# US 2023/0144521 A1 · Semiconductor device comprising electron blocking layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0144521 A1
- Document ID: US20230144521A1
- Status: Published application
- Kind: A1
- Application number: 18/094,185
- Filed: 2023-01-06
- Published: 2023-05-11
- Earliest claimed: 2017-01-26
- Assignees: Epistar Corporation
- Applicants: Epistar Corporation
- Inventors: Chia-Ming LIU; Chang-Hua HSIEH; Yung-Chung PAN; Chang-Yu TSAI; Ching-Chung HU; Ming-Pao CHEN; Chi SHEN; Wei-Chieh LIEN
- Web page: https://patentgrep.com/patent/US20230144521A1

## CPC

- H10H 20/822: Materials of the light-emitting regions
- H10H 20/812: within the light-emitting regions, e.g. having quantum confinement structures
- H10H 20/8162: {Current-blocking structures}
- H10H 20/825: containing nitrogen, e.g. GaN
- H10H 20/8252: {characterised by the dopants}
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

A semiconductor device comprises: a first semiconductor structure; a second semiconductor structure on the first semiconductor structure; an active region between the first semiconductor structure and the second semiconductor structure, wherein the active region comprises multiple alternating well layers and first barrier layers, wherein each of the first barrier layers has a band gap, the active region further comprises an upper surface facing the second semiconductor structure and a bottom surface opposite the upper surface; a first electron blocking layer between the second semiconductor structure and the active region, wherein the first electron blocking layer having a band gap greater than the band gap of one of the first barrier layers; a first aluminum-containing layer between the first electron blocking layer and the active region, wherein the first aluminum-containing layer has a first thickness and a band gap greater than the band gap of the first electron blocking layer; and a second aluminum-containing layer on a side of the first electron blocking layer opposite to the first aluminum-containing layer, wherein the second aluminum-containing layer has a second thickness and a band gap greater than the band gap of the first electron blocking layer; and wherein a ratio of the second thickness of the second aluminum-containing layer to the first thickness of the first aluminum-containing layer is between 0.8 and 1.2.

## Claims

### Claim 1

A semiconductor device, comprising:
a first semiconductor structure;
a second semiconductor structure on the first semiconductor structure;
an active region between the first semiconductor structure and the second semiconductor structure, wherein the active region comprises multiple alternating well layers and first barrier layers, wherein each of the first barrier layers has a band gap, the active region further comprises an upper surface facing the second semiconductor structure and a bottom surface opposite the upper surface;
a first electron blocking layer between the second semiconductor structure and the active region, wherein the first electron blocking layer having a band gap greater than the band gap of one of the first barrier layers;
a first aluminum-containing layer between the first electron blocking layer and the active region, wherein the first aluminum-containing layer has a first thickness and a band gap greater than the band gap of the first electron blocking layer; and
a second aluminum-containing layer on a side of the first electron blocking layer opposite to the first aluminum-containing layer, wherein the second aluminum-containing layer has a second thickness and a band gap greater than the band gap of the first electron blocking layer; and
wherein a ratio of the second thickness of the second aluminum-containing layer to the first thickness of the first aluminum-containing layer is between 0.8 and 1.2.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1, wherein the first electron blocking layer comprises InaAlbGa1-a-bN, the first aluminum-containing layer comprises IncAldGa(1-c-d)N, the second aluminum-containing layer comprises IneAlfGa1-e-fN, and 0≤c<a<1, 0≤e<a<1, 0<b<d<1, 0<b<f<1.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1, wherein e=0 and 0.5<f≤1.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1, wherein 0<a≤0.05.

### Claim 4 (depends on 1)

The semiconductor device according to claim 1, wherein the first aluminum-containing layer and the second aluminum-containing layer comprise the same material.

### Claim 5 (depends on 1)

The semiconductor device according to claim 1, wherein the first thickness and/or the second thickness ranges between 0.5 nm and 15 nm both inclusive.

### Claim 6 (depends on 1)

The semiconductor device according to claim 1, further comprising a second electron blocking region on the second aluminum-containing layer;
wherein the second electron blocking region having a band gap greater than the band gap of one of the first barrier layers and lower than the band gap of the first aluminum-containing layer.

### Claim 7 (depends on 6)

The semiconductor device according to claim 6, wherein the second electron blocking region comprises a single electron blocking layer comprising IncAldGa1-c-dN, wherein 0≤c≤0.005, 0<d≤0.5.

### Claim 8 (depends on 6)

The semiconductor device according to claim 6, wherein the second electron blocking region comprises alternating electron blocking layers and second barriers, a band gap of the electron blocking layer is higher than a band gap of each of the second barriers.

### Claim 9 (depends on 6)

The semiconductor device according to claim 6, wherein a concentration of a p-type dopant in the well layers neighboring the well layer closest to the second electron blocking region is not more than 1×1018/cm3.

### Claim 10 (depends on 1)

The semiconductor device according to claim 1, wherein the first electron blocking layer comprises InhAliGa1-h-iN and 0≤h≤0.05, 0<i≤0.3

### Claim 11 (depends on 1)

The semiconductor device according to claim 1, further comprising a confinement layer between the active region and the first aluminum-containing layer and having a thickness less than that of one of the first barriers.

### Claim 12 (depends on 11)

The semiconductor device according to claim 11, wherein the thickness of the confinement layer is not less than 3 nm.

### Claim 13 (depends on 1)

The semiconductor device according to claim 1, wherein a distance between the first aluminum-containing layer and the upper surface of the active region is at least 3 nm.

### Claim 14 (depends on 1)

The semiconductor device according to claim 1, further comprising a semiconductor stack between the active region and the first semiconductor structure, wherein the semiconductor stack comprises a first group stack comprising alternating first semiconductor layers and second semiconductor layers.

### Claim 15 (depends on 14)

The semiconductor device according to claim 14, wherein the semiconductor stack further comprises a second group stack on the first group stack, wherein the second group stack comprises alternating third semiconductor layers and fourth semiconductor layers.

### Claim 16 (depends on 15)

The semiconductor device according to claim 15, wherein the semiconductor stack further comprising an intermediate layer between the first group stack and the second group stack; and
each of the second semiconductor layer and the fourth semiconductor layer comprises indium, wherein the highest content of indium of the second semiconductor layer closest to the intermediate layer is higher than the highest content of indium of the fourth semiconductor layer closest to the intermediate layer.

### Claim 17 (depends on 1)

The semiconductor device according to claim 1, further comprising a p-type dopant above the bottom surface of the active region and comprising a concentration profile of the p-type dopant, wherein the concentration profile comprises a peak shape having a peak concentration value, wherein the peak concentration value lies at a distance of between 15 nm and 60 nm from the upper surface of the active region.

### Claim 18 (depends on 17)

The semiconductor device according to claim 17, wherein the peak shape comprises a full width at half maximum (FWHM) between 5 nm and 50 nm both inclusive.

### Claim 19 (depends on 17)

The semiconductor device according to claim 17, further comprising a topmost semiconductor surface, a distance between the topmost semiconductor surface and the peak concentration value is less than 200 nm.