# US 2023/0146612 A1 · Methods for improving mechanical property and biological stability of magnesium alloy and manufacturing material and applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0146612 A1
- Document ID: US20230146612A1
- Status: Published application
- Kind: A1
- Application number: 17/905,456
- Filed: 2021-02-25
- Published: 2023-05-11
- Earliest claimed: 2020-03-03
- Assignees: Hejie LI
- Inventors: Hejie LI; Tianfang WANG; Xiaosong LIU; Guoying NI
- Web page: https://patentgrep.com/patent/US20230146612A1

## CPC

- A61L 27/047: {Other specific metals or alloys not covered by A61L27/042 - A61L27/045 or A61L27/06}
- A61L 31/022: {Metals or alloys}
- A61L 27/34: Macromolecular materials
- A61L 31/10: Macromolecular materials
- A61L 31/148: {Materials at least partially resorbable by the body}
- A61L 31/16: Biologically active materials, e.g. therapeutic substances {(A61L31/047 takes precedence)}
- B24B 27/033: for grinding a surface for cleaning purposes, e.g. for descaling or for grinding off flaws in the surface
- C22C 23/00: Alloys based on magnesium
- C22C 23/02: with aluminium as the next major constituent
- C22F 1/02: in inert or controlled atmosphere or vacuum (adjusting the composition of the atmosphere C21D1/76)
- C22F 1/047: of alloys with magnesium as the next major constituent
- C22F 1/06: of magnesium or alloys based thereon
- A61L 2300/25: Peptides having up to 20 amino acids in a defined sequence
- A61L 2300/404: Biocides, antimicrobial agents, antiseptic agents
- A61L 2300/41: Anti-inflammatory agents, e.g. NSAIDs
- A61L 2300/608: having two or more layers
- A61L 2400/18: Modification of implant surfaces in order to improve biocompatibility, cell growth, fixation of biomolecules, e.g. plasma treatment
- A61L 2420/08: Coatings comprising two or more layers
- A61L 2430/02: for reconstruction of bones; weight-bearing implants
- B05D 3/002: {Pretreatement}
- B05D 7/14: to metal, e.g. car bodies (involving a chemical reaction between the metal and the coating C23)
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

A heat treatment method for improving the mechanical property and the biofunctional stability of a magnesium alloy is provided, comprising: (1) fully annealing an original cold-drawn magnesium alloy AZ31; (2) polishing a surface of the magnesium alloy AZ31 from the step (1) by a waterproof abrasive paper; (3) heating the magnesium alloy AZ31 obtained from the step (2) to a temperature of 330° C. to 350° C. and keeping the temperature for 3 to 4 hours; and (4) cooling the magnesium alloy AZ31 obtained from the step (3) to room temperature. A method for manufacturing a small-peptide-coated biomaterial and an application of the small-peptide-coated biomaterial are further provided.

## Claims

### Claim at position 1

1-15. (canceled)

### Claim 16

A heat treatment method for improving the mechanical property and the biofunctional stability of a magnesium alloy, comprising steps of:
(1) fully annealing an original cold-drawn magnesium alloy AZ31 in an interference-free atmosphere;
(2) polishing a surface of the magnesium alloy AZ31 from the step (1) by a waterproof abrasive paper to remove an original oxide layer while maintaining or improving the finish of the surface;
(3) heating the magnesium alloy AZ31 obtained from the step (2) in an interference-free atmosphere created by an inert gas or a vacuum, wherein the magnesium alloy AZ31 is heated to a temperature of 330° C. to 350° C. in the interference-free atmosphere and then the temperature is kept for 3 to 4 hours;
(4) cooling the magnesium alloy AZ31 obtained from the step (3) to room temperature, to obtain an equiaxed crystal structure which is texture-even and isotropic.

### Claim 17 (depends on 16)

The heat treatment method of claim 16, wherein the polishing the surface of the magnesium alloy AZ31 by the waterproof abrasive paper comprises initial polishing and finishing; the initial polishing is performed with a 400-mesh waterproof abrasive paper for 1 to 3 minutes to remove the original oxide layer, and then the finishing is immediately performed, wherein the finishing is performed with a 1200-mesh to 2400-mesh waterproof abrasive paper for 2 to 5 minutes, to keep the finish of the surface of the magnesium alloy AZ31.

### Claim 18 (depends on 17)

The heat treatment method of claim 17, wherein the initial polishing comprises grinding along one direction, with a strength effective to remove the oxide layer, the initial polishing is performed until the dark oxide layer on the surface of the magnesium alloy AZ31 is fully removed to expose the silver white magnesium metal itself, and a grinding direction in the finishing is perpendicular to the direction of the initial polishing, with a strength smaller than that in the initial polishing, until there is no obvious scratch on the surface of the magnesium alloy AZ31.

