# US 2023/0145863 A1 · Method for producing hardened steel components with a conditioned zinc anti-corrosive layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0145863 A1
- Document ID: US20230145863A1
- Status: Published application
- Kind: A1
- Application number: 17/802,576
- Filed: 2021-03-01
- Published: 2023-05-11
- Earliest claimed: 2020-02-28
- Assignees: voestalpine Stahl GmbH
- Applicants: Voestalpine Stahl GmbH
- Inventors: Ernst SCHACHINGER; Martin FLEISCHANDERL
- Web page: https://patentgrep.com/patent/US20230145863A1

## CPC

- C21D 8/0278: involving a particular surface treatment (C21D8/0294 takes precedence)
- C23C 22/62: Treatment of iron or alloys based thereon
- B21D 22/208: {by heating the blank or deep-drawing associated with heat treatment (C21D takes precedence)}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0242: {Flattening; Dressing; Flexing}
- C23C 22/50: Treatment of iron or alloys based thereon
- C23C 22/82: After-treatment
- C23C 28/023: {only coatings of metal elements only}
- C21D 2211/001: Austenite
- C21D 2211/008: Martensite
- C21D 2261/00: Machining or cutting being involved
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B21D: WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL (working or processing of wire B21F)

## Abstract

A method for producing hardened steel components is provided. A sheet bar is cut from a galvanized strip made of a hardenable steel alloy. The sheet bar is cold-formed into a component blank and heated to a temperature that produces a structural change to austenite. The austenitized component blank is conveyed to a form hardening tool and is held in a form-fitting manner by an upper tool and lower tool, which have a shape essentially corresponding to that of the component blank. Due to the contact of the material of the component blank with the tools, the heat is removed from the steel material quickly enough that a martensitic hardening occurs. After the galvanization of the metal strip and before the temperature increase for achieving the austenitization, tin is applied to the surface of the strip, sheet blank, or component blank.

## Claims

### Claim at position 1

1-17. (canceled)

### Claim 18

A method for producing hardened steel components, comprising the steps of:
cutting a steel sheet bar from a galvanized steel strip including a hardenable steel alloy;
cold-forming the steel sheet bar into a component blank;
heating the component blank to a temperature that produces a structural change in the steel alloy to austenite, yielding an austenitized component blank;
conveying the austenitized component blank to a form hardening tool including an upper tool and a lower tool that define a shape substantially corresponding to a shape of the austenitized component blank;
holding the austenitized component blank in a form-fitting manner contacting the upper tool and the lower tool, wherein due to the contact of the austenitized component blank with the upper tool and the lower tool, heat is removed from the steel alloy quickly enough to cause martensitic hardening of the steel alloy; and
before heating the component blank to the temperature that produces the structural change, applying tin to a surface of at least one of the galvanized steel strip, the steel sheet bar, and the component blank.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the tin is applied in an ionic form from a salt solution.

### Claim 20 (depends on 18)

The method according to claim 18, wherein the tin is applied using a chemical vapor deposition (CVD) or a physical vapor deposition (PVD) process.

### Claim 21 (depends on 18)

The method according to claim 18, wherein the tin is applied from an alkaline or acidic solution.

### Claim 22 (depends on 18)

The method according to claim 18, wherein the tin is applied using an aqueous stannate solution, which is adjusted to be alkaline or acidic.

### Claim 23 (depends on 18)

The method according to claim 18, wherein the tin is complexed with citric acid and is applied from a solution.

### Claim 24 (depends on 18)

The method according to claim 18, wherein the tin is applied from a solution in a layer having a wet thickness of about 1 to about 5 microns and a dry thickness of about 50 to about 150 nanometers.

### Claim 25 (depends on 18)

The method according to claim 18, wherein the tin is applied in an amount of about 30 to about 90 mg tin per square meter of the surface.

### Claim 26 (depends on 18)

The method according to claim 18, wherein the tin is applied from a solution comprising K2SnO3*3H2O, present in a concentration of about 150 to about 250 grams/liter.

### Claim 27 (depends on 26)

The method according to claim 26, wherein the solution further comprises KOH in a concentration of about 15 to about 25 grams per liter.

### Claim 28 (depends on 18)

The method according to claim 18, wherein the tin is applied from a solution having a pH value of about 12.5 to about 13.5.

### Claim 29 (depends on 18)

The method according to claim 18, wherein the tin is complexed with citric acid and is applied from a solution having a pH value of about 4 to about 5.5.

### Claim 30 (depends on 29)

The method according to claim 29, wherein the solution comprises the citric acid in a concentration of about 35 to about 40 g/l.

### Claim 31 (depends on 18)

The method according to claim 18, wherein the tin is applied from a solution comprising about 200 g/l K2SnO3*3H2O and about 20 g/l KOH.

### Claim 32

A galvanized cold-formed steel strip coated with about 40 to about 80 mg tin/m2.

### Claim 33 (depends on 32)

The galvanized steel strip according to claim 32, wherein the tin is deposited metallically or in ionic form.

### Claim 34 (depends on 32)

The galvanized steel strip according to claim 32, wherein the tin is deposited from a stannate solution.

### Claim 35 (depends on 32)

The galvanized steel strip according to claim 32, wherein the tin is deposited using a physical vapor deposition (PVD) or chemical vapor deposition (CVD) process.

### Claim 36

A method of using a galvanized steel strip formed from a hardenable steel alloy, comprising the steps of:
cutting the galvanized steel strip to form a steel sheet bar;
cold-forming the steel sheet bar into a component blank;
coating at least one of the galvanized steel strip, the sheet bar, and the component blank with tin, resulting in a tin-coated component blank;
heating the tin-coated component blank to a temperature that produces austenitization of the steel alloy, yielding an austenitized tin-coated component blank;
conveying the austenitized component blank to a form hardening tool including an upper tool and a lower tool; and
holding the austenitized component blank in a form-fitting manner contacting the upper tool and the lower tool, thereby removing heat from the steel alloy quickly enough to cause martensitic hardening of the steel alloy;
wherein the method is performed without cleaning the galvanized steel strip.

### Claim 37 (depends on 36)

The method of claim 36, wherein the tin is provided from a stannate solution.