# US 2023/0142982 A1 · Process for Forming a Laminate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0142982 A1
- Document ID: US20230142982A1
- Status: Published application
- Kind: A1
- Application number: 17/296,156
- Filed: 2019-11-27
- Published: 2023-05-11
- Earliest claimed: 2018-11-28
- Assignees: Dow Global Technologies LLC
- Applicants: Dow Global Technologies LLC
- Inventors: Rui Xie; Jie Wu
- Web page: https://patentgrep.com/patent/US20230142982A1

## CPC

- B32B 37/0038: {involving application of liquid to the layers prior to lamination, e.g. wet laminating (B32B37/12 takes precedence)}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 15/085: comprising polyolefins
- B32B 15/09: comprising polyesters
- B32B 27/08: of synthetic resin
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/36: comprising polyesters
- B32B 37/12: characterised by using adhesives
- C08G 18/10: Prepolymer processes involving reaction of isocyanates or isothiocyanates with compounds having active hydrogen in a first reaction step
- C08G 18/3814: {Polyamines}
- C08G 18/3885: {Phosphate compounds}
- C08G 18/4804: {Two or more polyethers of different physical or chemical nature}
- C08G 18/482: {Mixtures of polyethers containing at least one polyether containing nitrogen}
- C08G 18/4854: {Polyethers containing oxyalkylene groups having four carbon atoms in the alkylene group}
- C08G 18/5027: {directly linked to carbocyclic groups}
- C08G 18/6666: {Compounds of group C08G18/48 or C08G18/52}
- C08G 18/667: {with compounds of group C08G18/32 or polyamines of C08G18/38}
- C08G 18/7671: {containing only one alkylene bisphenyl group}
- C09J 5/04: involving separate application of adhesive ingredients to the different surfaces to be joined
- C09J 175/04: Polyurethanes
- C09J 175/06: from polyesters
- C09J 175/08: from polyethers
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- B32B 2037/1253: {curable adhesive}
- B32B 2255/06: on metal layer
- B32B 2255/10: on synthetic resin layer or on natural or synthetic rubber layer
- B32B 2255/26: Polymeric coating
- B32B 2307/748: Releasability
- B32B 2309/02: Temperature
- B32B 2309/04: Time
- B32B 2309/12: Pressure
- B32B 2311/24: Aluminium
- B32B 2323/04: Polyethylene
- B32B 2367/00: Polyesters, e.g. PET, i.e. polyethylene terephthalate
- C09J 2400/166: in the pretreated surface to be joined
- C09J 2467/008: in the pretreated surface to be joined
- C09J 2475/00: Presence of polyurethane
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

The present disclosure provides a process for forming a laminate. The process includes (A) uniformly applying an isocyanate component to a first substrate, the isocyanate component containing an isocyanate compound; (B) uniformly applying an isocyanate-reactive component to a second substrate, the isocyanate-reactive component containing an amine-terminated compound; (C) bringing the first substrate and the second substrate together, thereby mixing and reacting the isocyanate component and the isocyanate-reactive component to form an adhesive composition between the first substrate and the second substrate; (D) curing the adhesive composition to bond the first substrate and the second substrate; and (E) forming the laminate.

## Claims

### Claim 1

A process for forming a laminate comprising:
(A) uniformly applying an isocyanate component to a first substrate, the isocyanate component comprising an isocyanate compound;
(B) uniformly applying an isocyanate-reactive component to a second substrate, the isocyanate-reactive component comprising an amine-terminated compound;
(C) bringing the first substrate and the second substrate together, thereby mixing and reacting the isocyanate component and the isocyanate-reactive component to form an adhesive composition between the first substrate and the second substrate;
(D) curing the adhesive composition to bond the first substrate and the second substrate; and
(E) forming the laminate.

### Claim 2 (depends on 1)

The process of claim 1 comprising providing the isocyanate-reactive component comprising a diamine-terminated polyether.

### Claim 3 (depends on 1)

The process of claim 1 comprising providing the isocyanate-reactive component comprising from 20 wt % to 100 wt % of the amine-terminated compound, based on the total weight of the isocyanate-reactive component.

