# US 2023/0145732 A1 · Trench Fabrication Method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0145732 A1
- Document ID: US20230145732A1
- Status: Published application
- Kind: A1
- Application number: 17/952,754
- Filed: 2022-09-26
- Published: 2023-05-11
- Earliest claimed: 2021-11-10
- Assignees: Hangzhou Fullsemi Semiconductor Co., Ltd.
- Applicants: Hangzhou Fullsemi Semiconductor Co., Ltd.
- Inventors: Peng Lei
- Web page: https://patentgrep.com/patent/US20230145732A1

## CPC

- H10P 50/283: {by chemical means}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P 50/73: {using masks for insulating materials}
- H10W 20/0696: {by using sacrificial placeholders, e.g. using sacrificial plugs}
- H10W 20/089: {using processes for implementing desired shapes or dispositions of the openings, e.g. double patterning}
- H10W 20/47: comprising two or more dielectric layers having different properties, e.g. different dielectric constants
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a trench fabrication method including: forming a first dielectric layer on a semiconductor substrate; patterning/etching the first dielectric layer to form a first trench; forming a sacrificial layer for filling the first trench; forming a second dielectric layer for covering the first dielectric layer and the sacrificial layer; etching the second dielectric layer to form a second trench for exposing the sacrificial layer; and removing the sacrificial layer to form a trench whereby the first trench and the second trench are aligned and connected with each other. The trench fabrication method involves effecting deposition step by step and etching the dielectric layers step by step, so as to fabricate a trench with a high aspect ratio, render the fabrication process simple and easy, enhance process precision, reduce product defect risks, and increase product yield.

## Claims

### Claim 1

A trench fabrication method, comprising steps of:
providing a semiconductor substrate;
forming a first dielectric layer on the semiconductor substrate;
forming a first photoresist layer and patterning the first photoresist layer on the first dielectric layer;
etching the first dielectric layer using the patterned first photoresist layer as a mask to form a first trench penetrating the first dielectric layer, wherein the first trench comprises a first width;
removing the first photoresist layer to expose the first dielectric layer;
forming a sacrificial layer on the first dielectric layer, wherein the sacrificial layer fills in the first trench;
removing a portion of the sacrificial layer to expose the first dielectric layer outside the first trench and a top surface of the sacrificial layer in the first trench;
forming a second dielectric layer on the first dielectric layer and the top surface of the sacrificial layer in the first trench;
forming a second photoresist layer and patterning the second photoresist layer on the second dielectric layer;
etching the second dielectric layer using the patterned second photoresist layer as a mask to form a second trench penetrating the second dielectric layer, wherein the second trench align with the sacrificial layer in first trench, wherein the second trench comprises a second width, and wherein the top surface of the sacrificial layer is exposed from the second trench; and
removing the second photoresist layer and the sacrificial layer to form a trench for exposing the semiconductor substrate.

### Claim 2 (depends on 1)

The trench fabrication method of claim 1, wherein the second width of the second trench is greater than the first width of the first trench.

### Claim 3 (depends on 1)

The trench fabrication method of claim 1, wherein the first trench and the second trench are each axisymmetric, and wherein axes of the first and second trenches are colinear and perpendicular to a top surface of the substrate.

### Claim 4 (depends on 1)

The trench fabrication method of claim 1, wherein, between the step of removing the second photoresist layer and the step of removing the sacrificial layer, the step of forming the sacrificial layer and dielectric layer is recurringly performed M times, where M denotes a positive integer greater than or equal to 1.

### Claim 5 (depends on 1)

The trench fabrication method of claim 1, wherein the first dielectric layer and the second dielectric layer are made of the same material.

### Claim 6 (depends on 1)

The trench fabrication method of claim 1, wherein an aspect ratio of the first trench ranges from 1:1 to 100:1, and an aspect ratio of the second trench ranges from 1:1 to 100:1.

### Claim 7 (depends on 1)

The trench fabrication method of claim 1, wherein the first trench is a deep-hole trench or a deep-groove trench, and wherein the second trench is a deep-hole trench or a deep-groove trench.

### Claim 8 (depends on 1)

The trench fabrication method of claim 1, wherein a cross sectional shape of the first trench comprises one of rectangular, inverted-trapezoid, V-shaped and U-shaped, and wherein a cross sectional shape of the second trench comprises one of rectangular, inverted-trapezoid, V-shaped and U-shaped.

### Claim 9 (depends on 1)

The trench fabrication method of claim 1, wherein the first dielectric layer is one of a silicon oxide layer, a silicon nitride layer and a silicon oxynitride layer, and wherein the second dielectric layer is one of a silicon oxide layer, a silicon nitride layer and a silicon oxynitride layer.

### Claim 10 (depends on 1)

The trench fabrication method of claim 1, wherein the sacrificial layer is a BARC layer.