# US 2023/0144381 A1 · Ferritic stainless steel having improved surface characteristics and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0144381 A1
- Document ID: US20230144381A1
- Status: Published application
- Kind: A1
- Application number: 17/918,192
- Filed: 2020-10-14
- Published: 2023-05-11
- Earliest claimed: 2020-04-28
- Assignees: Posco
- Applicants: Posco
- Inventors: Junghyun Kong; Jin-suk Kim; Manjin Ha; Hyunwoong Min; Hanhyuk Go; Mun-soo Lee
- Web page: https://patentgrep.com/patent/US20230144381A1

## CPC

- C22C 38/32: with boron
- C21D 1/26: Methods of annealing
- C21D 1/74: Methods of treatment in inert gas, controlled atmosphere, vacuum or pulverulent material
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 7/04: of the surface
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0242: {Flattening; Dressing; Flexing}
- C21D 8/0247: characterised by the heat treatment
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 8/0278: involving a particular surface treatment (C21D8/0294 takes precedence)
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C21D 2211/005: Ferrite
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

Disclosed are a ferrite-based stainless steel having improved surface characteristics and a method for manufacturing same. The ferrite-based stainless steel according to the present invention includes, in percent by weight (wt %), 0.001 to 0.05% of C, 0.001 to 0.05% of N, 0.1 to 1.0% of Si, 0.1 to 1.0% of Mn, 12.0 to 22.0% of Cr, 0.01 to 1.0% of Ti, 0.01 to 1.0% of Nb, and the remainder of Fe and unavoidable impurities, wherein micro flaws having a length of 100 μm or more are distributed at a density of 5 pieces/mm2 or less.

## Claims

### Claim 1

A ferrite-based stainless steel having improved surface characteristics comprising, in percent by weight (wt %), 0.001 to 0.05% of C, 0.001 to 0.05% of N, 0.1 to 1.0% of Si, 0.1 to 1.0% of Mn, 12.0 to 22.0% of Cr, 0.01 to 1.0% of Ti, 0.01 to 1.0% of Nb, and the remainder of Fe and unavoidable impurities,
wherein micro flaws having a length of 100 μm or more are distributed at a density of 5 pieces/mm2 or less.

### Claim 2 (depends on 1)

The ferrite-based stainless steel according to claim 1, further comprising at least one of 0.01 to 2.0% of Mo, 0.10% or less (excluding 0) of Al, 1.0% or less (excluding 0) of Cu, 0.01 to 0.3% of V, 0.01 to 0.3% of Zr, and 0.0010 to 0.0100% of B.

### Claim 3 (depends on 1)

The ferrite-based stainless steel according to claim 1, wherein an area rate of micro flaws is 2% or less.

### Claim 4 (depends on 1)

The ferrite-based stainless steel according to claim 1, wherein an area rate of micro flaws is 1.6% or less, and
micro flaws having a length of 100 μm or more are distributed at a density of 2 pieces/mm2 or less.

### Claim 5 (depends on 1)

The ferrite-based stainless steel according to claim 1, wherein a distinctness of reflected image is 90 or more in a rolling direction (L direction) and a direction (C direction) perpendicular to the rolling direction, respectively.

### Claim 6 (depends on 5)

The ferrite-based stainless steel according to claim 5, wherein a deviation of distinctness of reflected image between the L direction and the C direction is 5 or less.

### Claim 7

A method for manufacturing a ferrite-based stainless steel having improved surface characteristics, the method comprising:
hot rolling a slab comprising, in percent by weight (wt %), 0.001 to 0.05% of C, 0.001 to 0.05% of N, 0.1 to 1.0% of Si, 0.1 to 1.0% of Mn, 12.0 to 22.0% of Cr, 0.01 to 1.0% of Ti, 0.01 to 1.0% of Nb, and the remainder of Fe and unavoidable impurities and hot annealing the hot-rolled steel sheet;
cold rolling and cold annealing the hot-rolled, annealed steel sheet twice or more by controlling a roll diameter to 70 mm or less;
bright annealing the cold-rolled, annealed steel sheet; and
skin pass rolling the bright-annealed steel sheet,
wherein surface polishing treatment is introduced after hot annealing or after primary cold rolling.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the ferrite-based stainless steel further comprises at least one of 0.01 to 2.0% of Mo, 0.10% or less (excluding 0) of Al, 1.0% or less (excluding 0) of Cu, 0.01 to 0.3% of V, 0.01 to 0.3% of Zr, and 0.0010 to 0.0100% of B.

### Claim 9 (depends on 7)

The method according to claim 7, wherein the cold rolling comprises:
primary cold rolling performed at a reduction ratio of 40% or more; and
secondary cold rolling performed at a reduction ratio of 40% or more,
wherein a total reduction ratio is 80% or more.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the cold rolling further comprising tertiary cold rolling performed at a reduction ratio of 40% or more.

### Claim 11 (depends on 7)

The method according to claim 7, wherein a re-heating temperature is from 1050 to 1280° C., and a final rolling temperature is from 800 to 950° C. during the hot rolling.

### Claim 12 (depends on 7)

The method according to claim 7, wherein the surface polishing treatment is performed by removing the surface layer by 7 μm or more using a polishing belt having a roughness of #70 mesh or more.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the surface polishing treatment is performed once or twice.

### Claim 14 (depends on 7)

The method according to claim 7, wherein the cold annealing is performed at a temperature of 850 to 1,100° C.

### Claim 15 (depends on 7)

The method according to claim 7, wherein the bright annealing is performed at a temperature of 850 to 1,100° C.

### Claim 16 (depends on 7)

The method according to claim 7, wherein the skin pass rolling is performed using a work roll having an average roughness of #600 or more.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the skin pass rolling is performed twice to five times.

### Claim 18 (depends on 16)

The method according to claim 16, wherein micro flaws having a length of 100 μm or more are distributed at a density of 5 pieces/mm2 or less.

### Claim 19 (depends on 7)

The method according to claim 7, wherein a distinctness of reflected image is 90 or more in a rolling direction (L direction) and a direction (C direction) perpendicular to the rolling direction, respectively.

### Claim 20 (depends on 19)

The method according to claim 19, wherein a deviation of distinctness of reflected image between the L direction and the C direction is 5 or less.