# US 2023/0142939 A1 · MANUFACTURING METHOD OF SiC SUBSTRATE

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0142939 A1
- Document ID: US20230142939A1
- Status: Published application
- Kind: A1
- Application number: 18/054,204
- Filed: 2022-11-10
- Published: 2023-05-11
- Earliest claimed: 2021-11-11
- Assignees: Disco Corporation
- Applicants: Disco Corporation
- Inventors: Katsuyoshi KOJIMA
- Web page: https://patentgrep.com/patent/US20230142939A1

## CPC

- B24B 7/228: {for grinding thin, brittle parts, e.g. semiconductors, wafers (grinding edges of thin, brittle parts B24B9/065)}
- B24B 9/065: {of thin, brittle parts, e.g. semiconductors, wafers}
- B24B 37/08: for double side lapping
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS

## Abstract

A method of manufacturing a SiC substrate includes grinding a sliced SiC substrate on a side of its front surface on which a Si-face is exposed, grinding the sliced SiC substrate on a side of its back surface on which a C-face is exposed, such that the back surface has an arithmetic mean height Sa of 1 nm or less, and then polishing the sliced SiC substrate on the side of only the front surface and not on the side of the back surface. In a case where the side of the back surface is ground as described above, the SiC substrate can be prevented from being warped even if the side of the back surface is not polished. This can shorten the manufacturing lead time for the SiC substrate used for the manufacture of power devices or the like and can also reduce the manufacturing cost.

## Claims

### Claim 1

A manufacturing method of a silicon carbide substrate, comprising:
a separation step of separating a sliced silicon carbide substrate from a silicon carbide ingot such that a silicon-face is exposed on a front surface and a carbon-face is exposed on a back surface;
a grinding step of, after the separation step, grinding the sliced silicon carbide substrate on both a side of the front surface and a side of the back surface of the sliced silicon carbide substrate; and
a polishing step of, after the grinding step, polishing the sliced silicon carbide substrate only on the side of the front surface and not on the side of the back surface,
wherein the grinding step includes
a first grinding step of grinding the sliced silicon carbide substrate on the side of the front surface, and
a second grinding step of grinding the sliced silicon carbide substrate on the side of the back surface, and
in the second grinding step, the sliced silicon carbide substrate is ground on the side of the back surface such that the back surface has an arithmetic mean height Sa of 1 nm or less.

### Claim 2 (depends on 1)

The manufacturing method of a silicon carbide substrate according to claim 1, wherein the second grinding step is performed using grinding stones that contain abrasive grits having an average grit size of 0.3 μm or smaller.