# US 2023/0155121 A1 · Lithium secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0155121 A1
- Document ID: US20230155121A1
- Status: Published application
- Kind: A1
- Application number: 17/916,678
- Filed: 2021-04-07
- Published: 2023-05-18
- Earliest claimed: 2020-04-09
- Assignees: Sumitomo Chemical Company, Limited
- Applicants: Sumitomo Chemical Company, Limited
- Inventors: Takitaro YAMAGUCHI; Shingo MATSUMOTO; Toshiaki KUMAGAI; Yoji MATSUO
- Web page: https://patentgrep.com/patent/US20230155121A1

## CPC

- H01M 4/463: {Aluminium based}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a lithium secondary battery including: an aluminum anode configured to occlude and release lithium ions: a cathode configured to occlude and release lithium ions; and an electrolyte, in which the aluminum anode is formed of an aluminum-containing metal, the cathode has a cathode active material, and the cathode active material contains a metal oxide containing nickel.

## Claims

### Claim 1

A lithium secondary battery comprising:
an aluminum anode configured to occlude and release lithium ions;
a cathode configured to occlude and release lithium ions; and
an electrolyte,
wherein the aluminum anode is formed of an aluminum-containing metal,
the cathode has a cathode active material, and
the cathode active material contains a metal oxide containing nickel.

### Claim 2 (depends on 1)

The lithium secondary battery according to claim 1,
wherein, in the aluminum-containing metal, a non-aluminum metal phase is dispersed in an aluminum metal phase.

### Claim 3 (depends on 1)

The lithium secondary battery according to claim 1,
wherein the aluminum-containing metal has an average corrosion rate of 0.2 mm/year or less measured by an immersion test under the following immersion conditions,
[immersion conditions]
immersion solution: 3.5% NaCl aqueous solution adjusted to a pH of 3 using acetic acid as a pH adjuster,
immersion temperature: 30° C.,
immersion time: 72 hours.

### Claim 4 (depends on 1)

The lithium secondary battery according to claim 1,
wherein the aluminum-containing metal has a Vickers hardness of 10 Hv or more and 70 Hv or less.

### Claim 5 (depends on 1)

The lithium secondary battery according to claim 1,
wherein the aluminum anode is a rolled material, and
in a cumulative frequency distribution curve of an absolute value of an angle formed by a rolled surface of the aluminum anode and a normal to a {111} plane, which is obtained by measuring a surface of the aluminum anode by an electron backscatter diffraction method, when a total is set to 100%, an angle at which a cumulative frequency from a low angle side is 50% or more is 20° or less.

### Claim 6 (depends on 1)

The lithium secondary battery according to claim 1,
wherein the aluminum anode is a rolled material, and
in a cumulative frequency distribution curve of an absolute value of an angle formed by a rolling direction of the aluminum anode and a normal to a {111} plane, which is obtained by measuring a surface of the aluminum anode by an electron backscatter diffraction method, when a total is set to 100%, an angle at which a cumulative frequency from a low angle side is 50% or more is 20° or less.

### Claim 7 (depends on 2)

The lithium secondary battery according to claim 2,
wherein the aluminum-containing metal has an average corrosion rate of 0.2 mm/year or less measured by an immersion test under the following immersion conditions,
[immersion conditions]
immersion solution: 3.5% NaCl aqueous solution adjusted to a pH of 3 using acetic acid as a pH adjuster,
immersion temperature: 30° C.,
immersion time: 72 hours.

### Claim 8 (depends on 2)

The lithium secondary battery according to claim 2,
wherein the aluminum-containing metal has a Vickers hardness of 10 Hv or more and 70 Hv or less.

### Claim 9 (depends on 2)

The lithium secondary battery according to claim 2,
wherein the aluminum anode is a rolled material, and
in a cumulative frequency distribution curve of an absolute value of an angle formed by a rolled surface of the aluminum anode and a normal to a {111} plane, which is obtained by measuring a surface of the aluminum anode by an electron backscatter diffraction method, when a total is set to 100%, an angle at which a cumulative frequency from a low angle side is 50% or more is 20° or less.

### Claim 10 (depends on 2)

The lithium secondary battery according to claim 2,
wherein the aluminum anode is a rolled material, and
in a cumulative frequency distribution curve of an absolute value of an angle formed by a rolling direction of the aluminum anode and a normal to a {111} plane, which is obtained by measuring a surface of the aluminum anode by an electron backscatter diffraction method, when a total is set to 100%, an angle at which a cumulative frequency from a low angle side is 50% or more is 20° or less.