### Claim 19 (depends on 16)

A method for manufacturing a small-peptide-coated biomaterial based on the magnesium alloy AZ31 of claim 16, comprising steps of: ultrasonically cleaning the magnesium alloy AZ31 to remove impurities on the surface of the magnesium alloy AZ31; dissolving polyurethane with chloroform, and then placing the treated magnesium alloy AZ31 into the chloroform solution dissolved with the polyurethane, so that the magnesium alloy AZ31 is fully enclosed in the solution; taking out the magnesium alloy AZ31, and letting the magnesium alloy AZ31 stand until the solution on the surface thereof is solidified; and then activating the polyurethane coated on the surface of the magnesium alloy AZ31 by using a click reaction in a plasma reactor; and finally placing the surface-activated polyurethane-coated magnesium alloy AZ31 into a sodium phosphate solution dissolved with polypeptide and applying vibration to allow them fully react to form the corresponding polypeptide coating.

### Claim 20 (depends on 19)

The method of claim 19, wherein the magnesium alloy AZ31 is the cold-drawn magnesium alloy AZ31 or the magnesium alloy AZ31 fully annealed in the interference-free atmosphere.

### Claim 21 (depends on 19)

The method of claim 19, wherein in the ultrasonically cleaning, the cleaning is performed for 3 to 5 minutes, and the cleaning liquid is pure water or 80% ethyl alcohol, to remove impurities on a surface of the magnesium alloy AZ31 and keep the surface of the magnesium alloy AZ31 clean.

### Claim 22 (depends on 19)

The method of claim 19, wherein the chloroform solution of polyurethane is a uniform, colourless, transparent, and viscous solution formed by mixing the white solid polyurethane with colourless and transparent chloroform solution having a purity not less than 99.5% in a ratio of 3 g:100 ml and then being vibrated and stirred at a normal temperature.

### Claim 23 (depends on 22)

The method of claim 22, wherein the magnesium alloy AZ31 is placed into the chloroform solution of polyurethane, fully immersed for 60 minutes, and intermittently vibrated and stirred.

### Claim 24 (depends on 19)

The method of claim 19, wherein in the solidification of the solution on the surface of the magnesium alloy AZ31, the chloroform is quickly volatilized so that one uniform, dense, and stable polyurethane coating is formed on the metal surface.

### Claim 25 (depends on 24)

The method of claim 24, wherein the magnesium alloy AZ31 with the solution on its surface solidified is surface-treated with oxygen plasma at 2.45 GHz for 1 minute in the plasma reactor and then stands in the atmospheric environment for 15 minutes to further promote the formation of peroxide groups and hydroxyl groups on the surface.

### Claim 26 (depends on 25)

The method of claim 25, wherein after the further promoting the formation of peroxide groups and hydroxyl groups on the surface, the magnesium alloy AZ31 is moved back into the plasma reactor, the vacuum degree is adjusted to 26.7, acrylic acid vapor is slowly introduced until reaching 66.7 Pa, after reacting for 1 minute, the magnesium alloy AZ31 is taken out and cleaned for 10 minutes in an ultrasonic cleaner, thereafter, the magnesium alloy AZ31 is transferred into a mixed aqueous solution, with pH of 5.0, of 1.25 mg/ml N-hydroxysuccinimide and 5 mg/ml 1-ethyl-3-(3-dimethylaminopropyl) carbodiimide, vibrated and stirred for 20 hours at 4° C., and then taken out, finally, the polyurethane coated on the surface of the magnesium alloy AZ31 is activated.

### Claim 27 (depends on 26)

The method of claim 26, wherein the sodium phosphate solution of polypeptide is a 5 mM uniform solution prepared by dissolving F3 with a purity greater than 95% into 0.1 M sodium phosphate solution.

### Claim 28 (depends on 27)

The method of claim 27, wherein the surface-activated polyester-coated magnesium alloy AZ31 is placed into the sodium phosphate solution of polypeptide, taken out after 20 hours of vibration, ultrasonically cleaned in ultrapure water for 10 minutes for twice and dried so that the manufacturing is completed.

### Claim 29 (depends on 19)

An application of the small-peptide-coated biomaterial manufactured by the method of claim 19, wherein the small-peptide-coated biomaterial is applied in the manufacture of a hard-tissue defect repair material.

### Claim 30 (depends on 29)

The application of claim 29, wherein the small-peptide-coated biomaterial is applied in the manufacture of a bone fixation material.