# US 2023/0146238 A1 · Thermoplastic polyurethane resin suitable for a laminating process and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0146238 A1
- Document ID: US20230146238A1
- Status: Published application
- Kind: A1
- Application number: 17/902,040
- Filed: 2022-09-02
- Published: 2023-05-11
- Earliest claimed: 2021-11-04
- Assignees: Nan Ya Plastics Corporation
- Applicants: Nan Ya Plastics Corporation
- Inventors: TE-CHAO LIAO; HAN-CHING HSU; CHEN-WEI CHANG
- Web page: https://patentgrep.com/patent/US20230146238A1

## CPC

- C08L 75/06: from polyesters
- C09J 175/06: from polyesters
- C08G 18/0895: {Manufacture of polymers by continuous processes (C08G18/0838 takes precedence)}
- C08G 18/12: using two or more compounds having active hydrogen in the first polymerisation step
- C08G 18/2825: {having at least 6 carbon atoms}
- C08G 18/3206: {aliphatic}
- C08G 18/4202: {Two or more polyesters of different physical or chemical nature (C08G18/44 takes precedence)}
- C08G 18/4238: {derived from dicarboxylic acids and dialcohols}
- C08G 18/664: {with compounds of group C08G18/3203}
- C08J 5/18: Manufacture of films or sheets
- C08J 2375/06: from polyesters
- C08L 2203/16: used for films
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A thermoplastic polyurethane resin suitable for a laminating process and a method for producing the same are provided. The thermoplastic polyurethane resin is formed of an isocyanate component, a polyol component, a chain extender component, and a chain terminator component that is a monohydric alcohol via a polymerization reaction. The polyol component includes a first polyol having a number average molecular weight between 600 and 2,000 g/mol and a second polyol having a number average molecular weight between 1,500 and 3,000 g/mol. The chain extender component includes a first chain extender and a second chain extender. The first chain extender is a dihydric alcohol having a carbon chain length of C2-6, and a molecular structure thereof is linear and symmetrical. The second chain extender is a dihydric alcohol having a carbon chain length of C3-10, and a molecular structure thereof has a side chain and/or an ether group.

## Claims

### Claim 1

A thermoplastic polyurethane resin suitable for a laminating process, characterized in that the thermoplastic polyurethane resin is formed from a reaction mixture via a polymerization reaction, and the reaction mixture includes:
an isocyanate component;
a polyol component, the polyol component including a first polyol and a second polyol; wherein the first polyol has a first number average molecular weight, the second polyol has a second number average molecular weight, the first number average molecular weight is between 600 g/mol and 2,000 g/mol, and the second number average molecular weight is between 1,500 g/mol and 3,000 g/mol; wherein the first number average molecular weight is less than the second number average molecular weight, and a difference between the first number average molecular weight and the second number average molecular weight is between 500 g/mol and 1,000 g/mol;
a chain extender component, the chain extender component including a first chain extender and a second chain extender; wherein the first chain extender is a dihydric alcohol having a carbon chain length of from C2 to C6, and a molecular structure of the first chain extender is linear and symmetrical; wherein the second chain extender is a dihydric alcohol having a carbon chain length of from C3 to C10, and a molecular structure of the second chain extender has at least one side chain and/or at least one ether group; and
a chain terminator component, the chain terminator component being a monohydric alcohol having a carbon chain length of from C4 to C18.

### Claim 2 (depends on 1)

The thermoplastic polyurethane resin according to claim 1, wherein, based on a total weight of the reaction mixture being 100 parts by weight, an amount of the isocyanate component is between 30 parts by weight and 35 parts by weight, an amount of the polyol component is between 60 parts by weight and 65 parts by weight, an amount of the chain extender component is between 5 parts by weight and 10 parts by weight, and an amount of the chain terminator component is between 0.01 parts by weight and 0.05 parts by weight.

### Claim 3 (depends on 1)

The thermoplastic polyurethane resin according to claim 1, wherein a weight ratio between the first polyol and the second polyol ranges from 8 to 12:48 to 52, and the first polyol having the first number average molecular weight promotes lowering of a softening temperature of the thermoplastic polyurethane resin.

### Claim 4 (depends on 1)

The thermoplastic polyurethane resin according to claim 1, wherein the first polyol is a first polyester polyol, and is at least one material selected from a group consisting of: poly(1,4-butylene adipate), polyethylene-1,4-butylene adipate glycol, and poly(1,6-hexamethylene adipate-succinic acid); wherein the second polyol is a second polyester polyol, and is at least one material selected from the group consisting of: poly(1,4-butylene adipate), polyethylene-1,4-butylene adipate glycol, and poly(1,6-hexamethylene adipate-succinic acid).

### Claim 5 (depends on 4)

The thermoplastic polyurethane resin according to claim 4, wherein a main chain of the first polyol and/or the second polyol is further branched by a short-chain diol to form an asymmetric molecular structure.

