third reactor R3 to produce a pre-sol to obtain a third product stream C;
(d) continuously adding water or dilute acid to product stream C to obtain sol gelation;
(e) continuously filling the obtained sol into a mould to obtain a hydrogel;
(f) drying the hydrogel to obtain a xerogel;
(g) sintering the xerogel at 850 to 1200° C. to obtain a silicate-containing glass and glass-ceramic; wherein the metal oxide component is present in the silicate-containing glass or silicate-containing glass-ceramic in an amount of 20 wt.% to 55 wt.%.

### Claim 14 (depends on 13)

The silicate-containing glass or silicate-containing glass-ceramic according to claim 13, wherein a refractive index nd of the silicate-containing glass or silicate-containing glass-ceramic is 1.45-1.8.

### Claim 15 (depends on 14)

The silicate-containing glass or silicate-containing glass-ceramic according to claim 14, wherein the refractive index nd of the silicate-containing glass or silicate-containing glass-ceramic is 1.48-1.75.

### Claim 16 (depends on 15)

The silicate-containing glass or silicate-containing glass-ceramic according to claim 15, wherein the refractive index nd of the silicate-containing glass or silicate-containing glass-ceramic is 1.5 to 1.7.

### Claim 17 (depends on 13)

The silicate-containing glass or the silicate-containing glass-ceramic according to claim 13, wherein the silicate-containing glass or the silicate-containing glass-ceramic is resistant to light with a wavelength of 300 to 900 nm is transparent.

### Claim 18 (depends on 17)

The silicate-containing glass or the silicate-containing glass-ceramic according to claim 17, wherein the silicate-containing glass or the silicate-containing glass-ceramic is resistant to light with a wavelength of 350 to 850 nm is transparent.

### Claim 19 (depends on 18)

The silicate-containing glass or the silicate-containing glass-ceramic according to claim 18, wherein the silicate-containing glass or the silicate-containing glass-ceramic is resistant to light with a wavelength of 380 to 780 nm is transparent.

### Claim 20 (depends on 13)

The silicate-containing glass or silicate-containing glass-ceramic according to claim 13, wherein the silicate-containing glass or silicate-containing glass-ceramic has a light transmittance in the visible light range, andthe difference in light transmittance with quartz glass in the visible light range is not more than 30%.