# US 2023/0144242 A1 · Method for making yttrium aluminum garnet (yag) nanopowders

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0144242 A1
- Document ID: US20230144242A1
- Status: Published application
- Kind: A1
- Application number: 17/984,707
- Filed: 2022-11-10
- Published: 2023-05-11
- Earliest claimed: 2021-11-10
- Assignees: Wuhan Institute of Technology
- Applicants: Wuhan Institute of Technology
- Inventors: XINGMAO JIANG; SHENGJUN YI; LANG YANG; BIYI CHEN; JIN'E TAN; PINCAI LAI; LONG CHEN; JINJIAN PAN
- Web page: https://patentgrep.com/patent/US20230144242A1

## CPC

- C01F 17/34: Aluminates, e.g. YAlO3 or Y3-xGdxAl5O12
- C01F 17/10: Preparation or treatment, e.g. separation or purification
- C04B 35/44: based on aluminates
- C09K 11/7774: {Aluminates}
- C09K 11/7792: {Aluminates}
- C01P 2002/30: Three-dimensional structures
- C01P 2002/54: one element only
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/5454: nanometer sized, i.e. below 100 nm
- C04B 2235/764: Garnet structure A3B2(CO4)3
- C04B 2235/9646: Optical properties
- Y02B 20/00: Energy efficient lighting technologies, e.g. halogen lamps or gas discharge lamps
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02B: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO BUILDINGS, e.g. HOUSING, HOUSE APPLIANCES OR RELATED END-USER APPLICATIONS

## Abstract

A method for making yttrium aluminum garnet (YAG) nanopowders, includes mixing carbohydrate and organic amine in a container according to a first ratio, stirring the carbohydrate and organic amine in the container under a heating condition for 2 minutes to 120 minutes for melting the carbohydrate and the organic amine to obtain a clear and transparent mixed solution, adding yttrium salt and aluminum salt at a second ratio to the clear and transparent mixed solution, and stirring the yttrium salt, the aluminum salt, and the clear and transparent mixed solution in the container under the heating condition for 5 minutes to120 minutes to form a uniform molten mixture, heating the uniform molten mixture to dehydrate and carbonize the carbohydrate to obtain a dark brown fluffy solid, and performing a heat treatment on the dark brown fluffy solid at 800° C. to 1500° C. to obtain the YAG nanopowders.

## Claims

### Claim 1

A method for making yttrium aluminum garnet (YAG) nanopowders, comprising:
mixing carbohydrate and organic amine in a container according to a first ratio, stirring the carbohydrate and organic amine in the container under a heating condition approximately from 25° C. to 180° C. for 2 minutes to 120 minutes for melting the carbohydrate and the organic amine to obtain a clear and transparent mixed solution;
adding yttrium salt and aluminum salt at a second ratio to the clear and transparent mixed solution, and stirring the yttrium salt, the aluminum salt, and the clear and transparent mixed solution in the container under the heating condition approximately from 25° C. to 180° C. for 5 minutes to 120 minutes for dissolving the yttrium salt and the aluminum salt in the clear and transparent mixed solution to form a uniform molten mixture;
heating the uniform molten mixture to dehydrate and carbonize the carbohydrate to obtain a dark brown fluffy solid; and
performing a heat treatment on the dark brown fluffy solid at 800° C. to 1500° C. for 2 hours to 40 hours to obtain the YAG nanopowders.

### Claim 2 (depends on 1)

The method of claim 1, wherein adding the yttrium salt and the aluminum salt at the second ratio to the clear and transparent mixed solution includes:
adding rare earth salt or transition metal salt at a third ratio to the clear and transparent mixed solution.

### Claim 3 (depends on 2)

The method of claim 2, wherein the third ratio includes a molar ratio between rare earth element in the rare earth salt or transition metal element in the transition metal salt and yttrium in the yttrium salt as 1:(10-300).

### Claim 4 (depends on 2)

The method of claim 2, wherein the third ratio includes a ratio between total moles of yttrium in the yttrium salt, aluminum in the aluminum salt, and rare earth element in the rare earth salt or transition metal element in the transition metal salt, and moles of the carbohydrate as (0.2-3):1.

### Claim 5 (depends on 2)

The method of claim 2, wherein:
the yttrium salt includes at least one of nitrate, sulfate, oxalate, acetate, phosphate, hypochlorite, or halide salt;
the aluminum salt includes at least one of nitrate, sulfate, oxalate, acetate, phosphate, hypochlorite, or halide salt;
the rare earth salt or transition metal salt includes at least one of nitrate, sulfate, oxalate, acetate, phosphate, hypochlorite, or halide salt.

### Claim 6 (depends on 2)

The method of claim 2, wherein heating the uniform molten mixture to dehydrate and carbonize the carbohydrate to obtain the dark brown fluffy solid includes:
microwaving the uniform molten mixture to dehydrate and carbonize the carbohydrate to provide a carbon templet to cause the yttrium salt, the aluminum salt, and the rare earth salt or transition metal salt to be evenly distributed on the carbon templet.

### Claim 7 (depends on 6)

The method of claim 6, wherein performing the heat treatment on the dark brown fluffy solid at 800° C. to 1500° C. for 2 hours to 40 hours to obtain the YAG nanopowders includes:
performing the heat treatment on the dark brown fluffy solid to remove the carbon templet.

### Claim 8 (depends on 1)

The method of claim 1, wherein:
the carbohydrate includes at least one of glucose, sucrose, fructose, lactose, starch, maltose, or ribose;
the organic amine includes at least one of aliphatic amine, alcohol amine, amide, alicyclic amine, aromatic amine, or naphthalene amine; and
the first ratio includes a mass ratio of the carbohydrate and the organic amine as 1:(0.1-50).

### Claim 9 (depends on 1)

The method of claim 1, wherein the second ratio includes a molar ratio between yttrium in the yttrium salt and aluminum in the aluminum salt as 1:(1-4).

### Claim 10 (depends on 1)

The method of claim 1, wherein heating the uniform molten mixture to dehydrate and carbonize the carbohydrate to obtain the dark brown fluffy solid includes:
heating the uniform molten mixture to dehydrate and carbonize the carbohydrate to obtain the dark brown fluffy solid using at least one of high temperature carbonization, hydrothermal carbonization, or microwave carbonization.

### Claim 11 (depends on 1)

The method of claim 1, wherein performing the heat treatment on the dark brown fluffy solid at 800° C. to 1500° C. for 2 hours to 40 hours to obtain the YAG nanopowders includes:
performing the heat treatment on the dark brown fluffy solid in at least one of an air atmosphere, an oxygen atmosphere, or an atmosphere with first inert gas and then air or oxygen.

### Claim 12 (depends on 1)

The method of claim 1, wherein the obtained YAG nanopowders have a particle size of 20 nanometers to 5000 nanometers.

### Claim 13 (depends on 1)

The method of claim 1, wherein the obtained YAG nanopowders have a particle size of 20 nanometers to 100 nanometers.

### Claim 14 (depends on 1)

The method of claim 1, wherein heating the uniform molten mixture to dehydrate and carbonize the carbohydrate to obtain the dark brown fluffy solid includes:
microwaving the uniform molten mixture to dehydrate and carbonize the carbohydrate to provide a carbon templet to cause the yttrium salt and the aluminum salt to be evenly distributed on the carbon templet.

### Claim 15 (depends on 12)

The method of claim 12, wherein performing the heat treatment on the dark brown fluffy solid at 800° C. to 1500° C. for 2 hours to 40 hours to obtain the YAG nanopowders includes:
performing the heat treatment on the dark brown fluffy solid to remove the carbon templet.