# US 2023/0183132 A1 · Color control and heat recuperation when producing activated clay

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0183132 A1
- Document ID: US20230183132A1
- Status: Published application
- Kind: A1
- Application number: 17/923,579
- Filed: 2021-04-27
- Published: 2023-06-15
- Earliest claimed: 2020-05-05
- Assignees: FLSmidth A/S
- Applicants: FLSmidth A/S
- Inventors: Rasmus Franklin Momme; Klaus Christian Thorslund
- Web page: https://patentgrep.com/patent/US20230183132A1

## CPC

- C04B 7/12: Natural pozzuolanas; Natural pozzuolana cements; {Artificial pozzuolanas or artificial pozzuolana cements other than those obtained from waste or combustion residues, e.g. burned clay; Treating inorganic materials to improve their pozzuolanic characteristics (cements containing slag C04B7/14)}
- C04B 14/12: Expanded clay
- C04B 14/108: {Shale, slate (colliery shale C04B18/125)}
- C04B 20/04: Heat treatment
- C04B 20/068: {Selection of ingredients added before or during the thermal treatment, e.g. expansion promoting agents or particle-coating materials}
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C04B 2103/0088: {Compounds chosen for their latent hydraulic characteristics, e.g. pozzuolanes}
- F27M 2003/03: Calcining
- Y02P 40/121: Energy efficiency measures, e.g. improving or optimising the production methods
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F27M: INDEXING SCHEME RELATING TO ASPECTS OF THE CHARGES OR FURNACES, KILNS, OVENS OR RETORTS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention relates to a method for producing a supplementary cementitious material for use in a cement product or concrete, the method comprising the steps of activating clay to the supplementary cementitious material at between 600 to 1000 degree Celsius; treating the activated supplementary cementitious material under reduced conditions to form a reduced product and cooling the reduced product to 300-400 degrees Celsius by a quenching process under oxidizing conditions.

## Claims

### Claim 1

A method for producing a supplementary cementitious material for use in a cement product or concrete, the method comprising the steps of
activating clay to the supplementary cementitious material at between 600 to 1000 degree Celsius;
treating the activated supplementary cementitious material, after the activation of clay at a temperature between 600 to 1000 degrees Celsius, under reducing conditions to form a reduced product; and
cooling the reduced product to a temperature in a range of 300 to 500 degrees Celsius, at a cooling rate with an average temperature change in the range of 10 to 100 degrees Celsius/second, by a quenching process under oxidizing conditions to rapidly slow and stop reaction kinetics of iron compounds that else can re-oxidize to Iron (III) species.

### Claim 2 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the reduced product is cooled to 300-400 degrees Celsius by a quenching process under oxidizing conditions.

### Claim 3 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the cooling is performed with a single and/or multi step quench cooling.

### Claim 4 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the quenching process is performed in oxidizing conditions using an oxygen source.

### Claim 5 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein then quenching process is performed in oxidizing conditions using ambient atmospheric air.

### Claim 6 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein said oxygen has a concentration of more than 10 vol % oxygen.

### Claim 7 (depends on 6)

The method for producing a supplementary cementitious material according to claim 6, wherein said oxygen is preheated in a single or multiple stage cyclone cooler, fluid bed cooler or a combination hereof.

### Claim 8 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein said quenching process is performed with an air ratio of 0.01 to 20, such as 0.1 to 10, preferably 0.25 to 4.0 kg air/kg supplementary cementitious material to below 400 degrees Celsius and preferably 300 degrees Celsius.

### Claim 9

The method for producing a supplementary cementitious material according to claim-8, wherein said quenching process is performed with an air ratio of 0.01 to 20, such as 0.1 to 10, preferably 0.25 to 4.0 kg air/kg supplementary cementitious material to below 500 degrees Celsius and preferably 300 degrees Celsius.

### Claim 10 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein heated quenching air containing oxygen, wherein the oxygen concentration in the quenching air is more than 10 vol % oxygen, is recuperated as combustion air in a pyroprocess to lower a specific fuel consumption of the activated supplementary cementitious material, and/or recuperated as drying air for raw material drying.

### Claim 11 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is blended with a cement product, wherein a color of the blended cement composition is perceived grey when 5 to 90% by weight of said cement composition is consisting of said reduced product.

### Claim 12 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is blended with a cement product, wherein a color of the blended cement composition is perceived grey when 5 to 90% by weight of said cement composition is consisting of said reduced product and further comprising an addition of dark color giving material, such as magnetite.

### Claim 13 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is blended with concrete, wherein a color of a concrete composition is perceived grey when 0.5 to 30% by weight of said concrete composition is consisting of said reduced product.

### Claim 14 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is blended with concrete, wherein a color of a concrete composition is perceived grey when 0.5 to 30% by weight of said concrete composition is consisting of said reduced product and further comprising an addition of dark color giving material, such as magnetite.

### Claim 15 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is activated clay.

### Claim 16 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is activated mixed clays or mixture of active clays.

### Claim 17 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is activated shale.

### Claim 18 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is activated mixed shales or mixtures of activated shales.

### Claim 19 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is mixtures of activated clay and activated shale or mixtures thereof.

### Claim 20 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is blended with concrete as a cement substitute or a clinker substitute.

### Claim 21 (depends on 1)

An apparatus (1) utilizing the method according to claim 1, said apparatus comprising:
a fan (2) configured for creating a draft through a preheater;
a filter (3) for collecting product dried clay;
a feed bin (4) for receiving the dried clay;
a crusher/dryer (5) for clay;
one or more cyclone (6) for preheating of the clay;
a calciner/combustion vessel (7) for activating clay to the supplementary cementitious material at a temperature between 600 to 1000 degree Celsius;
a reduction vessel (8) configured to receive the activated clay for color control;
a quenching cyclone (9) and a cooling cyclone (10) configured for cooling the reduced product to a temperature in a range of 300 to 500 degrees Celsius, at a cooling rate with an average temperature change in the range of 10 to 100 degrees Celsius/second, by a quenching process under oxidizing conditions to rapidly slow and stop reaction kinetics of iron compounds that else can re-oxidize to Iron (III) species; and
a fan for cooling (11).

### Claim 22 (depends on 21)

The apparatus according to claim 21, for use to activate clay to a supplementary cementitious material of grey color.

### Claim 23 (depends on 1)

The method for producing a supplementary cementitious material according to claim 1, wherein the supplementary cementitious material is blended with a cement product to obtain a blended cement composition, wherein the blended cement composition comprises 5 to 90% by weight of a calcined supplementary cementitious material.