# US 2023/0175087 A1 · Method for producing liquid pig iron from a DRI product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0175087 A1
- Document ID: US20230175087A1
- Status: Published application
- Kind: A1
- Application number: 17/922,236
- Filed: 2021-03-02
- Published: 2023-06-08
- Earliest claimed: 2020-04-30
- Assignees: SMS group GmbH
- Applicants: SMS group GmbH
- Inventors: Jochen SCHLÜTER; Ralf NÖRTHEMANN; Thomas HENKEL; Paul TOCKERT
- Web page: https://patentgrep.com/patent/US20230175087A1

## CPC

- C21B 13/12: in electric furnaces
- C21B 5/04: Making slag of special composition
- C21B 13/0006: {obtaining iron or steel in a molten state}
- C21B 13/0013: {introduction of iron oxide into a bath of molten iron containing a carbon reductant}
- C21B 13/008: {Use of special additives or fluxing agents}
- C21B 13/143: {Injection of partially reduced ore into a molten bath}
- C21B 2400/062: Jet nozzles or pressurised fluids for cooling, fragmenting or atomising slag
- Y02P 10/134: by avoiding CO2, e.g. using hydrogen
- Y02P 10/20: Recycling
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for producing liquid pig iron comprises: i) providing a DRI product with an iron content of at least 75.0 wt. %, a carbon content of at least 0.10 wt. % and a content of acidic and basic slag components, comprising CaO, SiO2, MgO and Al2O3 of max. 15.0 wt. %; ii) supplying the DRI product, adding slag formers, into an electrically operated smelting unit; iii) optionally supplying further iron and/or carbon components into the electrically operated smelting unit; iv) smelting the DRI product and optionally the further iron and/or carbon components in the presence of the slag formers, so that a liquid pig iron phase and a liquid slag phase are formed; v) adjusting the slag phase such that it has a basicity of (CaO+MgO/SiO2) from 0.95 to 1.5; vi) tapping the liquid pig iron phase; and vii) tapping and granulating the slag phase.

## Claims

### Claim at position 1

-21. (canceled)

### Claim 22

A method for producing liquid pig iron, comprising:
i) providing a directly reduced iron product (1) (DRI product) with an iron content of at least 75.0 wt. %, a carbon content of at least 0.10 wt. %, and a content of acidic and basic slag components, selected from the group consisting of CaO, SiO2, MgO and Al2O3, of max. 15.0 wt. %;
ii) supplying the DRI product (1) and slag formers (2) into an electrically operated smelting unit (3);
iii) optionally supplying further iron and/or carbon components (5) into the electrically operated smelting (3) unit;
iv) smelting the DRI product (1) and optionally the further iron and/or carbon components (5) in presence of the slag formers (2), so that a liquid pig iron phase (6) and a liquid slag phase (7) are formed;
v) adjusting the slag phase (7) such that it has a basicity of (CaO+MgO/SiO2) from 0.95 to 1.5;
vi) tapping the liquid pig iron phase (6); and
vii) tapping and granulating the slag phase (7).

### Claim 23 (depends on 22)

The method according to claim 22,
wherein the slag phase (7) is adjusted such that it has a basicity of (CaO+MgO/SiO2) from 1.0 to 1.25.

### Claim 24 (depends on 22)

The method according to claim 22,
wherein the slag phase (7) is adjusted such that it has a viscosity of 0.30 to 0.50 Pa*s.

### Claim 25 (depends on 22)

The method according to claim 22,
wherein the slag phase (7) is tapped at a tapping temperature in the range from 1300° C. to 1600° C.

### Claim 26 (depends on 22)

The method according to claim 22,
wherein the slag formers (2) are selected from the group consisting of CaO, SiO2, MgO, Al2O3, and mixed oxides thereof.

### Claim 27 (depends on 22)

The method according to claim 22,
wherein the slag formers (2) in accordance with step ii) are supplied up to a fraction of max. 10.0 wt. %, based on an amount of the DRI product.

### Claim 28 (depends on 22)

The method according to claim 22,
wherein the iron and/or carbon components (5) in accordance with step iii) are supplied up to a fraction of max. 20.0 wt. %, based on an amount of the DRI product.

### Claim 29 (depends on 22)

The method according to claim 22,
wherein granulation is carried out as wet or dry granulation.

### Claim 30 (depends on 22)

The method according to claim 22,
wherein supplying the slag formers (2) is carried out automatically via a process model integrated into a plant automation system, and
wherein a quantity of the slag formers (2) is calculated by the process model and determined as a function of process parameters.

### Claim 31 (depends on 22)

The method according to claim 22,
wherein the directly reduced iron product (1) is supplied to the smelting unit (3)
in hot form as HDRI product,
in cold form as CDRI product,
in hot briquette form as HBI product and/or
in particulate form with an average particle diameter of max. 10.0 mm.

### Claim 32 (depends on 22)

The method according to claim 22,
wherein the liquid pig iron phase (6) formed in accordance with step iv) is carburized to a carbon content of at least 2.50 wt. %.

### Claim 33 (depends on 22)

The method according to claim 22,
wherein the DRI product (1) and/or the slag formers (2) are supplied to the smelting unit (3) from a thermally insulated bunker reservoir (15).

### Claim 34 (depends on 22)

The method according to claim 22,
wherein the DRI product (1) is produced in a direct reduction plant (11) and is supplied to the smelting unit (3) and/or a bunker reservoir (15) under a protective gas atmosphere via a conveying device (14).

### Claim 35 (depends on 22)

A granulated slag obtained by the method according to claim 22, comprising:
35.0-40.0 wt. % SiO2,
30.0-43.0 wt. % CaO,
8.0-12.0 wt. % Al2O3,
4.0-12.0 wt. %- MgO,
along with unavoidable impurities comprising iron (Fe), MnO2 and/or sulfur (S).

### Claim 36 (depends on 35)

The granulated slag according to claim 35,
wherein a total content of SiO2, CaO and MgO amounts to at least 70.0 wt. %.

### Claim 37 (depends on 35)

The granulated slag according to claim 35, comprising
a vitreous solidification fraction of at least 95.0 wt. %, and
a total iron content of max. 1.0 wt. %.

### Claim 38 (depends on 35)

The granulated slag according to any claim 35, having an eluate allocation value of 0 or 1.

### Claim 39

A plant (10) for producing liquid pig iron, comprising:
a direct reduction plant (11) for producing a directly reduced iron product (1);
an electrically operated smelting unit (3) in which the directly reduced iron product (1) can be smelted; and
a conveying device (14) via which the directly reduced iron product (1) can be transported from the direct reduction plant (11) to the smelting unit (3).

### Claim 40 (depends on 39)

The plant (10) according to claim 39,
wherein the smelting unit (3) is an electric arc furnace (EAF), a submerged arc furnace (SAF), or an induction furnace (IF).

### Claim 41 (depends on 39)

The plant (10) according to claim 39,
wherein the conveying device (14) is a metal conveyor belt with a protective gas atmosphere.

### Claim 42 (depends on 39)

The plant (10) according to claim 39, further comprising a thermally insulated bunker reservoir (15).