# US 2023/0159389 A1 · Magnesium-based cementitious material, preparation method and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0159389 A1
- Document ID: US20230159389A1
- Status: Published application
- Kind: A1
- Application number: 17/941,047
- Filed: 2022-09-09
- Published: 2023-05-25
- Earliest claimed: 2021-11-19
- Assignees: Wuhan University of Technology
- Applicants: Wuhan University of Technology
- Inventors: Fazhou Wang; Zhichao Liu; Shuguang Hu
- Web page: https://patentgrep.com/patent/US20230159389A1

## CPC

- C04B 9/11: Mixtures thereof with other inorganic cementitious materials
- C04B 28/105: {Magnesium oxide or magnesium carbonate cements}
- C04B 9/20: Manufacture, e.g. preparing the batches (preheating, burning, calcining or cooling lime stone, magnesite or dolomite C04B2/10)
- C04B 2111/00068: {Mortar or concrete mixtures with an unusual water/cement ratio}
- C04B 2111/00215: {Mortar or concrete mixtures defined by their oxide composition}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Disclosed is a magnesium-based cementitious material, preparation method and application thereof. The magnesium-based cementitious material, comprising magnesite, sandstone, and water, wherein: the magnesite is provided with CaO, SiO2, Al2O3, Fe2O3, and MgO, a mass percentage of the CaO is less than 5%, a mass percentage of SiO2 is less than 5%, a mass percentage of Al2O3 is less than 5%, a mass percentage of Fe2O3 is less than 7%, a mass percentage of MgO is between 37% and 50%; the sandstone is provided with SiO2, CaO, Al2O3, and Fe2O3, a mass percentage of SiO2 is greater than 70%. The beneficial effects of this disclosure are: the cementitious material does not contain MgCl2, which avoids the reduction of the strength of the cementitious material due to the dissolution of MgCl2 in water; the magnesium-based cementitious material of this disclosure is immiscible with water and has strong water resistance.

## Claims

### Claim at position 1

1-3. (canceled)

### Claim 4

A preparation method for a magnesium-based cementitious material, comprising the following steps:
mixing magnesite and sandstone to obtained a mixture, and processing the mixture by molding to obtain a molded raw meal; wherein the magnesite is provided with CaO, SiO2, Al2O3, Fe2O3, and MgO, a mass percentage of the CaO is less than 5%, a mass percentage of SiO2 is less than 5%, a mass percentage of Al2O3 is less than 5%, a mass percentage of Fe2O3 is less than 7%, a mass percentage of MgO is between 37% and 50%; the sandstone is provided with SiO2, CaO, Al2O3, and Fe2O3, a mass percentage of SiO2 is greater than 70%, a mass percentage of CaO is less than 10%, a mass percentage of Al2O3 is less than 10%, and a mass percentage of Fe2O3 is less than 5%; and a mass ratio of the magnesite to the sandstone is 65-75:25-35;
calcining the molded raw meal to obtain a clinker;
mixing and shaping the clinker with water to obtain a primary cementitious material;
subjecting the primary cementitious material to carbonization curing to obtain the magnesium-based cementitious material.

### Claim 5 (depends on 4)

The preparation method for the magnesium-based cementitious material according to claim 4, the calcination comprises a first calcination and a second calcination that are sequentially performed; wherein the temperature of the first calcination is at a range of 830˜950° C. with a calcination time of 0.5˜1 h; the temperature of the second calcination is at a range of 1120˜1350° C. with a calcination time of 0.5˜3 h.

### Claim 6 (depends on 4)

The preparation method for the magnesium-based cementitious material according to claim 4, wherein the mass ratio of the clinker and water is 1:(0.1˜0.4).

### Claim 7 (depends on 4)

The preparation method for the magnesium-based cementitious material according to claim 4, wherein the molding comprises pressing or casting.

### Claim 8 (depends on 4)

The preparation method for the magnesium-based cementitious material according to claim 4, wherein the conditions of the carbonization curing are as follows: CO2 concentration of 20˜99%, gas pressure of 0.1˜0.4 MPa, relative humidity of 10˜99%, temperature of −20˜120° C., and carbonization curing time of 10 minutes to 28 days.

### Claim 9

(canceled)

### Claim 10 (depends on 4)

The preparation method for the magnesium-based cementitious material according to claim 4, wherein in the magnesite, the mass percentage of CaO is 0.89%, the mass percentage of SiO2 is 1.23%, the mass percentage of Al2O3 is 2.880%, the mass percentage of Fe2O3 is 5.75%, and the mass of MgO is 43.025%.

### Claim 11 (depends on 4)

The preparation method for the magnesium-based cementitious material according to claim 4, wherein in the magnesite, the mass percentage of SiO2 is 74.887%, the mass percentage of CaO is 5.366%, the mass percentage of Al2O3 is 8.142%, the mass percentage of Fe2O3 is 3.406%, and the mass percentage of MgO is 1.223%.