### Claim 4 (depends on 1)

The process of claim 1 comprising providing the isocyanate-reactive component comprising the amine-terminated compound and a polyol compound.

### Claim 5 (depends on 1)

The process of claim 1 comprising providing the isocyanate-reactive component comprising the amine-terminated compound, a phosphate ester polyol, and a polyether polyol.

### Claim 6 (depends on 1)

The process of claim 1, comprising providing the isocyanate component comprising an isocyanate prepolymer having an isocyanate content by weight from 3 wt % to 25 wt %.

### Claim 7 (depends on 1)

The process of claim 1, comprising
applying the isocyanate component to the first substrate at an isocyanate coat weight;
applying the isocyanate-reactive component to the second substrate at an isocyanate-reactive coat weight;
determining the Isocyanate:Isocyanate-Reactive Stoichiometric Ratio by calculating the molar ratio of isocyanate groups in the isocyanate component to the combined amount of amine groups and hydroxyl groups in the isocyanate-reactive component;
adjusting the isocyanate coat weight and the amine-terminated coat weight to obtain an Isocyanate:Isocyanate-Reactive Stoichiometric Ratio from 1.0 to 5.0.

### Claim 8 (depends on 1)

The process of claim 1, comprising
applying the isocyanate component at a viscosity at 25° C. from 5,000 cP to 20,000 cP;
forming an isocyanate-component layer on the first substrate having a coat weight from 0.1 g/m2 to 20 g/m2;
applying the isocyanate-reactive component at a viscosity at 25° C. from 1,000 cP to 20,000 cP; and
forming an isocyanate-reactive component layer on the second substrate having an weight from 0.1 g/m2 to 20 g/m2.

### Claim 9 (depends on 1)

The process of claim 1, comprising curing the adhesive composition at a temperature from 20° C. to 25° C. for a period from 60 minutes to 10 days.

### Claim 10 (depends on 1)

The process of claim 1, comprising
bringing the first substrate and the second substrate together at a temperature from 20° C. to 30° C.;
contacting the isocyanate component with the isocyanate-reactive component; and
applying a pressure from 5 psi to 100 psi to the first substrate and the second substrate.

### Claim 11 (depends on 1)

The process of claim 1, comprising
(A) uniformly applying the isocyanate component to the first substrate, the first substrate comprising a first film comprising a metal foil layer;
(B) uniformly applying the isocyanate-reactive component to the second substrate, the second substrate comprising a second film comprising an ethylene-based polymer layer;
(D) curing the adhesive composition at a temperature from 15° C. to 50° C. for a period of 90 minutes; and
(E) forming the laminate, the laminate having a bond strength of greater than 0.05 N/15 mm.

### Claim 12 (depends on 1)

The process of claim 1, comprising
(A) uniformly applying the isocyanate component to the first substrate, the first substrate comprising a first film comprising a polyethyleneterephthalate layer;
(B) uniformly applying the isocyanate-reactive component to the second substrate, the second substrate comprising a second film comprising an ethylene-based polymer layer;
(D) curing the adhesive composition at a temperature from 20° C. to 25° C. for a period of 90 minutes; and
(E) forming the laminate, the laminate having a bond strength of greater than 0.05 N/15 mm.

### Claim 13 (depends on 1)

A laminate formed by the process of claim 1.

### Claim 14

A two-component solvent-less adhesive composition comprising:
(A) an isocyanate component adapted for application to a first substrate, the isocyanate component comprising an isocyanate prepolymer;
(B) an isocyanate-reactive component adapted for application to a second substrate, the isocyanate-reactive component comprising an amine-terminated compound;
the two-component solvent-less adhesive composition having Isocyanate:Isocyanate-Reactive Stoichiometric Ratio from 1.0 to 5.0.

### Claim 15

A laminate comprising:
a first substrate;
a second substrate;
a solvent-less adhesive layer between the first substrate and the second substrate, the solvent-less adhesive layer comprising
(A) an isocyanate component comprising an isocyanate prepolymer; and
(B) an isocyanate-reactive component comprising an amine-terminated compound.