# US 2023/0155169 A1 · Method for producing an electrolytic copper foil

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0155169 A1
- Document ID: US20230155169A1
- Status: Published application
- Kind: A1
- Application number: 18/097,573
- Filed: 2023-01-17
- Published: 2023-05-18
- Earliest claimed: 2019-04-30
- Assignees: Nan Ya Plastics Corporation
- Applicants: Nan Ya Plastics Corporation
- Inventors: CHIA-LING CHEN; MING-JEN TZOU
- Web page: https://patentgrep.com/patent/US20230155169A1

## CPC

- C25D 1/04: Wires; Strips; Foils
- H01M 10/0562: Solid materials
- C25D 3/38: of copper
- C25D 5/10: Electroplating with more than one layer of the same or of different metals (for bearings C25D7/10)
- C25D 7/0614: {Strips or foils}
- H01M 4/0438: {by electrochemical processing (electroless electrochemical plating C23C18/54)}
- H01M 4/045: {Electrochemical coating; Electrochemical impregnation}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C25D 3/04: of chromium
- C25D 3/12: of nickel or cobalt
- C25D 3/22: of zinc
- C25D 3/42: of light metals
- C25D 3/54: of metals not provided for in groups C25D3/04 - C25D3/50
- C25D 5/12: at least one layer being of nickel or chromium
- C25D 5/14: two or more layers being of nickel or chromium, e.g. duplex or triplex layers
- H01M 10/0563: Liquid materials, e.g. for Li-SOCl2 cells
- H01M 10/0566: Liquid materials
- Y02E 60/10: Energy storage using batteries
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for producing an electrolytic copper foil is provided. The method includes preparing a copper electrolytic solution including at least one addition agent and performing an electroplating step including: electrolyzing the copper electrolytic solution to form a raw foil layer. The raw foil layer has a first surface and a second surface opposite to the first surface. In the X-ray diffraction spectrum of the first surface, a ratio of the diffraction peak intensity I(200) of the (200) crystal face of the first surface relative to the diffraction peak intensity I(111) of the (111) crystal face of the first surface is between 0.5 and 2.0. A ratio of the diffraction peak intensity I(200) of the (200) crystal face of the second surface relative to the diffraction peak intensity I(111) of the (111) crystal face of the second surface is between 0.5 and 2.0.

## Claims

### Claim 1

A method for producing an electrolytic copper foil, comprising:
preparing a copper electrolytic solution including at least one addition agent; wherein based on a total weight of the copper electrolytic solution, a concentration of the at least one addition agent is not more than 12 ppm; and
performing an electroplating step including: electrolyzing the copper electrolytic solution to form a raw foil layer;
wherein the raw foil layer has a first surface and a second surface opposite to the first surface;
wherein in the X-ray diffraction spectrum of the first surface, a ratio of the diffraction peak intensity I(200) of the (200) crystal face of the first surface relative to the diffraction peak intensity I(111) of the (111) crystal face of the first surface is between 0.5 and 2.0;
wherein in the X-ray diffraction spectrum of the second surface, a ratio of the diffraction peak intensity I(200) of the (200) crystal face of the second surface relative to the diffraction peak intensity I(111) of the (111) crystal face of the second surface is between 0.5 and 2.0.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the at least one addition agent includes a first addition agent, a second addition agent, and a third addition agent; wherein the first addition agent is a gelatin, the second addition agent is sulfonic acid or sulfonate which has a sulfur compound, and the third addition agent is a nonionic water soluble polymer.

### Claim 3 (depends on 2)

The method according to claim 2, wherein in the copper electrolytic solution, a sum of concentrations of the first addition agent, the second addition agent, and the third addition agent is not more than 12 ppm.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the gelatin has a weight average molecular weight between 1,000 and 5,000.

### Claim 5 (depends on 1)

The method according to claim 1, further comprising:
performing an anti-oxidation treatment step which includes: forming a first oxidation resistant layer on the first surface of the raw foil layer, and forming a second oxidation resistant layer on the second surface of the raw foil layer, such that the raw foil layer, the first oxidation resistant layer, and the second oxidation resistant layer are collectively formed into an electrolytic copper foil;
wherein based on a total weight of the electrolytic copper foil, each of the first oxidation resistant layer and the second oxidation resistant layer includes a non-copper metal element in an amount ranging from 1 ppm to 1,000 ppm; wherein the non-copper metal element is at least one element selected from the group consisting of chromium, zinc, nickel, molybdenum, manganese, phosphorus, and combinations thereof.