# US 2023/0143678 A1 · Method and system for depositing boron nitride using pulsed chemical vapor deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0143678 A1
- Document ID: US20230143678A1
- Status: Published application
- Kind: A1
- Application number: 17/966,660
- Filed: 2022-10-14
- Published: 2023-05-11
- Earliest claimed: 2021-10-19
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: René Henricus Jozef Vervuurt; Timothee Blanquart
- Web page: https://patentgrep.com/patent/US20230143678A1

## CPC

- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/342: {Boron nitride}
- C23C 16/45536: {Use of plasma, radiation or electromagnetic fields}
- C23C 16/5096: {Flat-bed apparatus}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/68: Organic materials, e.g. photoresists
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Methods and systems for depositing a boron nitride film on a substrate are disclosed. More particularly, the disclosure relates to methods and systems that can be used for depositing a boron nitride film by a pulsed CVD process.

## Claims

### Claim 1

A cyclic deposition method of depositing a boron nitride film on a surface of a substrate, the method comprising:
providing the substrate in a reaction chamber;
providing a reactant into the reaction chamber;
forming a plasma using the reactant; and
pulsing a precursor into the reaction chamber to thereby form the boron nitride film,
wherein the precursor comprises boron and nitrogen.

### Claim 2 (depends on 1)

The method of claim 1, wherein the precursor consists of boron, nitrogen, and hydrogen.

### Claim 3 (depends on 1)

The method of claim 1, wherein the precursor does not comprise carbon.

### Claim 4 (depends on 1)

The method of claim 1, wherein the precursor comprises borazine or a substituted borazine.

### Claim 5 (depends on 1)

The method of claim 1, wherein the reactant comprises an argon-containing gas or a helium-containing gas.

### Claim 6 (depends on 5)

The method of claim 5, wherein the argon or helium-containing gas further comprises hydrogen or nitrogen.

### Claim 7 (depends on 6)

The method of claim 6, wherein the reactant comprises at least one of 30-99% argon or helium and 1- 70% hydrogen.

### Claim 8 (depends on 6)

The method of claim 6, wherein the reactant comprises at least one of 10-90% argon and 10-90% nitrogen.

### Claim 9 (depends on 1)

The method of claim 1, wherein the reactant is provided continuously during the pulsing of the precursor into the reaction chamber.

### Claim 10 (depends on 1)

The method of claim 1, wherein the plasma is provided continuously during the pulsing of the precursor into the reaction chamber.

### Claim 11 (depends on 1)

The method of claim 1, wherein the plasma is provided directly using capacitively coupled plasma.

### Claim 12 (depends on 1)

The method claim 1, wherein the method comprises a cyclical CVD process.

### Claim 13 (depends on 1)

The method of claim 1, wherein a pressure within the reaction chamber is between about 150 Pa and about 300 Pa.

### Claim 14 (depends on 1)

The method of claim 1, wherein the temperature within the reaction chamber is between about 300 and about 500° C.

### Claim 15 (depends on 1)

The method of claim 1, wherein the plasma is provided using an RF power of between about 75 W and about 300 W for a 300 mm substrate.

### Claim 16 (depends on 1)

The method of claim 1, wherein the boron nitride film is deposited at a rate of greater than 0.03 nm/min.

### Claim 17 (depends on 1)

The method of claim 1, wherein the boron nitride film is deposited at a rate of greater than 0.05 nm/min.

### Claim 18 (depends on 1)

A structure comprising a boron nitride film formed according to the method of claim 1.

### Claim 19 (depends on 18)

The structure of claim 18, wherein the dielectric constant of the boron nitride film is less than 3.5.

### Claim 20 (depends on 18)

The structure of claim 18, wherein the dielectric constant of the boron nitride film is less than 3.0.