# US 2023/0191380 A1 · Phosphorus-modified mfi-structured molecular sieve, catalytic cracking auxiliary and catalytic cracking catalyst containing phosphorus-modified mfi-structured molecular sieves, and processes for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0191380 A1
- Document ID: US20230191380A1
- Status: Published application
- Kind: A1
- Application number: 17/996,187
- Filed: 2021-04-13
- Published: 2023-06-22
- Earliest claimed: 2020-04-13
- Assignees: China Petroleum & Chemical Corporation; Research Institute of Petroleum Processing, Sinopec
- Applicants: China Petroleum & Chemical Corporation; Research Institute of Petroleum Processing, Sinopec
- Inventors: Yibin LUO; Chengqiang WANG; Ying OUYANG; Enhui XING; Xingtian SHU
- Web page: https://patentgrep.com/patent/US20230191380A1

## CPC

- B01J 29/80: Mixtures of different zeolites
- C01B 39/10: the replacing atoms being {at least} phosphorus atoms
- B01J 21/16: Clays or other mineral silicates
- B01J 27/16: containing oxygen {, i.e. acids, anhydrides and their derivates with N, S, B or halogens without carriers or on carriers based on C, Si, Al or Zr; also salts of Si, Al and Zr}
- B01J 29/084: {Y-type faujasite}
- B01J 29/40: of the pentasil type, e.g. types ZSM-5, ZSM-8 or ZSM-11, as exemplified by patent documents US3702886, GB1334243 and US3709979, respectively
- B01J 29/85: Silicoaluminophosphates [SAPO compounds]
- B01J 35/647: {2-50 nm}
- B01J 35/70: characterised by their crystalline properties, e.g. semi-crystalline (catalysts comprising carbon B01J21/18; molecular sieves B01J29/00)
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/0072: {Preparation of particles, e.g. dispersion of droplets in an oil bath}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/28: Phosphorising
- C01B 39/026: {After-treatment}
- C01B 39/38: Type ZSM-5
- C01B 39/54: Phosphates, e.g. APO or SAPO compounds
- C10G 11/05: Crystalline alumino-silicates, e.g. molecular sieves
- B01J 35/30: characterised by their physical properties
- B01J 2029/062: {Mixtures of different aluminosilicates}
- B01J 2229/183: in framework positions
- B01J 2229/186: not in framework positions
- B01J 2229/37: Acid treatment
- B01J 2235/00: Indexing scheme associated with group B01J35/00, related to the analysis techniques used to determine the catalysts form or properties
- C10G 2300/1044: Heavy gasoline or naphtha having a boiling range of about 100 - 180 °C
- C10G 2300/107: Atmospheric residues having a boiling point of at least about 538 °C
- C10G 2300/1074: Vacuum distillates
- C10G 2300/205: Metal content
- C10G 2300/206: Asphaltenes
- C10G 2300/301: Boiling range
- C10G 2300/304: Pour point, cloud point, cold flow properties
- C10G 2300/308: Gravity, density, e.g. API
- C10G 2400/20: C2-C4 olefins
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A phosphorus-modified MFI-structured molecular sieve is characterized in that the molecular sieve has a K value, satisfying: 70%≤K≤90%; for example, 75%≤K≤90%; further for example, 78%≤K≤85%. The K value is as defined in the specification. A cracking auxiliary or cracking catalyst contains the phosphorus-modified MFI molecular sieve.

## Claims

### Claim 1

A phosphorus-modified MFI-structured molecular sieve, which is characterized in that the molecular sieve has a K value, satisfying 70%≤K≤90%; for example, 75%≤K≤90%; further for example, 78%≤K≤85%;
wherein, K=P1/P2×100%,
P1 represents the mass content of phosphorus within a region having an area of 100 square nanometers and a vertical depth from 0 to 2 nm at any crystal surface of the crystal grain of a molecular sieve, as measured by the XPS method,
P2 represents the mass content of phosphorus within a region having an area of 100 square nanometers and a vertical depth from 5 to 10 nm at any crystal surface of the crystal grain of a molecular sieve, as measured by the EPMA method.

