# US 2023/0155000 A1 · Selective Laser Annealing Method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0155000 A1
- Document ID: US20230155000A1
- Status: Published application
- Kind: A1
- Application number: 18/093,434
- Filed: 2023-01-05
- Published: 2023-05-18
- Earliest claimed: 2020-06-05
- Assignees: Infineon Technologies AG
- Applicants: Infineon Technologies AG
- Inventors: Albert Birner; Rudolf Berger; Helmut Brech; Olaf Storbeck; Haifeng Sun; John Twynam
- Web page: https://patentgrep.com/patent/US20230155000A1

## CPC

- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10D 30/475: {having wider bandgap layer formed on top of lower bandgap active layer, e.g. undoped barrier HEMTs such as i-AlGaN/GaN HEMTs}
- H10D 62/235: {of IGFETs (IGFETs having buried channels H10D30/637)}
- H10D 62/824: comprising only Group III-V materials heterojunctions, e.g. GaN/AlGaN heterojunctions
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D 64/0116: {to Group III-V semiconductors}
- H10D 64/251: {Source or drain electrodes for field-effect devices}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P 30/206: {into Group III-V semiconductors}
- H10P 30/21: {of electrically active species}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10W 74/137: {the encapsulations being directly on the semiconductor body (H10W74/134 takes precedence)}
- H10W 74/43: comprising oxides, nitrides or carbides, e.g. ceramics or glasses
- H10D 62/149: {Source or drain regions of field-effect devices}
- H10D 62/343: {Gate regions of field-effect devices having PN junction gates}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method includes providing a semiconductor body, forming a thermosensitive element on or within the semiconductor body, forming a structured laser-reflective mask on the upper surface of the semiconductor body that covers the thermosensitive element and includes first and second openings, and performing a laser thermal annealing process that transmits laser energy through the first and second openings and into the semiconductor body, wherein the thermosensitive element comprises a critical temperature at which the thermosensitive element is irreparably damaged, wherein the laser thermal annealing process brings portions of the semiconductor body that are underneath the first and second openings to above the critical temperature, and wherein during the laser thermal annealing process the thermosensitive element remains below the critical temperature.

## Claims

### Claim 1

A method of forming a semiconductor device, the method comprising:
providing a semiconductor body;
forming a thermosensitive element on or within the semiconductor body,
forming a structured laser-reflective mask on the upper surface of the semiconductor body that covers the thermosensitive element and comprises first and second openings; and
performing a laser thermal annealing process that transmits laser energy through the first and second openings and into the semiconductor body,
wherein the thermosensitive element comprises a critical temperature at which the thermosensitive element is irreparably damaged,
wherein the laser thermal annealing process brings portions of the semiconductor body that are underneath the first and second openings to above the critical temperature, and
wherein during the laser thermal annealing process the thermosensitive element remains below the critical temperature.

### Claim 2 (depends on 1)

The method of claim 1, wherein the thermosensitive element is a gate electrode of a MOSFET device.

### Claim 3 (depends on 1)

The method of claim 1, wherein the thermosensitive element is a gate structure of a HEMT device, and wherein the gate structure comprises a region of doped III-nitride semiconductor material.

### Claim 4 (depends on 1)

The method of claim 1, further comprising implanting dopant atoms into the upper surface of the semiconductor body, and wherein performing the laser thermal anneal comprises activating the implanted dopant atoms.

### Claim 5 (depends on 4)

The method of claim 4, wherein forming the structured laser-reflective mask comprises depositing a layer of reflective material on the upper surface of the type III-nitride semiconductor portion and forming first and second openings in the layer of laser reflective material, and wherein the implanting of dopant atoms comprises implanting the dopant atoms through the first and second openings.

### Claim 6 (depends on 5)

The method of claim 5, wherein during the laser thermal anneal, the first and second openings substantially transmit energy from a laser into the semiconductor body and the structured laser-reflective mask substantially reflects energy from the laser.

### Claim 7 (depends on 4)

The method of claim 4, wherein the structured laser-reflective mask comprises a plurality of first-type dielectric material layers arranged alternatingly with a plurality of second-type dielectric material layers, and wherein a first-type dielectric material of the plurality of first type dielectric material layers has a different refractive index as a second-type dielectric material of the plurality of second type dielectric material layers.

### Claim 8 (depends on 7)

The method of claim 7, wherein a melting point of the first-type dielectric material and a melting point of the second-type dielectric material are each greater than an activation temperature that activates the implanted dopant atoms.

### Claim 9 (depends on 7)

The method of claim 7, wherein at least one of the first-type dielectric material layers and the second-type dielectric material layers is formed by a chemical vapour deposition technique or a physical sputtering technique.

### Claim 10 (depends on 7)

The method of claim 7, wherein the laser thermal anneal is applied with a laser being applied to the structured laser-reflective mask at an incident angle θ, and wherein each of the first-type dielectric material layers and the second-type dielectric material layers have a thickness of (λ/4η)·√(1-sin2(θ)/η2), wherein λ is a wavelength of the laser, and wherein η is a refractive index of the first-type dielectric material or second type dielectric material of the respective layer.

### Claim 11 (depends on 1)

The method of claim 1, wherein the material of the structured laser-reflective mask has an energy bandgap that is higher than the semiconductor body.

### Claim 12 (depends on 1)

The method of claim 1, wherein the laser thermal anneal is performed such that λ <1240/E, wherein E is an energy bandgap of a type III-nitride semiconductor of the type III-nitride semiconductor portion in electron-volts, and wherein λ is a wavelength of light from the laser thermal anneal in nanometres.

### Claim 13 (depends on 1)

The method of claim 1, wherein the semiconductor body comprises a type III-nitride semiconductor portion that comprises a channel layer and a barrier layer, wherein the channel layer comprises InXGa(1-X)N, where x≥0, wherein the barrier layer comprises InxAlyGazN, where x≥0, y>0 and z=1-x-y, and wherein the passivation layer is a layer of silicon nitride.

### Claim 13

A semiconductor device, comprising:
a semiconductor body comprising a base carrier portion and a type III-nitride semiconductor portion disposed on the base carrier portion, the type III-nitride semiconductor portion comprising a heterojunction and two-dimensional charge carrier gas;
one or more ohmic contacts that form an ohmic connection with the two-dimensional charge carrier gas;
an electrically insulating passivation layer formed on the base carrier portion directly over the one or more ohmic contacts; and
a gate structure that is configured to control a conductive state of the two-dimensional charge carrier gas.

### Claim 14 (depends on 13)

The semiconductor device of claim 13, wherein the type III-nitride semiconductor portion comprises a channel layer and a barrier layer, wherein the channel layer comprises InxGa(1-x)N, where x≥0, wherein the barrier layer comprises InxAlyGazN, where x≥0, y>0 and z=1-x-y, and wherein the passivation layer is a layer of silicon nitride.

### Claim 15 (depends on 13)

The semiconductor device of claim 13, wherein the one or more ohmic contacts comprise conductive metal regions formed on a surface of the type III-nitride semiconductor portion and doped regions implanted in the type III-nitride portion beneath the conductive metal regions, wherein the conductive metal regions directly cover and contact the implanted doped regions.