# US 2023/0155159 A1 · Lamination Device and Method for Discharging Defective Electrode Cell Assembly of Lamination Device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0155159 A1
- Document ID: US20230155159A1
- Status: Published application
- Kind: A1
- Application number: 17/917,677
- Filed: 2022-01-28
- Published: 2023-05-18
- Earliest claimed: 2021-02-04
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Hyun Jae Park; Ha Yong Jung; Jong Myung Lee; Gyu Hwan Choe; Kyu Sang Lee
- Web page: https://patentgrep.com/patent/US20230155159A1

## CPC

- H01M 10/0404: {Machines for assembling batteries}
- G01B 11/026: {by measuring distance between sensor and object (G01B11/0608 takes precedence)}
- G01B 11/06: for measuring thickness {; e.g. of sheet material (thickness measurement by thermal means G01B21/085)}
- G01N 21/95: characterised by the material or shape of the object to be examined (G01N21/89 - G01N21/91, G01N21/94 take precedence)
- B32B 41/00: Arrangements for controlling or monitoring lamination processes; Safety arrangements
- G01B 11/022: {by means of tv-camera scanning}
- G01B 11/0691: {of objects while moving (G01B11/0616 takes precedence)}
- G01B 2210/44: with detectors on both sides of the object to be measured
- G01B 2210/50: Using chromatic effects to achieve wavelength-dependent depth resolution
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- G01B: MEASURING LENGTH, THICKNESS OR SIMILAR LINEAR DIMENSIONS; MEASURING ANGLES; MEASURING AREAS; MEASURING IRREGULARITIES OF SURFACES OR CONTOURS
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A lamination apparatus configured to manufacture an electrode cell assembly may include a lamination part configured to manufacture the electrode cell assembly through lamination, an inspection part configured to detect a defective electrode cell assembly by measuring a thickness of the manufactured electrode cell assembly, a discharge part configured to separate and discharge the defective electrode cell assembly from a normal electrode cell assembly, and a control part configured to perform control so as to calculate a time point at which the defective electrode cell assembly reaches the discharge part on the basis of distance data between a point at which the defective electrode cell assembly is detected and the discharge part and separate and discharge the defective electrode cell assembly when the defective electrode cell assembly reaches the discharge part. A method of discharging a defective electrode cell assembly by the lamination apparatus is also disclosed.

## Claims

### Claim 1

A lamination apparatus for manufacturing an electrode cell assembly by laminating an electrode and a separator respectively unwound from an electrode roll and a separator roll, the lamination apparatus comprising:
a lamination part configured to laminate the electrode cell assembly;
an inspection part configured to detect a defective electrode cell assembly by measuring a thickness of the electrode cell assembly;
a discharge part configured to separate the defective electrode cell assembly from the lamination apparatus and to discharge the defective electrode cell assembly from the lamination apparatus; and
a control part configured to calculate a time point at which the defective electrode cell assembly reaches the discharge part on the basis of distance data between a point at which the defective electrode cell assembly is detected and the discharge part and separate, the control part configured to discharge the defective electrode cell assembly when the defective electrode cell assembly reaches the discharge part.

### Claim 2 (depends on 1)

The lamination apparatus of claim 1, further comprising a conveyor configured to receive the electrode assembly thereon, wherein the time point at which the defective electrode cell assembly reaches the discharge part is obtained by dividing the distance data by a conveying speed of a conveyor.

### Claim 3 (depends on 1)

The lamination apparatus of claim 1, further comprising a conveyor driving part configured to convey the electrode cell assembly and an encoder installed at the conveyor driving part, wherein the distance data is detected by the encoder.

### Claim 4 (depends on 1)

The lamination apparatus of claim 1, wherein the inspection part includes a thickness measuring part configured to measure a thickness of the electrode cell assembly and a vision inspection part configured to inspect at least one of an appearance, a shape, and dimensions of the electrode cell assembly.

### Claim 5 (depends on 4)

The lamination apparatus of claim 4, wherein the thickness measuring part is installed before the vision inspection part in a conveying direction of the lamination apparatus.

### Claim 6 (depends on 1)

The lamination apparatus of claim 1, wherein the lamination apparatus is configured to measure the thickness of the battery cell assembly in a non-contact manner.

### Claim 7 (depends on 6)

The lamination apparatus of claim 6, further comprising a confocal thickness sensor configured to measure the thickness of the battery cell assembly.

### Claim 8 (depends on 7)

The lamination apparatus of claim 7, wherein the confocal thickness sensor is installed on a stage configured to move in three dimensions.

### Claim 9 (depends on 7)

The lamination apparatus of claim 7, wherein the confocal thickness sensor is an upper confocal thickness sensor, the apparatus further comprising a lower confocal thickness sensor, the upper and lower confocal thickness sensors being respectively disposed above and below a conveyor configured to receive the electrode cell assembly thereon, and
the apparatus is configured to measure the thickness of the electrode cell assembly by calculating a difference of a distance between the electrode cell assembly and the upper confocal thickness sensor disposed thereabove and a distance between the electrode cell assembly and the lower confocal thickness sensor disposed therebelow.

### Claim 10 (depends on 9)

The lamination apparatus of claim 9, wherein the upper and lower confocal thickness sensors are mounted on a same bracket, and the same bracket is installed on a stage configured to move in three dimensions.

### Claim 11 (depends on 1)

The lamination apparatus of claim 1, wherein the control part is configured to discharge one electrode cell assembly adjacent to the defective electrode cell assembly together with the defective electrode cell assembly.

### Claim 12

A method of discharging a defective electrode cell assembly using a lamination apparatus, the method comprising:
detecting the defective electrode cell assembly by measuring a thickness of the defective electrode cell assembly after the electrode and the separator are laminated to form the defective electrode cell assembly;
calculating a time point at which the defective electrode cell assembly reaches a discharge part of the lamination apparatus on the basis of distance data between a point at which the defective electrode cell assembly is detected and the discharge part; and
separating and discharging the defective electrode cell assembly from a normal electrode cell assembly at the time point at which the defective electrode cell assembly reaches the discharge part.

### Claim 13 (depends on 12)

The method of claim 12, wherein the time point at which the defective electrode cell assembly reaches the discharge part is obtained by dividing the distance data by a conveying speed of a conveyor of the lamination apparatus.

### Claim 14 (depends on 12)

The method of claim 12, wherein the distance data is detected by an encoder installed at a conveyor driving part of the lamination apparatus configured to convey the defective electrode cell assembly.

### Claim 15 (depends on 12)

The method of claim 12, wherein the thickness of the defective electrode cell assembly is measured in a non-contact manner.

### Claim 16 (depends on 15)

The method of claim 15, wherein the thickness of the defective electrode cell assembly is measured by a confocal thickness sensor.

### Claim 17 (depends on 16)

The method of claim 16, wherein the confocal thickness sensor is movable in at least one of a vertical direction and a horizontal direction.

### Claim 18 (depends on 17)

The method of claim 17, wherein the confocal thickness sensor is an upper confocal thickness sensor, the lamination apparatus has a lower confocal thickness sensor, and the upper and lower confocal thickness sensors are respectively disposed above and below the electrode cell assembly, and
the thickness of the electrode cell assembly is measured by a difference of a distance between the defective electrode cell assembly and the upper confocal thickness sensor disposed thereabove and a distance between the defective electrode cell assembly and the lower confocal thickness sensor disposed therebelow.

### Claim 19 (depends on 12)

The method of claim 12, wherein the normal electrode cell assembly adjacent to the defective electrode cell assembly is discharged together with the defective electrode cell assembly.