# US 2023/0145884 A1 · Halogen free flame-retardant materials and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0145884 A1
- Document ID: US20230145884A1
- Status: Published application
- Kind: A1
- Application number: 17/519,587
- Filed: 2021-11-05
- Published: 2023-05-11
- Earliest claimed: 2021-11-05
- Assignees: Industrial Technology Research Institute
- Applicants: Industrial Technology Research Institute
- Inventors: Wen-Chung Liang; Chi-Lang Wu; Chen-Yu Huang
- Web page: https://patentgrep.com/patent/US20230145884A1

## CPC

- C09K 21/14: Macromolecular materials
- C08L 75/04: Polyurethanes
- C08L 83/06: containing silicon bound to oxygen-containing groups (C08L83/12 takes precedence)
- C09K 21/02: Inorganic materials
- C08K 3/36: Silica
- C08K 2201/011: Nanostructured additives
- C08L 2201/02: Flame or fire retardant/resistant
- C09K 2003/1078: {Fire-resistant, heat-resistant materials}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

The disclosure provides a forming method of a halogen-free flame-retardant material. The method includes the followings. A twin-screw extruder including a first zone and a second zone is used. A mixture in the first zone is mixed, melted and heated to form a molten mixture. The mixture includes a halogen-free flame retardant, a wear-resistant modifier, a thermoplastic elastomer, and an antioxidant. In addition, a silane-modified nano-silica aqueous suspension is introduced into the second zone to mix the silane-modified nano-silica aqueous suspension with the molten mixture from the first zone. The first zone and the second zone are continuously connected regions.

## Claims

### Claim 1

A forming method of a halogen-free flame-retardant material, comprising:
using a twin-screw extruder comprising a first zone and a second zone;
mixing, melting and heating a mixture in the first zone to form a molten mixture, wherein the mixture comprises a halogen-free flame retardant, a wear-resistant modifier, a thermoplastic elastomer, and an antioxidant; and
introducing a silane-modified nano-silica aqueous suspension into the second zone to mix the silane-modified nano-silica aqueous suspension with the molten mixture from the first zone,
wherein the first zone and the second zone are continuously connected regions.

### Claim 2 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein the silane-modified nano-silica aqueous suspension comprises silane, nano-silica powder, and water.

### Claim 3 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein the mixture further comprises a volume resistivity enhancer modified elastomer.

### Claim 4 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein the halogen-free flame retardant comprises a phosphorus nitrogen flame retardant, aluminum phenylphosphinate, aluminum hypophosphite, melamine cyanurate, a phosphate amine salt, or phosphate esters.

### Claim 5 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein the wear-resistant modifier comprises a siloxane polymer, vinyl polydimethylsiloxane, or a methicone silsesquioxane crosspolymer.

### Claim 6 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein the thermoplastic elastomer comprises polyether type thermoplastic polyurethane, polyester type thermoplastic polyurethane, a polyether type thermoplastic polyester elastomer, or a polyester type thermoplastic polyester elastomer.

### Claim 7 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein the antioxidant comprises bis[3-(1,1-dimethylethyl)-4-hydroxy-5-methylbenzenepropionic acid] tripolyethylene glycol or a hindered phenolic composite type antioxidant.

### Claim 8 (depends on 3)

The forming method of a halogen-free flame-retardant material as described in claim 3, wherein the volume resistivity enhancer modified elastomer comprises a styrene-ethylene/butylene-styrene copolymer thermoplastic elastomer or a polyolefin elastomer.

### Claim 9 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein based on 100 parts by weight of the total weight of the mixture, a content of the halogen-free flame retardant is 15 to 45 parts by weight.

### Claim 10 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein based on 100 parts by weight of a weight of the thermoplastic elastomer, a content of the wear-resistant modifier is 1 to 10 parts by weight.

### Claim 11 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein based on 100 parts by weight of a weight of the thermoplastic elastomer, a content of the antioxidant is 0.2 to 1.5 parts by weight.

### Claim 12 (depends on 2)

The forming method of a halogen-free flame-retardant material as described in claim 2, wherein based on 100 parts by weight of the total weight of the mixture, a content of the nano-silica powder is 0.5 to 12 parts by weight.

### Claim 13 (depends on 3)

The forming method of a halogen-free flame-retardant material as described in claim 3, wherein based on 100 parts by weight of the total weight of the mixture, a content of the volume resistivity enhancer modified elastomer is 5 to 30 parts by weight.

### Claim 14 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein a pump pressure for introducing the silane-modified nano-silica aqueous suspension into the second zone is 20 to 50 bars.

### Claim 15 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein the first zone of the twin-screw extruder has a temperature of 120° C. to 200° C.

### Claim 16 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein the second zone of the twin-screw extruder has a temperature of 120° C. to 200° C.

### Claim 17 (depends on 1)

The forming method of a halogen-free flame-retardant material as described in claim 1, wherein a screw rotation speed in the first zone and the second zone of the twin-screw extruder is 60 rpm to 300 rpm.

### Claim 18 (depends on 1)

A halogen-free flame-retardant material prepared using the forming method as described in claim 1, wherein the halogen-free flame-retardant material has a wear resistance of less than 40 mg, a hardness (shore A) of less than 85, a tensile strength of greater than 120 kgf/cm2, an elongation of greater than 300%, and a flame retardancy achieving a UL94 V-0 rating at a specimen thickness of 0.8 mm.

### Claim 19 (depends on 18)

A wear-resistant halogen-free flame-retardant cable sheathing material, comprising the halogen-free flame-retardant material as described in claim 18.