# US 2023/0142926 A1 · Semiconductor device patterning methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0142926 A1
- Document ID: US20230142926A1
- Status: Published application
- Kind: A1
- Application number: 18/096,347
- Filed: 2023-01-12
- Published: 2023-05-11
- Earliest claimed: 2020-10-27
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Yong Wang; Doreen Wei Ying Yong; Bhaskar Jyoti Bhuyan; John Sudijono
- Web page: https://patentgrep.com/patent/US20230142926A1

## CPC

- C23C 16/0227: {by cleaning or etching}
- C23C 16/345: {Silicon nitride}
- B05D 1/327: {Masking layer made of washable film}
- B05D 1/60: {Deposition of organic layers from vapour phase (vapour phase deposition in general C23C14/00, C23C16/00)}
- C23C 16/04: Coating on selected surface areas, e.g. using masks
- C23C 16/56: After-treatment
- C23C 22/77: Controlling or regulating of the coating process
- C23C 22/82: After-treatment
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

Methods of patterning semiconductor devices comprising selective deposition methods are described. A blocking layer is deposited on a metal surface of a semiconductor device before deposition of a dielectric material on a dielectric surface. Methods include exposing a substrate surface including a metal surface and a dielectric surface to a heterocyclic reactant comprising a headgroup and a tailgroup in a processing chamber and selectively depositing the heterocyclic reactant on the metal surface to form a passivation layer, wherein the heterocyclic headgroup selectively reacts and binds to the metal surface.

## Claims

### Claim 1

A semiconductor device patterning method comprising:
in a substrate processing chamber, exposing a semiconductor device substrate surface including a metal surface and a dielectric surface to a vapor phase heterocyclic reactant comprising a heterocyclic headgroup and a tailgroup;
in the substrate processing chamber, selectively depositing the vapor phase heterocyclic reactant on the metal surface to cover the metal surface with a blocking layer, wherein the heterocyclic headgroup selectively binds to the metal surface;
in the substrate processing chamber, depositing a dielectric material on the dielectric surface not covered by the blocking layer at a dielectric deposition temperature up to 350° C. at which the heterocyclic reactant remains bound to the metal surface and maintains stability; and
decomposing the blocking layer covering the metal surface in the substrate processing chamber at temperature higher than the dielectric deposition temperature to form a pattern on the semiconductor device substrate surface.

### Claim 2 (depends on 1)

The method of claim 1, wherein selectively depositing the vapor phase heterocyclic reactant on the metal surface and depositing the dielectric material on the dielectric surface not covered by the blocking layer utilize an atomic layer deposition process in the substrate processing chamber.

### Claim 3 (depends on 2)

The method of claim 2, wherein the heterocyclic headgroup comprises one or more of N, O, S, Se and P atoms.

### Claim 4 (depends on 2)

The method of claim 2, wherein the heterocyclic headgroup comprises one or more of pyrrole, pyrrolidine, pyrazole, imidazole, furan, biimidazole, thiophene, thiazole, thiadiazole, pyridine, pyridazine, pyrimidine, quinoxaline, indazole, thiazine, phosphinine, phosphinoline, and phosphole.

### Claim 5 (depends on 2)

The method of claim 2, wherein the tailgroup comprises one or more of a phenyl group and a carbon chain.

### Claim 6 (depends on 5)

The method of claim 5, wherein the carbon chain has a length is in the range of from 1 to 50 carbon atoms.

### Claim 7 (depends on 5)

The method of claim 5, wherein the tailgroup has a length in the range of from 1 Å to 75 Å.

### Claim 8 (depends on 5)

The method of claim 5, wherein tailgroup has one or more substitute R groups in the range of from 1 to 50.

### Claim 9 (depends on 8)

The method of claim 8, wherein the substitute R group comprises one or more of alkyl, cycloalkyl, aryl groups which may be linear or branched containing the following bonds carbon-carbon single/double/triple bonds.

### Claim 10 (depends on 2)

The method of claim 2, wherein the metal surface comprises one or more of copper, cobalt, nickel, tungsten, vanadium, ruthenium, chromium, iron, platinum, gold, silver, molybdenum, gallium, indium, indium tin oxide, fluorine doped tin oxide and Al-doped zinc oxide.

### Claim 11 (depends on 10)

The method of claim 10, wherein the heterocyclic reactant remains bound to the metal surface at a higher temperature, wherein the higher temperature is in the range of 50° C. to 350° C.

### Claim 12 (depends on 5)

The method of claim 5, wherein the carbon chain has a length and the tailgroup has substitutions such that a sum of the carbon chain length and tailgroup substitutions is not greater than 50 carbon atoms.

### Claim 13 (depends on 2)

The method of claim 2, wherein the density of the blocking layer is in the range of from 1×1013 to 1×1014 molecules per cm2.

### Claim 14 (depends on 2)

The method of claim 2, wherein the thickness of the blocking layer is in the range of from 5 Å to 100 Å.

### Claim 15 (depends on 2)

The method of claim 2, wherein the dielectric surface comprises one or more of SiOx, SixNy, Si, SiON, AlOx, Al2O3, HfOx, ZrO2, TiOx, TiN, TaxO5, Ta2O5, Y2O3, La2O3, AN, MgO, CaF2, LiF, SrO, SiC, BaO, HfSiO4, LaAlO3, Nb2O5, BaTiO3, SrTiO3, Bi4Ti3O12, Pb(Zr, Ti)O3, CaCu3Ti4O12, LiNbO3, BaTiO3, LiNbO3 and KNbO3.

### Claim 16 (depends on 15)

The method of claim 15, wherein the vapor pressure of the heterocyclic reactant is in the range of from 0.00001 mmHg to 150 mmHg at 25° C.

### Claim 17

A semiconductor device patterning method comprising:
in a substrate processing chamber, exposing a semiconductor device substrate surface including a metal surface and a dielectric surface to a heterocyclic reactant comprising a headgroup and a tailgroup;
selectively depositing the heterocyclic reactant on the metal surface to form a blocking layer, wherein the heterocyclic headgroup selectively binds to the metal surface and wherein the heterocyclic headgroup comprises one or more of N, O, S, Se and P atoms, and wherein the tailgroup comprises one or more of a phenyl group and a carbon chain and the carbon chain has a length is in the range of from 1 to 50 carbon atoms;
in the substrate processing chamber, depositing a dielectric material on the dielectric surface not covered by the blocking layer at a dielectric deposition temperature; and
decomposing the blocking layer covering the metal surface in the substrate processing chamber at temperature higher than the dielectric deposition temperature to form a pattern on the semiconductor device substrate surface.

### Claim 18 (depends on 17)

The method of claim 17, wherein selectively depositing the vapor phase heterocyclic reactant on the metal surface and depositing the dielectric material on the dielectric surface not covered by the blocking layer utilize an atomic layer deposition process in the substrate processing chamber.

### Claim 19 (depends on 18)

The method of claim 18, wherein the density of the blocking layer is in the range of from 1×1013 to 1×1014 molecules per cm2.

### Claim 20 (depends on 17)

A non-transitory computer readable medium including instructions, that, when executed by a controller of a substrate processing chamber, causes the substrate processing chamber to perform the process of claim 17.