# US 2023/0185195 A1 · Material for forming underlayer film, resist underlayer film, method of producing resist underlayer film, and laminate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0185195 A1
- Document ID: US20230185195A1
- Status: Published application
- Kind: A1
- Application number: 18/168,261
- Filed: 2023-02-13
- Published: 2023-06-15
- Earliest claimed: 2017-05-31
- Assignees: Mitsui Chemicals, Inc.
- Applicants: Mitsui Chemicals, Inc.
- Inventors: Koji INOUE; Takashi ODA; Keisuke KAWASHIMA
- Web page: https://patentgrep.com/patent/US20230185195A1

## CPC

- G03F 7/11: having cover layers or intermediate layers, e.g. subbing layers {(G03F7/091 - G03F7/093, B41N3/03 take precedence)}
- B32B 27/00: Layered products comprising {a layer of} synthetic resin {(fibrous or filamentary layer made of a synthetic resin B32B5/02; particulate layer made of a synthetic resin B32B5/16; foamed layer made of a synthetic resin B32B5/18)}
- C08G 61/08: of carbocyclic compounds containing one or more carbon-to-carbon double bonds in the ring
- C08G 61/12: Macromolecular compounds containing atoms other than carbon in the main chain of the macromolecule
- C09D 165/00: Coating compositions based on macromolecular compounds obtained by reactions forming a carbon-to-carbon link in the main chain (C09D107/00 - C09D157/00, C09D161/00 take precedence); Coating compositions based on derivatives of such polymers
- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- G03F 7/094: {Multilayer resist systems, e.g. planarising layers}
- G03F 7/168: {Finishing the coated layer, e.g. drying, baking, soaking}
- C08G 2261/12: Copolymers
- C08G 2261/135: Cross-linked structures
- C08G 2261/1426: containing carboxy groups (COOH) and/or -C(=O)O-moieties
- C08G 2261/228: Polymers, i.e. more than 10 repeat units
- C08G 2261/3324: derived from norbornene
- C08G 2261/3325: derived from other polycyclic systems
- C08G 2261/3342: derived from cycloolefins containing heteroatoms
- C08G 2261/418: Ring opening metathesis polymerisation [ROMP]
- C08G 2261/598: Chemical stability
- C08G 2261/76: crosslinking
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

A material for forming an underlayer film according to the present invention is a material for forming an underlayer film which is used to form a resist underlayer film used in a multi-layer resist process, the material including a cyclic olefin polymer which has a repeating structural unit [A] represented by Formula (1) and a repeating structural unit [B] represented by Formula (2), in which a molar ratio [A]/[B] of the structural unit [A] to the structural unit [B] in the cyclic olefin polymer is greater than or equal to 5/95 and less than or equal to 95/5.

