# US 2023/0178372 A1 · Fin field-effect transistor semiconductor device and method of forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0178372 A1
- Document ID: US20230178372A1
- Status: Published application
- Kind: A1
- Application number: 17/545,209
- Filed: 2021-12-08
- Published: 2023-06-08
- Earliest claimed: 2021-12-08
- Assignees: Texas Instruments Incorporated
- Applicants: Texas Instruments Incorporated
- Inventors: Bhaskar Srinivasan; Walter Scott Idol; Ming-Yeh Chuang; Brian Goodlin
- Web page: https://patentgrep.com/patent/US20230178372A1

## CPC

- H10D 30/65: Lateral DMOS [LDMOS] FETs
- H10P 32/14: within a single semiconductor body or layer in a solid phase; between different semiconductor bodies or layers, both in a solid phase
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/0241: {doping of vertical sidewalls, e.g. using tilted or multi-angled implants}
- H10D 30/0281: {of lateral DMOS [LDMOS] FETs}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 62/393: {Body regions of DMOS transistors or IGBTs (cell layout of DMOS H10D62/127)}
- H10P 32/1412: {through the applied layer}
- H10P 32/171: {being group IV material}
- H10D 62/157: {Impurity concentrations or distributions}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A fin field-effect transistor (“FinFET”) semiconductor device and method of forming the same. In one example, a semiconductor fin is formed over a semiconductor substrate. A conformal dielectric layer is formed on a top and side surfaces of the fin. A doped semiconductor layer is formed over the conformal dielectric layer, the doped semiconductor layer including a dopant. The doped semiconductor layer is heated thereby driving the dopant through the conformal dielectric layer and forming a doped region of the fin.

## Claims

### Claim 1

A method of forming an integrated circuit, comprising:
forming a semiconductor fin over a semiconductor substrate;
forming a conformal dielectric layer on a top and side surfaces of the fin;
forming a doped semiconductor layer over the conformal dielectric layer, the doped semiconductor layer including a dopant;
heating the doped semiconductor layer thereby driving the dopant through the conformal dielectric layer thereby forming a doped region of the fin.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein the conformal dielectric layer is a thermal oxide layer.

### Claim 3 (depends on 1)

The method as recited in claim 1, wherein the doped semiconductor layer includes polysilicon.

### Claim 4 (depends on 1)

The method as recited in claim 1, wherein the dopant includes boron.

### Claim 5 (depends on 1)

The method as recited in claim 1, wherein the conformal dielectric layer has a thickness of about 3.0 nm.

### Claim 6 (depends on 1)

The method as recited in claim 1, wherein the doped semiconductor layer has a thickness of about 40 nm.

### Claim 7 (depends on 1)

The method as recited in claim 1, further comprising forming an undoped semiconductor layer over the doped semiconductor layer and then annealing the doped and undoped semiconductor layers.

### Claim 8 (depends on 7)

The method as recited in claim 7, wherein the doped and undoped semiconductor layers are formed in a furnace, and further comprising performing an air break between the forming the doped dielectric layer and the undoped semiconductor layer.

### Claim 9 (depends on 1)

The method as recited in claim 1, wherein the doped semiconductor layer has an as-formed dopant concentration of about 1e18 cm−3.

### Claim 10 (depends on 1)

The method as recited in claim 1, wherein the doped region is a drift region of a metal-oxide semiconductor (MOS) Fin field-effect transistor (FinFET).

### Claim 11

A method of forming a semiconductor device, comprising:
forming a fin above a substrate;
forming a thermal oxide layer over a top surface and sidewalls of the fin; and
forming a doped layer over the thermal oxide layer, the thermal oxide layer being configured to control a dopant diffusion of the doped layer into the fin.

### Claim 12 (depends on 11)

The method as recited in claim 11 further comprising forming an undoped layer over the doped layer.

### Claim 13 (depends on 12)

The method as recited in claim 12 wherein the undoped layer is an undoped polysilicon layer in a range of 150 nm to 300 nm.

### Claim 14 (depends on 11)

The method as recited in claim 11 wherein the thermal oxide layer is in a range of 2.0 to 5.0 nm.

### Claim 15 (depends on 11)

The method as recited in claim 11 wherein the doped layer is in a range of 20 nm to 100 nm.

### Claim 16 (depends on 11)

The method as recited in claim 11 wherein the doped layer comprises at least one of boron, phosphorus and arsenic.

### Claim 17 (depends on 11)

The method as recited in claim 11 wherein a dopant in the doped layer is diffused into the fin through the thermal oxide layer by a thermal annealing process at 900° C. to 1200° C. for 20 to 50 minutes.

### Claim 18 (depends on 11)

The method as recited in claim 11 further comprising forming the thermal oxide layer at a bottom of a trench proximate the fin and forming the doped layer thereover.

### Claim 19 (depends on 11)

The method e as recited in claim 11 wherein a doping density of the doped layer at the top surface as compared to the sidewalls is within 20 percent.