# US 2023/0155133 A1 · Lithium metal negative electrode and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0155133 A1
- Document ID: US20230155133A1
- Status: Published application
- Kind: A1
- Application number: 17/525,096
- Filed: 2021-11-12
- Published: 2023-05-18
- Earliest claimed: 2021-11-12
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Kanako Okada; Jesse M. Roy; Li Yang; Mary E. Fortier
- Web page: https://patentgrep.com/patent/US20230155133A1

## CPC

- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 4/0402: {Methods of deposition of the material}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/366: {as layered products}
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0025: Organic electrolyte
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A negative electrode for an electrochemical cell of a secondary lithium metal battery is manufactured by a method in which a precursor solution is applied to a major surface of a lithium metal substrate to form a protective interfacial layer thereon. The precursor solution includes a first organic solvent mixture, a dioxolane, and a fluorinated organosilane. The protective interfacial layer exhibits a composite structure including a polymeric matrix component and a lithium-containing dispersed component embedded in the polymeric matrix component.

## Claims

### Claim 1

A method of manufacturing a negative electrode for an electrochemical cell of a secondary lithium metal battery, the method comprising:
applying a precursor solution to a major surface of a lithium metal substrate to form a protective interfacial layer thereon,
wherein the precursor solution includes an organic solvent mixture, a dioxolane, and a fluorinated organosilane, and
wherein the protective interfacial layer exhibits a composite structure including a polymeric matrix component and a lithium-containing dispersed component embedded in the polymeric matrix component.

### Claim 2 (depends on 1)

The method of claim 1 wherein the dioxolane is a chemical compound that contains a dioxolane ring.

### Claim 3 (depends on 1)

The method of claim 1 wherein the dioxolane is 1,3-dioxolane.

### Claim 4 (depends on 1)

The method of claim 1 wherein the dioxolane is included in the precursor solution in an amount constituting, by weight, 1% to 60% of the precursor solution.

### Claim 5 (depends on 1)

The method of claim 1 wherein the fluorinated organosilane is a chemical compound having the formula: R′R″nSiX4-n, wherein n=0, 1, or 2, and wherein R′ is a polyfluorinated C1-C8 alkyl group, R″ is a methyl group, and X is a methoxy group or a chlorine atom.

### Claim 6 (depends on 5)

The method of claim 5 wherein the fluorinated organosilane is at least one of (3,3,3-trifluoropropylmethyl)dimethoxysilane, (3,3,3-Trifluoropropyl)trimethoxysilane, 1H,1H,2H,2H-perfluorooctylmethyldimethoxysilane, 1H,1H,2H,2H-perfluorooctyltrimethoxysilane, 1H,1H,2H,2H-perfluorooctyldimethylchlorosilane, 1H,1H,2H,2H-perfluorooctylmethyldichlorosilane, (1H,1H,2H,2H-perfluoro-n-hexyl)methyldichlorosilane, or 1H,1H,2H,2H-perfluorooctyltrichlorosilane.

### Claim 7 (depends on 1)

The method of claim 1 wherein the fluorinated organosilane is included in the precursor solution in an amount constituting, by weight, 1% to 10% of the precursor solution.

### Claim 8 (depends on 1)

The method of claim 1 wherein the organic solvent mixture comprises a mixture of an acyclic ether and a cyclic ether.

### Claim 9 (depends on 8)

The method of claim 8 wherein the organic solvent mixture comprises a mixture of 1,2-dimethoxyethane and tetrahydrofuran.

### Claim 10 (depends on 1)

The method of claim 1 wherein the polymeric matrix component is chemically bonded to the major surface of the lithium metal substrate via a plurality of silicon-oxygen bonds and/or alkoxide bonds.

### Claim 11 (depends on 1)

The method of claim 1 wherein the polymeric matrix component comprises a plurality of siloxane bonds.

### Claim 12 (depends on 1)

The method of claim 1 wherein the lithium-containing dispersed component comprises lithium fluoride.

### Claim 13 (depends on 1)

The method of claim 1 further comprising:
removing unreacted dioxolane compounds, fluorinated organosilane compounds, and/or mobile reaction byproducts from the protective interfacial layer.

### Claim 14 (depends on 13)

The method of claim 13 wherein the unreacted dioxolane compounds, fluorinated organosilane compounds, and/or mobile reaction byproducts are removed from the protective interfacial layer by washing the protective interfacial layer with a nonpolar organic solvent.

### Claim 15

A method of manufacturing a negative electrode for an electrochemical cell of a secondary lithium metal battery, the method comprising:
forming a continuous lithium metal layer on a major surface of a metal substrate; and
applying a precursor solution to a major facing surface of the continuous lithium metal layer to form a protective interfacial layer directly on the major facing surface of the continuous lithium metal layer,
wherein the precursor solution includes an organic solvent mixture, a dioxolane, and a fluorinated organosilane,
wherein the protective interfacial layer exhibits a composite structure including a polymeric matrix component and a lithium-containing dispersed component embedded in the polymeric matrix component, and
wherein the polymeric matrix component is chemically bonded to the major facing surface of the continuous lithium metal layer via a plurality of silicon-oxygen bonds and/or alkoxide bonds.

### Claim 16 (depends on 15)

The method of claim 15 wherein the polymeric matrix component comprises a plurality of siloxane bonds, and wherein the lithium-containing dispersed component comprises lithium fluoride.

### Claim 17

An electrochemical cell of a lithium metal battery, the electrochemical cell comprising:
a positive electrode including a transition metal oxide that can undergo a reversible intercalation of lithium ions;
a lithium metal negative electrode spaced apart from the positive electrode, the lithium metal negative electrode including a lithium metal layer disposed on a negative electrode current collector, the lithium metal layer having a major facing surface that faces toward the positive electrode; and
a nonaqueous liquid electrolyte in ionic contact with the positive electrode and the lithium metal negative electrode,
wherein a protective interfacial layer is formed directly on the major facing surface of the lithium metal layer, along an interface between the lithium metal negative electrode and the nonaqueous liquid electrolyte,
wherein the protective interfacial layer exhibits a composite structure including a polymeric matrix component and a lithium-containing dispersed component embedded in the polymeric matrix component, and
wherein the polymeric matrix component is chemically bonded to the lithium metal layer via a plurality of silicon-oxygen bonds and/or alkoxide bonds.

### Claim 18 (depends on 17)

The electrochemical cell of claim 17 wherein the lithium metal layer comprises, by weight, greater than 97% lithium.

### Claim 19 (depends on 17)

The electrochemical cell of claim 17 wherein the transition metal oxide of the positive electrode is a high-nickel content lithium nickel cobalt manganese oxide having the chemical formula: LiNi1-a-bCoaMnbO2, wherein a=0.1-0.2 and b=0.1-0.2.

### Claim 20 (depends on 17)

The electrochemical cell of claim 17 wherein the nonaqueous liquid electrolyte comprises a nonaqueous aprotic organic solvent and a lithium salt dissolved in the nonaqueous aprotic organic solvent.