## Claims

### Claim 1

A laminate comprising:
a substrate; and
a resist underlayer film containing a material for forming an underlayer film,
which is formed on one surface of the substrate,
wherein the material for forming an underlayer film is a material of a film containing a cyclic olefin polymer,
the cyclic olefin polymer is soluble in an organic solvent at any concentration of at least greater than or equal to 0.01% by mass and less than or equal to 50% by mass, and
a residual film rate of the cyclic olefin polymer in the film which is measured using the following method 4 is greater than or equal to 50% and less than or equal to 100%,
method 4: a coating film which is formed of the cyclic olefin polymer and has a thickness (α) of greater than or equal to 200 nm and less than or equal to 500 nm is formed on a silicon wafer, the obtained coating film is treated at 200° C. for 10 minutes, immersed in propylene glycol-1monomethyl ether-2-acetate at 23° C. for 10 minutes, and dried under conditions of 150° C. for 3 minutes, and a remaining solvent in the coating film is removed, and a thickness (β) of the coating film obtained by removing the remaining solvent is measured, and the residual film rate (=β/α×100)(%) is calculated,
wherein a refractive index (n value) of the cyclic olefin polymer at a wavelength of 193 nm which is measured using the following method 2 is greater than or equal to 1.5 and less than or equal to 2.0,
method 2: a coating film which is formed of the cyclic olefin polymer and has a thickness of 250 nm is formed on a silicon wafer, and the refractive index (n value) of the obtained coating film at a wavelength of 193 nm is set as the refractive index (n value) of the cyclic olefin polymer,
wherein an extinction coefficient (k value) of the cyclic olefin polymer which is measured using the following method 3 is greater than or equal to 0.0001 and less than or equal to 0.5,
method 3: a coating film which is formed of the cyclic olefin polymer and has a thickness of 250 nm is formed on a silicon wafer, and the extinction coefficient (k value) of the obtained coating film is set as the extinction coefficient (k value) of the cyclic olefin polymer,
wherein a flatness ΔFT of a surface (α) of the resist underlayer film on a side opposite to the substrate which is calculated using the following equation is greater than or equal to 0% and less than or equal to 5%.
flatness (ΔFT)=[(Hmax−Hmin)/Hav]×100(%)
where film thicknesses of the resist underlayer film are measured in ten optional sites of the surface (α), an average value of these measured values is set as Hav, a maximum value in the film thicknesses of the resist underlayer film is set as Hmax, and a minimum value in the film thicknesses of the resist underlayer film is set as Hmin,
wherein a content of a crosslinking agent in the material for forming an underlayer film is less than 5 parts by mass in a case where a total content of polymer components contained in the material for forming an underlayer film is set to 100 parts by mass.

### Claim 2 (depends on 1)

The laminate according to claim 1,
wherein an average value Hav of the film thickness of the resist underlayer film is greater than or equal to 5 nm and less than or equal to 1000 nm,
where film thicknesses of the resist underlayer film are measured in ten optional sites of the surface (α) of the resist underlayer film on the side opposite to the substrate, and the average value of these measured values is set as Hav.

### Claim 3 (depends on 1)

The laminate according to claim 1,
wherein the cyclic olefin polymer has a repeating structural unit [A] represented by Formula (1) and a repeating structural unit [B] represented by Formula (2),
a molar ratio [A]/[B] of the structural unit [A] to the structural unit [B] in the cyclic olefin polymer is greater than or equal to 5/95 and less than or equal to 95/5,
in Formula (1), at least one of R1 to R4 is selected from hydrogen, an alkyl group having 1 to 10 carbon atoms, an aryl group having 6 to 20 carbon atoms, an alkoxy group having 1 to 10 carbon atoms, an aryloxy group having 6 to 20 carbon atoms, an alkoxyalkyl group having 2 to 10 carbon atoms, an aryloxyalkyl group having 7 to 20 carbon atoms, an alkoxycarbonyl group having 2 to 20 carbon atoms, a dialkylaminocarbonyl group having 3 to 10 carbon atoms, an aryloxycarbonyl group having 7 to 20 carbon atoms, an alkylarylaminocarbonyl group having 8 to 20 carbon atoms, an alkoxycarbonylalkyl group having 3 to 30 carbon atoms, an alkoxycarbonylaryl group having 8 to 30 carbon atoms, an aryloxycarbonylalkyl group having 8 to 20 carbon atoms, an alkoxyalkyloxycarbonyl group having 3 to 20 carbon atoms, and an alkoxycarbonylalkyloxycarbonyl group having 4 to 30 carbon atoms, R1 to R4 may be bonded to one another to form a ring structure, and n represents an integer of 0 to 2, and
in Formula (2), at least one of R5 to R8 is selected from hydrogen, an alkyl group having 1 to 10 carbon atoms, an aryl group having 6 to 20 carbon atoms, an alkoxy group having 1 to 10 carbon atoms, an aryloxy group having 6 to 20 carbon atoms, an alkoxyalkyl group having 2 to 10 carbon atoms, an aryloxyalkyl group having 7 to 20 carbon atoms, an alkoxycarbonyl group having 2 to 20 carbon atoms, a dialkylaminocarbonyl group having 3 to 10 carbon atoms, an aryloxycarbonyl group having 7 to 20 carbon atoms, an alkylarylaminocarbonyl group having 8 to 20 carbon atoms, an alkoxycarbonylalkyl group having 3 to 30 carbon atoms, an alkoxycarbonylaryl group having 8 to 30 carbon atoms, an aryloxycarbonylalkyl group having 8 to 20 carbon atoms, an alkoxyalkyloxycarbonyl group having 3 to 20 carbon atoms, and an alkoxycarbonylalkyloxycarbonyl group having 4 to 30 carbon atoms, R5 to R8 may be bonded to one another to form a ring structure, n represents an integer of 0 to 2, and X1 represents —O— or —S—.