### Claim 2 (depends on 1)

The molecular sieve according to claim 1, wherein the molar ratio of the phosphorus content as P2O5 to the alumina content is ≥0.01; for example, ≥0.2; further for example, ≥0.3; still further for example, 0.4-0.7.

### Claim 3 (depends on 1)

The molecular sieve according to claim 1, wherein the phosphorus-modified MFI-structured molecular sieve is a micropore ZSM-5 molecular sieve or a hierarchical ZSM-5 molecular sieve.

### Claim 4 (depends on 1)

The molecular sieve according to claim 1, wherein the micropore ZSM-5 molecular sieve has a silica/alumina molar ratio of 15-1000, for example, 20-200.

### Claim 5 (depends on 1)

The molecular sieve according to claim 1, wherein the hierarchical ZSM-5 molecular sieve has a proportion of the mesopore volume relative to the total pore volume of greater than 10%, an average pore diameter of 2-20 nm, and a silica/alumina molar ratio of 15-1000, for example, 20-200.

### Claim 6 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, 30, 31, 32, 33, 34, 35, 36, 37, 38, 39, 40)

A catalytic cracking auxiliary, based on the dry basis of the catalytic cracking auxiliary, the catalytic cracking auxiliary contains 5-75 wt %, for example, 8-60 wt % of the phosphorus-modified MFI-structured molecular sieve according to claim 1, 1-40 wt % of a binder and 0-65 wt %, for example, 5-55 wt % of a second clay.

### Claim 7 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, 30, 31, 32, 33, 34, 35, 36, 37, 38, 39, 40, 41, 42, 43, 44, 45, 46, 47, 48, 49, 50, 51, 52, 53, 54, 55, 56, 57, 58, 59, 60)

A catalytic cracking catalyst containing phosphorus-modified MFI-structured molecular sieve(s), based on the dry basis of the catalyst, the catalytic cracking catalyst contains 1-25 wt % of Y zeolite, 5-50 wt % of the phosphorus-modified MFI-structured molecular sieve according to claim 1, 1-60 wt % of an inorganic binder and optionally 0-60 wt % of a second clay.

### Claim 8 (depends on 7)

The catalytic cracking catalyst according to claim 7, wherein the binder or the inorganic binder comprises a phosphorus-aluminum inorganic binder and/or other inorganic binder(s),
for example, the phosphorus-aluminum inorganic binder is a phosphorus-aluminum glue and/or a first clay-containing phosphorus-aluminum inorganic binder, further for example, the first clay is selected from kaolin, sepiolite, attapulgite, rectorite, smectite and diatomite; further for example, the first clay-containing phosphorus-aluminum inorganic binder contains 10-40 wt %, for example, 15-40 wt % of aluminum component (as Al2O3), 45-90 wt %, for example, 45-80 wt % of phosphorus component (as P2O5) and greater than 0 and not more than 40 wt % of a first clay on a dry basis, and the first clay-containing phosphorus-aluminum inorganic binder has a P/Al weight ratio of 1.0-6.0, a pH of 1-3.5, and a solid content of 15-60 wt %;
For example, the second clay is selected from kaolin, sepiolite, attapulgite, rectorite, smectite, diatomite, giagerite, halloysite, hydrotalcite, and bentonite;
for example, the other inorganic binder(s) is selected from pseudo-boehmite, alumina sol, silica-alumina sol, and water glass;

### Claim 9 (depends on 7)

The catalytic cracking catalyst according to claim 7, wherein the Y zeolite comprises at least one of PSRY zeolite, PSRY-S zeolite, rare earth-containing PSRY zeolite, rare earth-containing PSRY-S zeolite, USY zeolite, rare earth-containing USY zeolite, REY zeolite, REHY zeolite, and HY zeolite.