### Claim 6 (depends on 1)

The thermoplastic polyurethane resin according to claim 1, wherein the first chain extender is at least one material selected from a group consisting of 1,4-butanediol and ethylene glycol, the second chain extender is at least one material selected from a group consisting of 2-methyl-1,3-propanediol, neopentyl glycol, 3-methyl-1,5-pentanediol, diethylene glycol, and dipropylene glycol, a weight ratio between the first chain extender and the second chain extender ranges from 4.5 to 4.75:0.25 to 0.5, and the second chain extender having the at least one side chain and/or the at least one ether group promotes reducing of a crystallinity of the thermoplastic polyurethane resin.

### Claim 7 (depends on 1)

The thermoplastic polyurethane resin according to claim 1, wherein the chain terminator component is at least one material selected from a group consisting of 1-butanol, 1-octanol, 1-dodecanol and 1-octadecanol.

### Claim 8 (depends on 1)

The thermoplastic polyurethane resin according to claim 1, wherein an NCO/OH equivalent ratio of the reaction mixture in the polymerization reaction is between 0.98 and 1.02.

### Claim 9 (depends on 1)

The thermoplastic polyurethane resin according to claim 1, wherein the thermoplastic polyurethane resin satisfies following conditions:
(1) a ratio (Mw/Mn) between a weight average molecular weight (Mw) and a number average molecular weight (Mn) of the thermoplastic polyurethane resin analyzed by a gel permeation chromatography (GPC) is between 1.250 and 1.300;
(2) a crystallinity of the thermoplastic polyurethane resin analyzed by a differential scanning calorimeter (DSC) is between 10% and 30%;
(3) a melt flow index (MFI) of the thermoplastic polyurethane resin is between 5 g/10 min (190° C.) and 8 g/10 min (190° C.);
(4) a viscosity change rate of the thermoplastic polyurethane resin analyzed by a dynamic mechanical analyzer (DMA) under test conditions of a constant temperature of 190° C. and a shear rate of 0 to 1000 s−1 is between 300 (Ns)/m2 and 600 (Ns)/m2; and
(5) a softening temperature of at least 95 wt. % of resin components in the thermoplastic polyurethane resin is lower than a laminating temperature of the laminating process, wherein the softening temperature is between 150° C. and 180° C., and the laminating temperature is between 170° C. and 200° C.

### Claim 10

A thermoplastic polyurethane resin suitable for a laminating process, characterized in that a polymer chain of the thermoplastic polyurethane resin includes: at least one short chain segment, at least one long chain segment, at least one first extension segment, at least one second extension segment, and at least one chain termination segment;
wherein the at least one short chain segment is formed of residues of a first polyol except for hydroxyl groups, the at least one long chain segment is formed of residues of a second polyol except for hydroxyl groups, the first polyol has a first number average molecular weight, the second polyol has a second number average molecular weight, the first number average molecular weight is between 600 g/mol and 2,000 g/mol, the second number average molecular weight is between 1,500 g/mol and 3,000 g/mol, the first number average molecular weight is less than the second number average molecular weight, and a difference between the first number average molecular weight and the second number average molecular weight is between 500 g/mol and 1,000 g/mol;
wherein the at least one first extension segment is formed of residues of a first chain extender except for hydroxyl groups, the at least one second extension segment is formed of residues of a second chain extender except for hydroxyl groups, the first chain extender has a carbon chain length of from C2 to C6, a molecular structure of the first chain extender is linear and symmetrical, the second chain extender has a carbon chain length of from C3 to C10, and a molecular structure of the second chain extender has at least one side chain and/or at least one ether group;
wherein the at least one chain termination segment is formed of residues of a chain terminator component except for hydroxyl groups, the chain terminator component is a monohydric alcohol having a carbon chain length of from C4 to C18, and the at least one chain termination segment is located at a tail end of the polymer chain.

### Claim 11

A method for producing a thermoplastic polyurethane resin suitable for a laminating process, the method comprising:
respectively adding an isocyanate component, a polyol component, and a chain extender component into an extruder to form a reaction mixture;
performing a polymerization reaction on the reaction mixture in the extruder to increase a molecular weight of the reaction mixture, so that the reaction mixture is formed into the thermoplastic polyurethane resin; wherein an NCO/OH equivalent ratio of the reaction mixture in the polymerization reaction is controlled to be between 0.98 and 1.02; and
adding a chain terminator component into the extruder to terminate the polymerization reaction when the thermoplastic polyurethane resin reaches a predetermined molecular weight or a predetermined viscosity in the polymerization reaction;
wherein the polyol component includes a first polyol and a second polyol, the first polyol has a first number average molecular weight, the second polyol has a second number average molecular weight, the first number average molecular weight is between 600 g/mol and 2,000 g/mol, and the second number average molecular weight is between 1,500 g/mol and 3,000 g/mol; wherein the first number average molecular weight is less than the second number average molecular weight, and a difference between the first number average molecular weight and the second number average molecular weight is between 500 g/mol and 1,000 g/mol;
wherein the chain extender component includes a first chain extender and a second chain extender, the first chain extender is a dihydric alcohol having a carbon chain length of from C2 to C6, and a molecular structure of the first chain extender is linear and symmetrical; wherein the second chain extender is a dihydric alcohol having a carbon chain length of from C3 to C10, and a molecular structure of the second chain extender has at least one side chain and/or at least one ether group; wherein the chain terminator component is a monohydric alcohol having a carbon chain length of from C4 to C18.