- Applicants: LG Energy Solution, Ltd.
- Inventors: Hyunwoong YUN; Sunwook HWANG; Hoejin HAH
- Web page: https://patentgrep.com/patent/US20230155134A1

## CPC

- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 4/623: {fluorinated polymers}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/663: {containing carbon or carbonaceous materials as conductive part, e.g. graphite, carbon fibres}
- H01M 4/668: {Composites of electroconductive material and synthetic resins}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- H01M 10/0568: characterised by the solutes
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0025: Organic electrolyte
- H01M 2300/0037: Mixture of solvents
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode current collector for a lithium secondary battery includes a tab extending from a positive electrode current collector substrate. An anti-corrosion layer made of one selected from the group consisting of a primer layer, a conductive polymer layer, and a conductive epoxy layer is formed over the entire surface of the tab. A positive electrode of a lithium secondary battery includes the positive current collector.

## Claims

### Claim 1

A positive electrode current collector for a lithium secondary battery comprising:
a tab and a positive electrode current collector substrate, the tab extending from the positive electrode current collector substrate; and
an anti-corrosion layer made of a layer selected from the group consisting of a primer layer, a conductive polymer layer, and a conductive epoxy layer, the anti-corrosion layer is being formed over the entire surface of the tab.

### Claim 2 (depends on 1)

The positive electrode current collector according to claim 1,
wherein the anti-corrosion layer is additionally formed on a part or the entire surface of at least one surface of the positive electrode current collector substrate.

### Claim 3 (depends on 1)

The positive electrode current collector according to claim 1, wherein the primer layer includes:
at least one conductive material selected from the group consisting of natural graphite, artificial graphite, graphene, carbon black, channel black, furnace black, lamp black, thermal black, carbon nanotube, graphite nanofiber, carbon nanofiber, aluminum, nickel, and a polyphenylene derivative; and
a binding material.

### Claim 4 (depends on 3)

The positive electrode current collector according to claim 3, wherein the binding material is at least one binding material selected from the group consisting of polyvinylidene fluoride, polyvinyl alcohol, carboxymethylcellulose (CMC), starch, hydroxypropylcellulose, regenerated cellulose, polyvinylpyrrolidone, tetrafluoroethylene, polyethylene, polypropylene, ethylene-propylene-diene terpolymer (EPDM), sulfonated EPDM, styrene butylene rubber, and fluorine rubber.

### Claim 5 (depends on 3)

The positive electrode current collector according to claim 3, wherein a range of a weight ratio between the conductive material and the binding material is 1:99 to 99:1.

### Claim 6 (depends on 1)

The positive electrode current collector according to claim 1, wherein the conductive polymer layer includes at least one conductive polymer selected from the group consisting of poly(3,4-ethylenedioxythiophene)/poly(4-styrene sulfonate) (PEDOT/PSS), polyaniline (PANI), polypyrrole (PPy), polythiophene (PT), polyacetylene (PA), and poly para-phenylene vinylene (PPV).

### Claim 7 (depends on 1)

The positive electrode current collector according to claim 1, wherein the conductive epoxy layer includes:
at least one conductive filler selected from the group consisting of metal powder of gold, platinum, silver, copper, or nickel; carbon or carbon fiber, graphite; and composite powder thereof; and
a binder.

### Claim 8 (depends on 7)

The positive electrode current collector according to claim 7, wherein the binder is at least one material selected from the group consisting of acrylic-based, epoxy-based, polyurethane-based, silicon-based, polyimide-based, phenolic-based, or polyester-based polymer material, composite polymer resins thereof, and low melting point glass.

### Claim 9 (depends on 7)

The positive electrode current collector according to claim 7, wherein a range of a weight ratio between the conductive filler and the binder is 1:99 to 99:1.

### Claim 10 (depends on 1)

The positive electrode current collector according to claim 1, wherein a thickness of the anti-corrosion layer is 0.1 μm to 100 μm.

### Claim 11 (depends on 1)

The positive electrode current collector according to claim 1, wherein the positive electrode current collector includes aluminum (Al).

### Claim 12 (depends on 1)

A positive electrode having a positive electrode mixture layer formed on at least one surface of the positive electrode current collector according to claim 1.

### Claim 13 (depends on 12)

A battery including an electrode assembly is impregnated with a lithium non-aqueous electrolyte, the electrode assembly comprising:
the positive electrode according to claim 12;
a negative electrode having a negative electrode mixture layer formed on at least one surface of a negative electrode current collector; and
a separator interposed between the positive electrode and negative electrode.

### Claim 14 (depends on 13)

The battery according to claim 13, wherein the lithium non-aqueous electrolyte includes a lithium salt and a non-aqueous solvent, and
wherein the lithium salt includes an imide-based salt selected from the group consisting of lithium bis(fluorosulfonyl)imide (LiFSI), lithium bis(trifluoromethanesulfonyl)imide (LiTFSI), lithium bis(perfluoroethylsulfonyl)imide (LiBETI), lithium (fluorosulfonyl)(nonafluorobutanesulfoyl)imide (LiFNFSI), and lithium (fluorosulfonyl)(trifluoromethanesulfonyl)imide (LiFTI or LiFTA).

### Claim 15 (depends on 13)

The battery according to claim 13, wherein the battery is a lithium ion battery, a lithium polymer battery, a lithium metal battery, or a lithium-free battery.

### Claim 16

A battery comprising:
a positive electrode including a current collector substrate and a tab coupled to one end of the current collector substrate;
a negative electrode; and
a separator between the positive electrode and the negative electrode,
wherein the tab includes an anti-corrosion layer formed on a surface of the tab.

### Claim 17 (depends on 16)

The battery of claim 16, wherein the current collector substrate includes the anti-corrosion layer formed on a surface of the current collector substrate.

### Claim 18 (depends on 16)

The battery of claim 16, wherein the anti-corrosion layer is formed on the entire surface of the tab.

### Claim 19

An electrode assembly comprising:
a positive electrode including a current collector substrate and a tab coupled to one end of the current collector substrate;
a negative electrode; and
a separator between the positive electrode and the negative electrode,
wherein the tab includes an anti-corrosion layer formed on a surface of the tab.

### Claim 20 (depends on 16)

The battery of claim 16, wherein the current collector substrate includes the anti-corrosion layer formed on a surface of the current collector substrate.