# US 2023/0192488 A1 · A method of separating and recovering bromine from printed circuit board incineration ash by two-step process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0192488 A1
- Document ID: US20230192488A1
- Status: Published application
- Kind: A1
- Application number: 16/627,721
- Filed: 2019-01-15
- Published: 2023-06-22
- Earliest claimed: 2018-09-17
- Assignees: Beijing University of Technology
- Applicants: Beijing University of Technology
- Inventors: DEAN PAN; YUFENG WU
- Web page: https://patentgrep.com/patent/US20230192488A1

## CPC

- C01B 7/096: {Bromine}
- C01G 9/06: Sulfates
- C01G 21/20: Sulfates
- C22B 7/008: {by an alkaline or ammoniacal leaching}
- C22B 7/02: Working-up flue dust
- C22B 13/045: {Recovery from waste materials}
- C22B 19/24: {with leaching with alkaline solutions, e.g. ammonia}
- C22B 19/30: from metallic residues or scraps
- C22B 11/044: {from pyrometallurgical residues, e.g. from ashes, dross, flue dust, mud, skim, slag, sludge}
- C22B 15/0063: {Hydrometallurgy}
- Y02P 10/20: Recycling
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention relates to the field of efficient separation and recovery of bromine by full wet method, especially to a two-step separating method of bromide and recovery of lead and zinc from printed circuit board Incineration ash. It mainly includes first sodium hydroxide alkaline leaching, secondary sodium peroxide alkaline leaching, pH adjustment, separate lead and zinc, bromide evaporation and crystallization to recover crude bromide and other steps. Compared with traditional comprehensive recovery process of ash, the invention uses sodium hydroxide to dissolve bromide, lead and zinc, and uses the strong oxidation of sodium peroxide in alkaline environment, copper bromide and other bromine are oxidized and leached; through two-step method, the efficient leaching of bromine, lead and zinc is realized, silver and other precious metals are enriched at the same time. It is beneficial to subsequent recovery of precious metals and has the characteristics of short tail liquid discharge.

## Claims

### Claim 1

A method of separating and recovering bromine from circuit board Incineration ash by two-step process:
(1) first alkali leaching: proceed first alkali leaching for circuit board incineration ash in a sodium hydroxide solution, first leaching residue and a first leaching solution are obtained after filtration;
(2) secondary alkali leaching: add water to the first leaching residue obtained in step (1) for secondary alkali leaching, and filter to get secondary leaching residue and a secondary leaching solution, the secondary leaching residue is gathered for treatment;
(3) lead and zinc removal: combine the first leaching solution obtained in step (1) and the secondary leaching solution obtained in step (2) to obtain a combined leaching solution, a mass ratio of the first leaching solution to the secondary leaching solution is 1:3-3:1, add 98% industrial concentrated sulfuric acid to the combined leaching solution until pH of the combined leaching solution reaches 6.5-8, lead-zinc removal residue and a lead-zinc removal solution are obtained by filtration;
(4) bromide evaporation and crystallization: proceed evaporation and crystallization for the lead-zinc removal solution obtained in step (3), crude bromide is obtained;
(5) lead separation: add the lead-zinc removal residue obtained in step (3) into water, solid-liquid ratio of the lead-zinc removal residue and water is 1:1-1:2 Kg/L, add 98% industrial concentrated sulfuric acid with stirring until pH reaches 4.5-6; filter to get lead sulfate and a lead separation solution;
(6) zinc evaporation and crystallization: proceed evaporation and crystallization for the lead separation solution obtained in step (5), crude zinc sulfate is obtained.

### Claim 2 (depends on 1)

A method of separating and recovering bromine from circuit board Incineration ash by two-step process according to claim 1, wherein a mass concentration of the sodium hydroxide is 5%-15%, a solid-liquid ratio of the circuit board incineration ash to the sodium hydroxide solution is 1:10-1:15 Kg/L, leaching temperature is 55-75° C., leaching time is 0.5-1 h.

### Claim 3 (depends on 1)

A method of separating and recovering bromine from circuit board Incineration ash by two-step process according to claim 1, wherein a solid-liquid ratio of the first leaching residue to water is 1:5-1:10 Kg/L, leaching temperature is room temperature and add sodium peroxide in leaching process, a solid-liquid ratio of sodium peroxide and water is 20:1-50:1 Kg/m3, after adding sodium peroxide, stir 0.5-2 hours.