# US 2023/0151515 A1 · Bielastic fabric and its manufacturing process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0151515 A1
- Document ID: US20230151515A1
- Status: Published application
- Kind: A1
- Application number: 18/090,752
- Filed: 2022-12-29
- Published: 2023-05-18
- Earliest claimed: 2015-10-28
- Assignees: Artex AB
- Applicants: Artex S.R.L.
- Inventors: Luca Denna; Massimiliano Denna; Roberto Denna
- Web page: https://patentgrep.com/patent/US20230151515A1

## CPC

- D04B 1/18: elastic threads
- D06P 3/8204: {fibres of different chemical nature}
- D06P 5/02: After-treatment
- D10B 2331/02: polyamides (D10B2331/08 takes precedence)
- D10B 2331/06: polyethers
- D10B 2331/08: polyamino acids or polypeptides
- D10B 2331/12: polyureas
- D10B 2401/061: elastic
- D04B: KNITTING
- D06P: DYEING OR PRINTING TEXTILES; DYEING LEATHER, FURS OR SOLID MACROMOLECULAR SUBSTANCES IN ANY FORM
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

There are described a bielastic fabric comprising biopolyamide yarn and elastane yarn, having excellent elastic properties and high dimensional stability, and a cost-effective, efficient process for obtaining it.

## Claims

### Claim 1

A process of manufacturing a bielastic fabric comprising a biopolyamide yarn and an elastane yarn, the process comprising the steps of:
a) stitching the biopolyamide yarn and the elastane yarn to obtain a fabric,
b) heat-setting the fabric at a temperature that is not higher than 160° C. for a time period of 100 seconds or less; and, optionally,
c) dyeing the fabric thus heat-set,
wherein the biopolyamide yarn is a yarn of a polyamide made of polymerized monomers partly or totally derived from castor oil.

### Claim 2 (depends on 1)

The process of claim 1, wherein the heat-setting step b) is carried out over the time period of 30-70 seconds.

### Claim 3 (depends on 1)

The process of claim 1, wherein the heat-setting step b) is carried out at the temperature of 100-160° C.

### Claim 4 (depends on 1)

The process of claim 1, wherein the heat-setting step b) is carried out in warm air, in a tentering machine.

### Claim 5 (depends on 1)

The process of claim 1, wherein the dyeing step c) comprises the following substeps:
i) scouring at 80-100° C. for 10-20 minutes,
ii) neutralizing of the scouring at 50-70° C. for 5-20 minutes,
iii) dyeing, with a dye dosage for 15-30 minutes at 90-110° C. with permanence for 20-40 minutes,
iv) stripping at 30-50° C. for 5-20 minutes,
v) treating with a fixer at 50-90° C. for 10-30 minutes, and
vi) conducting a final cold washing.

### Claim 6 (depends on 1)

The process of claim 1, wherein the biopolyamide yarn of step a) has a count of 10-200 dTex.

### Claim 7 (depends on 1)

The process of claim 1, wherein the elastane yarn of step a) has a count of 10-200 dTex.

### Claim 8 (depends on 6)

The process of claim 6, wherein the biopolyamide yarn of step a) has the count of 20-150 dTex.

### Claim 9 (depends on 7)

The process of claim 7, wherein the elastane yarn of step a) has the count of 15-100 dTex.

### Claim 10 (depends on 1)

The process of claim 1, wherein the fabric obtained in step a) comprises at least 60% of the biopolyamide yarn and at least 5% of the elastane yarn.

### Claim 11 (depends on 1)

The process of claim 1, wherein the stitching of step a) is a jersey stitching or an interlock stitching.

### Claim 12 (depends on 1)

The process of claim 1, wherein the fabric includes a weft direction and a warp direction, such that the fabric obtained in step a) comprises 75-90% of the biopolyamide yarn and 10-25% of the elastane yarn, and has a jersey stitch, and a basis weight of 180-210 g/sqm, and, after step b), has 45-90% of elasticity in the weft direction and 35-80% of elasticity in the warp direction, or
wherein the fabric obtained in step a) comprises 75-90% of the biopolyamide yarn and 10-25% of the elastane yarn, and has a jersey stitch, and a basis weight of 100-140 g/sqm, and, after step b), has 120-200% of elasticity in the weft direction and 120-200% of elasticity in the warp direction, or
wherein the fabric obtained in step a) comprises 75-90% of the biopolyamide yarn and 10-25% of the elastane yarn, and has an interlock stitch, and a basis weight of 160-200 g/sqm, and, after step b), has 110-190% of elasticity in the weft direction and 50-100% of elasticity in the warp direction.

### Claim 13 (depends on 1)

The process of claim 1, wherein the fabric includes a weft direction and a warp direction, such that the fabric obtained in step a) comprises 80-90% of the biopolyamide yarn and 10-20% of the elastane yarn, and has a jersey stitch, and a basis weight of 190-200 g/sqm, and, after step b), has 50-80% of elasticity in the weft direction and 45-70% of elasticity in the warp direction, or
wherein the fabric obtained in step a) comprises 70-80% of the biopolyamide yarn and 20-30% of the elastane yarn, and has a jersey stitch, and a basis weight of 110-130 g/sqm, and, after step b), has 140-180% of elasticity in the weft direction and 140-180% of elasticity in the warp direction, or
wherein the fabric obtained in step a) comprises 70-80% of the biopolyamide yarn and 20-30% of the elastane yarn, and has an interlock stitch, and a basis weight of 170-190 g/sqm, and, after step b), has 130-180% of elasticity in the weft direction and 60-90% of elasticity in the warp direction.

### Claim 14 (depends on 1)

The process of claim 1, wherein the polyamide in the biopolyamide yarn of step a) is biopolyamide 6, biopolyamide 6.6, biopolyamide 6.10, biopolyamide 6.12, biopolyamide 11, biopolyamide 12, or a mixture thereof.