### Claim 4 (depends on 3)

The laminate according to claim 3,
wherein in Formula (1), n represents 0.

### Claim 5 (depends on 1)

The laminate according to claim 1,
wherein a weight-average molecular weight (Mw) of the cyclic olefin polymer in terms of polystyrene which is measured using gel permeation chromatography is greater than or equal to 1000 and less than or equal to 20000.

### Claim 6 (depends on 1)

The laminate according to claim 1,
wherein a content of the cyclic olefin polymer in the material for forming an underlayer film is greater than or equal to 50% by mass and less than or equal to 100% by mass in a case where a total content of the material for forming an underlayer film is set to 100% by mass.

### Claim 7 (depends on 1)

The laminate according to claim 1,
wherein the substrate has an uneven structure on at least one surface thereof, the resist underlayer film is formed on the uneven structure,
the uneven structure has a height of greater than or equal to 5 nm and less than or equal to 500 nm, and
an interval between projections is greater than or equal to 1 nm and less than or equal to 10 mm.

### Claim 8

A laminate comprising:
a substrate; and
a resist underlayer film containing a material for forming an underlayer film, which is
formed on one surface of the substrate,
wherein the material for forming an underlayer film which is used to form a resist underlayer film used in a multi-layer resist process, the material comprising:
a cyclic olefin polymer,
wherein a residual film rate of the material for forming an underlayer film which is
measured using the following method 4 is greater than or equal to 50% and less than or equal to 100%,
method 4: a coating film which is formed of the material for forming an underlayer film and has a thickness (α) of greater than or equal to 200 nm and less than or equal to 500 nm is formed on a silicon wafer, the obtained coating film is treated at 200° C. for 10 minutes, immersed in propylene glycol-1-monomethyl ether-2-acetate at 23° C. for 10 minutes, and dried under conditions of 150° C. for 3 minutes, and a remaining solvent in the coating film is removed, and a thickness (β) of the coating film obtained by removing the remaining solvent is measured, and the residual film rate (=β/α×100)(%) is calculated,
wherein a refractive index (n value) of the cyclic olefin polymer at a wavelength of 193 nm which is measured using the following method 2 is greater than or equal to 1.5 and less than or equal to 2.0, method 2: a coating film which is formed of the cyclic olefin polymer and has a thickness of 250 nm is formed on a silicon wafer, and the refractive index (n value) of the obtained coating film at a wavelength of 193 nm is set as the refractive index (n value) of the cyclic olefin polymer,
wherein an extinction coefficient (k value) of the cyclic olefin polymer which is measured using the following method 3 is greater than or equal to 0.0001 and less than or equal to 0.5,
method 3: a coating film which is formed of the cyclic olefin polymer and has a thickness of 250 nm is formed on a silicon wafer, and the extinction coefficient (k value) of the obtained coating film is set as the extinction coefficient (k value) of the cyclic olefin polymer,
wherein a flatness ΔFT of a surface (α) of the resist underlayer film on a side opposite to the substrate which is calculated using the following equation is greater than or equal to 0% and less than or equal to 5%.
flatness (ΔFT)=[(Hmax−Hmin)/Hav]×100(%)
where film thicknesses of the resist underlayer film are measured in ten optional sites of the surface (α), an average value of these measured values is set as Hav, a maximum value in the film thicknesses of the resist underlayer film is set as Hmax, and a minimum value in the film thicknesses of the resist underlayer film is set as Hmin,
wherein a content of a crosslinking agent in the material for forming an underlayer film is less than 5 parts by mass in a case where a total content of polymer components contained in the material for forming an underlayer film is set to 100 parts by mass.

