# US 2023/0145566 A1 · Method of eliminating microstructure inheritance of hypereutectic aluminum-silicon alloys

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0145566 A1
- Document ID: US20230145566A1
- Status: Published application
- Kind: A1
- Application number: 17/529,950
- Filed: 2021-11-18
- Published: 2023-05-11
- Earliest claimed: 2021-11-08
- Assignees: GM Global Technology Operations LLC; Shanghai Jiao Tong University
- Applicants: GM Global Technology Operations LLC; Shanghai Jiao Tong University
- Inventors: Qigui Wang; Wenying Yang; Bing Ye
- Web page: https://patentgrep.com/patent/US20230145566A1

## CPC

- B22D 1/00: Treatment of fused masses in the ladle or the supply runners before casting {(for continuous casting B22D11/10; metallurgical processing, e.g. refining of iron or other metal C21, C22, C25C)}
- C22C 1/026: {Alloys based on aluminium}
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- C22C 21/02: with silicon as the next major constituent
- C22F 1/043: of alloys with silicon as the next major constituent
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

A method of eliminating microstructure inheritance of hypereutectic aluminum-silicon alloys. The method includes heating a first amount of the Al—Si alloy to a predetermined temperature above a liquidus temperature of the Al—Si alloy to form a first amount melt; holding the first amount melt at the predetermined temperature for a predetermined amount of time; stirring the first amount melt during the predetermined amount of time; heating a second amount of the Al—Si alloy above the liquidus temperature of the Al—Si alloy to form a second amount melt; and mixing the first amount melt and the second amount melt to form a processed Al—Si casting alloy. The predetermined temperature is between about 750° C. to 850° C. The predetermined amount of time is between 0.1 hour to 0.5 hour. The processed Al—Si casting alloy contains about 30 wt % to about 40 wt % of the first amount of the Al—Si alloy.

## Claims

### Claim 1

A method of eliminating microstructure inheritance in a hypereutectic aluminum-silicon (Al—Si) alloy, comprising:
heating a first amount of the Al—Si alloy to a predetermined temperature above a liquidus temperature of the Al—Si alloy to form a first amount melt;
holding the first amount melt at the predetermined temperature for a first predetermined amount of time; and
stirring the first amount melt for a second predetermined amount of time.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
heating a second amount of the Al—Si alloy above the liquidus temperature of the Al—Si alloy to form a second amount melt; and
mixing a stirred first amount melt with the second amount melt to form a processed Al—Si alloy.

### Claim 3 (depends on 1)

The method of claim 1, wherein the second predetermined amount of time is less than the first predetermined amount of time.

### Claim 4 (depends on 1)

The method of claim 1, wherein the predetermined temperature is greater than 800° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the predetermined temperature is between about 750° C. to about 850° C.

### Claim 6 (depends on 5)

The method of claim 5, wherein the predetermined temperature is between about 790° C. to about 810° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first predetermined amount of time is between 0.1 hour to 0.5 hour.

### Claim 8 (depends on 7)

The method of claim 7, wherein the second predetermined amount of time is equal to the predetermined amount of time.

### Claim 9 (depends on 1)

The method of claim 1, wherein stirring the first amount melt includes contact-less magnetic stirring.

### Claim 10 (depends on 1)

The method of claim 1, wherein the processed Al—Si alloy includes a first amount melt from about 25 weight percent (wt %) to about 50 w %.

### Claim 11

A method of casting a workpiece, comprising:
heating an Al—Si alloy to a processing temperature between about 750° C. to about 850° C. to form an Al—Si alloy melt;
maintaining the Al—Si alloy melt at the processing temperature for a processing time between about 0.1 hour to about 0.5 hour to form a processed Al—Si alloy melt; and
pouring the processed Al—Si alloy melt into a mold cavity defining the workpiece.

### Claim 12 (depends on 11)

The method of claim 11, further comprising:
mixing a non-processed Al—Si alloy melt to the processed Al—Si alloy melt to form a casting alloy mixture; and
pouring the casting alloy mixture into the mold cavity defining the workpiece.

### Claim 13 (depends on 11)

The method of claim 11, further comprising stirring the Al—Si alloy melt at the processing temperature for the processing time between about 0.1 hour to about 0.5 hour to form the processed Al—Si alloy melt.

### Claim 14 (depends on 13)

The method of claim 13, wherein the casting alloy mixture includes about 30 weight percent (wt %) to about 40 wt % of the processed Al—Si alloy melt.

### Claim 15 (depends on 14)

The method of claim 14, wherein the casting mixture includes about 35 wt % of the processed Al—Si alloy melt.

### Claim 16

A method of processing a hypereutectic aluminum-silicon (Al—Si) alloy for casting, comprising:
heating an Al—Si alloy to form an Al—Si alloy melt;
stirring a first portion of the Al—Si alloy melt for a predetermined time at a predetermined temperature to form a processed Al—Si alloy melt; and
mixing a second portion of the Al—Si alloy melt to the processed Al—Si alloy melt to form a processed Al—Si casting alloy.

### Claim 17 (depends on 16)

The method of claim 16, wherein the predetermined time is from about 0.1 hour to about 0.5 hour.

### Claim 18 (depends on 16)

The method of claim 16, wherein the predetermined temperature is from about 750° C. to about 850° C.

### Claim 19 (depends on 16)

The method of claim 16, wherein the processed Al—Si casting alloy comprises about 30 weight percent (wt %) to about 40 wt % of the processed Al—Si alloy melt.

### Claim 20 (depends on 16)

The method of claim 16, wherein stirring the first portion of the Al—Si alloy melt includes contact-less magnetic stirring.