# US 2023/0175089 A1 · Procedure For Hardening Slides Of A Perforating Press And The Slides Obtained

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0175089 A1
- Document ID: US20230175089A1
- Status: Published application
- Kind: A1
- Application number: 18/061,782
- Filed: 2022-12-05
- Published: 2023-06-08
- Earliest claimed: 2021-12-06
- Assignees: Soenen Technology NV
- Applicants: Soenen Technology NV
- Inventors: Luc DE SUTTER
- Web page: https://patentgrep.com/patent/US20230175089A1

## CPC

- C21D 9/0068: {for particular articles not mentioned below}
- B21D 28/246: {Selection of punches}
- B23C 3/002: {Milling elongated workpieces}
- B23F 1/06: by milling
- B26F 1/02: Perforating by punching, e.g. with relatively-reciprocating punch and bed
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 1/42: Induction heating
- C21D 1/773: under reduced pressure or vacuum
- C21D 8/00: Modifying the physical properties of ferrous metals or ferrous alloys by deformation combined with, or followed by, heat treatment (hardening articles or materials formed by forging or rolling with no further heating beyond that required for the formation C21D1/02)
- C21D 9/32: for gear wheels, worm wheels, or the like
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- B23C 2260/80: Serrations
- C21D 6/00: Heat treatment of ferrous alloys
- C21D 2211/001: Austenite
- C21D 2211/008: Martensite
- C21D 2261/00: Machining or cutting being involved
- Y02P 10/25: Process efficiency
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B21D: WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL (working or processing of wire B21F)
- B23C: MILLING (broaching B23D; broach-milling in making gears B23F; arrangement for copying or controlling B23Q)
- B23F: MAKING GEARS OR TOOTHED RACKS (by stamping B21D; by rolling B21H; by forging or pressing B21K; by casting B22; arrangements for copying or controlling B23Q; machines or devices for grinding or polishing, in general B24B)
- B26F: PERFORATING; PUNCHING; CUTTING-OUT; STAMPING-OUT; SEVERING BY MEANS OTHER THAN CUTTING (marking-out, perforating or making buttonholes A41H25/00; shoemaking A43D; surgery A61B; punching metal B21D; drilling metal B23B; cutting of metal by applying heat locally, e.g. flame cutting, B23K; cutting by abrasive fluid jets B24C5/02; details common to machines for severing B26D; drilling wood B27C; drilling stone B28D; working of plastics or substances in a plastic state B29; making boxes, cartons, envelopes or bags, of paper or similarly worked materials, e.g. metal foil, B31B; of glass C03B; of leather C14B; of textile materials D06H; for light guides G02B6/25; of tickets G07B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to a method of hardening slides of a perforating press comprising providing a steel beam; hardening of the steel beam in a vacuum furnace; tempering the steel beam twice; first straightening of the steel beam at a temperature of 20° C. ± 10° C.; milling of an at least partially continuous sawtooth profile, along a longitudinal direction of the steel beam, on a first side of the steel beam; wherein, after milling the at least partially continuous sawtooth profile on the first side of the steel beam, a second side of the steel beam, lying opposite the first side, is hardened by means of induction currents, after which the steel beam is again tempered twice and after which the steel beam is straightened a second time at a temperature of 20° C. ± 10° C. The invention also relates to a slide for a perforating press hardened according to the method.

## Claims

### Claim 1

Method of hardening slides of a perforating press comprising:
providing a steel beam;
hardening of the steel beam in a vacuum furnace;
tempering the steel beam twice;
first straightening of the steel beam at a temperature of 20° C. ± 10° C.;
milling of an at least partially continuous sawtooth profile, along a longitudinal direction of the steel beam, on a first side of the steel beam;
wherein, after milling the at least partially continuous sawtooth profile on the first side of the steel beam, a second side of the steel beam, lying opposite the first side, is hardened by means of induction currents, after which the steel beam is again tempered twice and after which the steel beam is straightened a second time at a temperature of 20° C. ± 10° C.

### Claim 2 (depends on 1)

Method according to claim 1, wherein steel of the steel beam comprises 0.70 ± 0.10 wt% carbon, 0.20 ± 0.05 wt% silicon, 0.50 ± 0.10 wt% manganese, 5.00 ± 0.50 wt% chromium, 2.30 ± 0.25 wt% molybdenum and 0.50 ± 0.10 wt% vanadium.

### Claim 3 (depends on 1)

Method according to claim 1, wherein before hardening the steel beam in the vacuum furnace, the steel beam is milled all around to remove hammer scale.

### Claim 4 (depends on 1)

Method according to claim 1, wherein the tempering after hardening of the steel beam takes place in the vacuum furnace at a temperature of at least 620° C. and at most 650° C. for a holding time of at least 90 minutes.

### Claim 5 (depends on 4)

Method according to claim 4, wherein the steel beam after tempering has a hardness of at least 40 and at most 50 on the Rockwell C scale.

### Claim 6 (depends on 1)

Method according to claim 1, wherein the steel beam is hardened in the vacuum furnace at a hardening temperature of at least 1000° C. and at most 1050° C.

### Claim 7 (depends on 6)

Method according to claim 6, wherein the steel beam is heated in the vacuum furnace for a period of at least 3 hours and at most 5 hours from a temperature of 20° C. ± 10° C. to the hardening temperature, after which the steel beam after reaching of the hardening temperature remains in the furnace for at least 30 minutes at the hardening temperature ±10%.

### Claim 8 (depends on 1)

Method according to claim 1, wherein the tempering after hardening of the second side of the steel beam by means of induction currents takes place at a temperature of at least 520° C. and at most 540° C.

### Claim 9 (depends on 8)

Method according to claim 8, wherein the second side of the steel beam, after tempering to a depth of at least 3 mm, measured from the second side, has a hardness of at least 60 on the Rockwell C scale.

### Claim 10 (depends on 1)

Method according to claim 1, wherein all sides with the exception of the first side are finished smoothly before applying the at least partially continuous sawtooth profile to the first side.

### Claim 11 (depends on 1)

Method according to claim 1, wherein when the at least partially continuous sawtooth profile is applied to the first side, at least 0.5 mm and at most 1.5 mm extra material remains on the sawtooth profile, the extra material being removed during smooth finishing of the first side after hardening of the second side of the steel beam by means of induction currents.

### Claim 12 (depends on 1)

Method according to claim 1, wherein after the first straightening of the steel beam, the steel beam has a curvature along the longitudinal direction of the steel beam of at most 3 mm per meter.

### Claim 13 (depends on 1)

Method according to claim 1, wherein after the second straightening of the steel beam, the steel beam has a curvature along the longitudinal direction of at most 0.5 mm per meter of the steel beam.

### Claim 14 (depends on 1)

Slide for a perforating press, comprising a beam-shaped steel body, wherein the beam-shaped steel body extends in a longitudinal direction, wherein the beam-shaped steel body comprises on a first side an at least partially continuous sawtooth profile according to a longitudinal direction of the steel beam, wherein the slide has been hardened by a method according to claim 1.