### Claim 10 (depends on 1)

A process of preparing the phosphorus-modified MFI-structured molecular sieve according to claim 1, which is characterized in that the phosphorus-modified MFI-structured molecular sieve is obtained through an immersion method, comprising: the contact by mixing an aqueous solution of the phosphorus-containing compound at a temperature of 40-150° C., for example, 50-150° C., further for example, 70-130° C. and an MFI-structured molecular sieve at 40-150° C., for example, 50-150° C., further for example, 70-130° C. at substantially the same temperature for at least 0.1 hours, then the drying, and the calcining at 200-600° C., air or water vapor for at least 0.1 hours; or, vigorously mixing and stirring a phosphorus-containing compound, an MFI-structured molecular sieve and water, adjusting the temperature to 40-150° C., for example, 50-150° C., further for example, 70-130° C., maintaining for at least 0.1 hours, then drying, and calcining at 200-600° C., air or water vapor for at least 0.1 hours.

### Claim 11 (depends on 10)

The process of preparing the phosphorus-modified MFI-structured molecular sieve according to claim 10, wherein the phosphorus-containing compound is selected from organic phosphorous compounds and/or inorganic phosphorous compounds; for example, the organic phosphorous compound is selected from trimethyl phosphate, triphenylphosphine, trimethyl phosphite, tetrabutylphosphonium bromide, tetrabutylphosphonium chloride, tetrabutylphosphonium hydroxide, triphenylethylphosphonium bromide, triphenylbutylphosphonium bromide, triphenylbenzylphosphonium bromide, hexamethylphosphoric triamide, dibenzyl diethylphosphoramidite, 1,3-bis((triethyl-phosphaneyl)methyl)benzene, the inorganic phosphorous compound is selected from phosphoric acid, ammonium hydrogen phosphate, diammonium hydrogen phosphate, ammonium phosphate, boron phosphate.

### Claim 12 (depends on 11)

The process of preparing the phosphorus-modified MFI-structured molecular sieve according to claim 11, wherein the molar ratio of the phosphorus-containing compound (as phosphorus) (as oxide) to the MFI-structured molecular sieve (for example, hydrogen-type ZSM-5 molecular sieve) (as aluminum) (as oxide) is 0.01-2; for example, 0.1-1.5; further for example, 0.2-1.5.

### Claim 13 (depends on 12)

The process of preparing the phosphorus-modified MFI-structured molecular sieve according to claim 12, wherein the phosphorus-containing compound is a mixture of boron phosphate and one or more selected from trimethyl phosphate, triphenylphosphine, trimethyl phosphite, phosphoric acid, ammonium hydrogen phosphate, diammonium hydrogen phosphate, and ammonium phosphate, in the mixture, boron phosphate comprises 10%-80% by weight, for example, boron phosphate comprises 20%-40% by weight.

### Claim 14 (depends on 13)

The process of preparing the phosphorus-modified MFI-structured molecular sieve according to claim 13, wherein the weight ratio of water/molecular sieve in the contacting is 0.5-1, and the contacting time is 0.5-40 hours.

### Claim 15 (depends on 14)

The process of preparing the phosphorus-modified MFI-structured molecular sieve according to claim 14, wherein the calcining is performed at 450-550° C., under the water vapor atmosphere.

### Claim 16 (depends on 6)

A process of preparing the catalytic cracking auxiliary according to claim 6, wherein the process comprises, a phosphorus-modified MFI-structured molecular sieve, a binder, and optionally a second clay are vigorously mixed and stirred with water, and then spray-dried to produce the catalytic cracking auxiliary.

### Claim 17 (depends on 16)

The process of preparing the catalytic cracking auxiliary according to claim 16, wherein the binder includes or is a phosphorus-aluminum inorganic binder.

