Post-treatment methods and systems for core-shell catalysts
AssigneesGuangzhou Hkust Fok Ying Tung Research Institute, The Hong Kong University of Science and Technology
InventorsMinhua SHAO, Hsi-Wen WU
Life of this patent
Estimating the term…
Loading patent…
AssigneesGuangzhou Hkust Fok Ying Tung Research Institute, The Hong Kong University of Science and Technology
InventorsMinhua SHAO, Hsi-Wen WU
Estimating the term…
Provided is a post-treatment method and system for a core-shell catalyst, which relate to the field of fuel cell materials. The post-treatment method of the present disclosure includes the following steps: a core-shell catalyst is added into an electrolyte solution containing citric acid or ethylenediamine tetraacetic acid, a gas containing oxygen is introduced into the electrolyte solution followed by stirring for a predetermined reaction time, the open circuit potential of the reactor base is recorded during the reaction time, and the open circuit potential should stabilize at 0.90˜1.0 V vs. RHE when the reaction is completed. The molar ratio of citric acid or ethylenediamine tetraacetic acid to platinum of the core-shell catalyst is 10 to 1000:1. A percentage of oxygen in the gas is 10 to 100% by volume. The post-treatment method of the present disclosure can significantly improve the platinum mass activity and PGM mass activity and durability of core-shell catalyst.
1-10. (canceled)
A post-treatment method for a core-shell catalyst, including steps of:
A post-treatment system for a core-shell catalyst, including:
Dependencies are inferred from the claim text.