### Claim 9 (depends on 8)

The laminate according to claim 8,
wherein the cyclic olefin polymer has a repeating structural unit [A] represented by Formula (1) and a repeating structural unit [B] represented by Formula (2),
a molar ratio [A]/[B] of the structural unit [A] to the structural unit [B] in the cyclic olefin polymer is greater than or equal to 5/95 and less than or equal to 95/5,
in Formula (1), at least one of R1 to R4 is selected from hydrogen, an alkyl group having 1 to 10 carbon atoms, an aryl group having 6 to 20 carbon atoms, an alkoxy group having 1 to 10 carbon atoms, an aryloxy group having 6 to 20 carbon atoms, an alkoxyalkyl group having 2 to 10 carbon atoms, an aryloxyalkyl group having 7 to 20 carbon atoms, an alkoxycarbonyl group having 2 to 20 carbon atoms, a dialkylaminocarbonyl group having 3 to 10 carbon atoms, an aryloxycarbonyl group having 7 to 20 carbon atoms, an alkylarylaminocarbonyl group having 8 to 20 carbon atoms, an alkoxycarbonylalkyl group having 3 to 30 carbon atoms, an alkoxycarbonylaryl group having 8 to 30 carbon atoms, an aryloxycarbonylalkyl group having 8 to 20 carbon atoms, an alkoxyalkyloxycarbonyl group having 3 to 20 carbon atoms, and an alkoxycarbonylalkyloxycarbonyl group having 4 to 30 carbon atoms, R1 to R4 may be bonded to one another to form a ring structure, and n represents an integer of 0 to 2, and
in Formula (2), at least one of R5 to R8 is selected from hydrogen, an alkyl group having 1 to 10 carbon atoms, an aryl group having 6 to 20 carbon atoms, an alkoxy group having 1 to 10 carbon atoms, an aryloxy group having 6 to 20 carbon atoms, an alkoxyalkyl group having 2 to 10 carbon atoms, an aryloxyalkyl group having 7 to 20 carbon atoms, an alkoxycarbonyl group having 2 to 20 carbon atoms, a dialkylaminocarbonyl group having 3 to 10 carbon atoms, an aryloxycarbonyl group having 7 to 20 carbon atoms, an alkylarylaminocarbonyl group having 8 to 20 carbon atoms, an alkoxycarbonylalkyl group having 3 to 30 carbon atoms, an alkoxycarbonylaryl group having 8 to 30 carbon atoms, an aryloxycarbonylalkyl group having 8 to 20 carbon atoms, an alkoxyalkyloxycarbonyl group having 3 to 20 carbon atoms, and an alkoxycarbonylalkyloxycarbonyl group having 4 to 30 carbon atoms, R5 to R8 may be bonded to one another to form a ring structure, n represents an integer of 0 to 2, and X1 represents —O— or —S—.

### Claim 10 (depends on 9)

The laminate according to claim 9,
wherein in Formula (1), n represents 0.

### Claim 11 (depends on 8)

The laminate according to claim 8,
wherein a weight-average molecular weight (Mw) of the cyclic olefin polymer in terms of polystyrene which is measured using gel permeation chromatography is greater than or equal to 1000 and less than or equal to 20000.

### Claim 12 (depends on 8)

The laminate according to claim 8,
wherein a content of the cyclic olefin polymer in the material for forming an underlayer film is greater than or equal to 50% by mass and less than or equal to 100% by mass in a case where a total content of the material for forming an underlayer film is set to 100% by mass.