### Claim 18 (depends on 17)

The process of preparing the catalytic cracking auxiliary according to claim 17, wherein the phosphorus-aluminum inorganic binder is a phosphorus-aluminum glue and/or a first clay-containing phosphorus-aluminum inorganic binder; based on the dry basis weight of the first clay-containing phosphorus-aluminum inorganic binder, the first clay-containing phosphorus-aluminum inorganic binder contains 10-40 wt %, for example, 15-40 wt %, or 10-30 wt %, or 15-35 wt % or 20-40 wt % of an aluminum component (as Al2O3), 45-90 wt %, for example, 45-80 wt %, or 50-75 wt % or 60-80 wt % of a phosphorus component (as P2O5) and on a dry basis, greater than 0 and not more than 40 wt %, for example, 8-35 wt % of a first clay, and the first clay-containing phosphorus-aluminum inorganic binder has a P/Al weight ratio of 1.0-6.0, for example, 1.2-6.0, further for example, 2.0-5.0, a pH of 1-3.5, for example, 2.0-3.0, and a solid content of 15-60 wt %; the first clay comprises at least one of kaolin, sepiolite, attapulgite, rectorite, smectite and diatomite.

### Claim 19 (depends on 18)

The process of preparing the catalytic cracking auxiliary according to claim 18, wherein the second clay is at least one selected from kaolin, sepiolite, attapulgite, rectorite, smectite, giagerite, halloysite, hydrotalcite, bentonite, and diatomite.

### Claim 20 (depends on 19)

The process of preparing the catalytic cracking auxiliary according to claim 19, wherein based on the total weight of the catalytic cracking auxiliary, the binder comprises based on the dry weight, 3-39 wt % of the phosphorus-aluminum inorganic binder and based on the dry weight, 1-30 wt % of other inorganic binder(s).

### Claim 21 (depends on 20)

The process of preparing the catalytic cracking auxiliary according to claim 20, wherein the other inorganic binder may also include at least one of pseudo-boehmite, alumina sol, silica-alumina sol, and water glass.

### Claim 22 (depends on 21)

The process of preparing the catalytic cracking auxiliary according to claim 21, wherein the process further comprises: the spray-dried product is subjected to a first calcining, and then washed, and optionally dried to produce the catalytic cracking auxiliary; wherein for the first calcining, the calcining temperature is 300-650° C., the calcining time is 0.5-8 h; the drying temperature is 100-200° C., the drying time is 0.5-24 h.

### Claim 23 (depends on 22)

The process of preparing the catalytic cracking auxiliary according to claim 22, wherein the process further comprises: the first clay-containing phosphorus-aluminum inorganic binder is prepared with the following steps: an alumina source, the first clay and water are vigorously mixed and stirred to disperse into a slurry having a solid content of 5-48 wt %; wherein the alumina source is aluminum hydroxide and/or alumina that can be peptized by an acid, relative to 10-40 parts by weight, for example, 15-40 parts by weight of the alumina source (as Al2O3), the used amount of the first clay based on the dry weight is greater than 0 part by weight and not more than 40 parts by weight; a concentrated phosphoric acid is added to the slurry under stirring according to the weight ratio of P/Al=1-6, and the resulting mixed slurry is reacted at 50-99° C. for 15-90 minutes; wherein P in the P/Al is the weight of phosphorus as the simple substance in phosphoric acid, Al is the weight of aluminum as the simple substance in the alumina source.

### Claim 24 (depends on 7)

A process of preparing the catalytic cracking catalyst according to claim 7, wherein the process comprises a Y zeolite, the phosphorus-modified MFI-structured molecular sieve, an inorganic binder and optionally a second clay are vigorously mixed and stirred with water, and spray-dried to produce the catalytic cracking catalyst.

### Claim 25 (depends on 24)

The process of preparing the catalytic cracking catalyst according to claim 24, wherein the inorganic binder includes or is a phosphorus-aluminum inorganic binder.

### Claim 26 (depends on 25)

The process of preparing the catalytic cracking catalyst according to claim 25, wherein the phosphorus-aluminum inorganic binder is a phosphorus-aluminum glue and/or a first clay-containing phosphorus-aluminum inorganic binder; based on the dry basis weight of the first clay-containing phosphorus-aluminum inorganic binder, the first clay-containing phosphorus-aluminum inorganic binder contains 10-40 wt %, for example, 15-40 wt % of aluminum component (as Al2O3), 45-90 wt %, for example, 45-80 wt % of phosphorus component (as P2O5) and greater than 0 and not more than 40 wt % of a first clay on a dry basis, and the first clay-containing phosphorus-aluminum inorganic binder has a P/Al weight ratio of 1.0-6.0, a pH of 1-3.5, and a solid content of 15-60 wt %; the first clay comprises at least one of kaolin, sepiolite, attapulgite, rectorite, smectite, and diatomite.

### Claim 27 (depends on 26)

The process of preparing the catalytic cracking catalyst according to claim 26 wherein the second clay is at least one selected from kaolin, sepiolite, attapulgite, rectorite, smectite, giagerite, halloysite, hydrotalcite, bentonite, and diatomite.

### Claim 28 (depends on 27)

The process of preparing the catalytic cracking catalyst according to claim 27, wherein based on the catalytic cracking catalyst, the inorganic binder comprises on the dry basis 3-39 wt % of the phosphorus-aluminum inorganic binder and on the dry basis 1-30 wt % of the other inorganic binder, the other inorganic binder(s) is at least one selected from pseudo-boehmite, alumina sol, silica-alumina sol, and water glass.

### Claim 29 (depends on 28)

The process of preparing the catalytic cracking catalyst according to claim 28, wherein the process further comprises: the spray-dried product is subjected to a first calcining, and then washed, and optionally dried to produce the catalytic cracking catalyst; wherein for the first calcining, the calcining temperature is 300-650° C., the calcining time is 0.5-8 h; the drying temperature is 100-200° C., the drying time is 0.5-24 h.

### Claim 30 (depends on 29)

The process of preparing the catalytic cracking catalyst according to claim 29, wherein the process further comprises: the first clay-containing phosphorus-aluminum inorganic binder is prepared with the following steps: an alumina source, the first clay and water are vigorously mixed and stirred to disperse into a slurry having a solid content of 5-48 wt %; wherein the alumina source is aluminum hydroxide and/or alumina that can be peptized by an acid, relative to 10-40 parts by weight, for example, 15-40 parts by weight of the alumina source (as Al2O3), the used amount of the first clay based on the dry weight is greater than 0 part by weight and not more than 40 parts by weight; a concentrated phosphoric acid is added to the slurry under stirring according to the weight ratio of P/Al=1-6, and the resulting mixed slurry is reacted at 50-99° C. for 15-90 minutes; wherein P in the P/Al is the weight of phosphorus as the simple substance in phosphoric acid, Al is the weight of aluminum as the simple substance in the alumina source.

### Claim at position 31

31-32. (canceled)

### Claim 33 (depends on 6)

A process for catalytically cracking a hydrocarbon oil, which is characterized in that the process comprises: the hydrocarbon oil is reacted by contacting the catalytic cracking auxiliary according to claim 6 under a catalytic cracking condition.

### Claim 34 (depends on 33)

The process for catalytically cracking the hydrocarbon oil according to claim 33, wherein the process comprises: the hydrocarbon oil is reacted by contacting a catalyst mixture containing the catalytic cracking auxiliary and a catalytic cracking catalyst under the catalytic cracking condition; in the catalyst mixture, the content of the catalytic cracking auxiliary is 0.1-30 wt %.

### Claim 35 (depends on 33)

The process for catalytically cracking the hydrocarbon oil according to claim 33, wherein the catalytic cracking condition includes: the reaction temperature is 500-800° C.; the hydrocarbon oil is one or more selected from crude oil, naphtha, gasoline, atmospheric residue, vacuum residue, atmospheric gas oil, vacuum gas oil, straight-run gas oil, propane light/heavy deasphalted oil, coker gas oil and coal liquefication product.