# US 2023/0136571 A1 · Heat-curable powder coating composition and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0136571 A1
- Document ID: US20230136571A1
- Status: Published application
- Kind: A1
- Application number: 17/912,530
- Filed: 2021-03-31
- Published: 2023-05-04
- Earliest claimed: 2021-02-01
- Assignees: Foshan Yikeju New Material Co., Ltd.
- Applicants: Foshan Yikeju New Material Co., Ltd.
- Inventors: Ming Wu
- Web page: https://patentgrep.com/patent/US20230136571A1

## CPC

- C09D 5/033: {characterised by the additives}
- C08G 18/246: {containing also tin-carbon bonds}
- C08G 18/6715: {Unsaturated monofunctional alcohols or amines}
- C08G 18/672: {Esters of acrylic or alkyl acrylic acid having only one group containing active hydrogen}
- C08G 18/73: acyclic
- C08G 18/755: {and at least one isocyanate or isothiocyanate group linked to a secondary carbon atom of the cycloaliphatic ring, e.g. isophorone diisocyanate}
- C08G 18/8166: {with unsaturated monofunctional alcohols or amines}
- C08G 18/8175: {with esters of acrylic or alkylacrylic acid having only one group containing active hydrogen}
- C08G 63/54: the acids or hydroxy compounds containing carbocyclic rings
- C08G 63/676: in which at least one of the two components contains aliphatic unsaturation
- C09D 7/63: organic
- C09D 7/65: macromolecular (C09D7/41-C09D7/48 take precedence)
- C09D 7/80: Processes for incorporating ingredients
- C09D 167/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C09D167/06 takes precedence)
- C09D 167/06: Unsaturated polyesters having carbon-to-carbon unsaturation
- C09D 175/16: having terminal carbon-to-carbon unsaturated bonds
- C08G 2150/20: Compositions for powder coatings
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

The invention relates to the field of powder coatings, and specifically discloses a heat-curable powder coating composition and a preparation method thereof. The powder coating composition comprises: i) component A comprising at least one amorphous solid polyester resin compound having a Michael donor reactive group; ii) component B comprising at least one amorphous ethylenically unsaturated solid polyester resin with a Michael acceptor reactive group; iii) component C comprising at least one (semi) crystalline solid reactive diluent; iv) component D comprising at least one epoxy group-containing solid substance; v) component E comprising at least one basic catalyst. The present invention also discloses a preparation method of the above heat-curable powder coating composition. By adopting the invention, ultra-low temperature curing can be realized. The curing temperature is as low as 90-110° C., and the curing time is short.

## Claims

### Claim 1

A heat-curable powder coating composition, comprising:
i) component A, comprising at least one amorphous solid polyester resin having a Michael donor reactive group;
ii) component B, comprising at least one amorphous ethylenically unsaturated solid polyester resin having a Michael acceptor reactive group;
iii) component C, comprising at least one (semi) crystalline solid reactive diluent;
iv) component D, comprising at least one solid substance containing an epoxy group; and
v) component E, comprising at least one basic catalyst.

### Claim 2 (depends on 1)

The heat-curable powder coating composition according to claim 1, wherein component C comprises at least one (semi) crystalline vinyl functionalized polyurethane resin.

### Claim 3 (depends on 2)

The heat-curable powder coating composition according to claim 2, wherein component C comprises at least one (semi) crystalline vinyl ether functionalized polyurethane resin containing a vinyl ether functional group.

### Claim 4 (depends on 3)

The heat-curable powder coating composition according to claim 3, wherein component C is a product of a reaction between a compound containing a vinyl ether group or a vinyl ester group or a vinyl ether-ester group and/or a derivative of the compound, and an isocyanate group-containing compound and/or a derivative of the isocyanate group-containing compound.

### Claim 5 (depends on 4)

The heat-curable powder coating composition according to claim 4, wherein the isocyanate group-containing compound is one or more selected from the group consisting of toluene diisocyanate, hexamethylene diisocyanate and isophorone diisocyanate;
wherein the toluene diisocyanate is a mixture of toluene 2,6-diisocyanate and toluene 2,4-diisocyanate;
wherein the compound containing the vinyl ether group is one or more selected from the group consisting of 6-hydroxyhexyl vinyl ether, 4-hydroxybutyl vinyl ether, 2-hydroxyethyl vinyl ether, and diethylene glycol monovinyl ether.

### Claim 6

(canceled)

### Claim 7

(canceled)

### Claim 8 (depends on 4)

The heat-curable powder coating composition according to claim 4, wherein component C is obtained by the following method:
adding a compound with a vinyl ether group, an auxiliary agent and water into a reaction apparatus, stirring under nitrogen protection, and heating to 35-50° C.;
slowly adding an isocyanate group-containing compound dropwise to the reaction apparatus at a temperature of 35-50° C.; and
after adding the isocyanate group-containing compound, keeping a temperature of the reaction apparatus lower than 110° C. for 30 minutes, and then removing low molecular weight volatiles by vacuuming to obtain a final product.

### Claim 9 (depends on 4)

The heat-curable powder coating composition according to claim 4, wherein component C satisfies at least one of the following conditions:
a. component C has a number average molecular weight Mn of 100-8000 Da;
b. the vinyl ether functional group of component C has an equivalent weight of 100-4000 g/mol;
c. component C has a melting point of 30-110° C. and a crystallization point of 20-80° C.; and
d. component C has a viscosity of 0.01-20 Pa.s at 100° C.

### Claim 10 (depends on 1)

The heat-curable powder coating composition according to claim 1, wherein component A comprises at least one amorphous solid polyester resin having 2 or more C—H Michael donor reactive groups, and the molecular structure of the group is as follows:
wherein R is H, alkyl or aryl; X and Y are identical or different groups, X and Y are alkoxy, alkyl, aryl or aralkyl.

### Claim 11

(canceled)

### Claim 12

(canceled)

### Claim 13 (depends on 1)

The heat-curable powder coating composition according to claim 1, wherein component B comprises at least one amorphous ethylenically unsaturated solid polyester resin having 2 or more unsaturated C═C Michael acceptor reactive groups.

### Claim 14

(canceled)

### Claim 15

(canceled)

### Claim 16 (depends on 1)

The heat-curable powder coating composition according to claim 1, wherein
component D is an epoxy resin containing an epoxy group, an acrylic polyester containing an epoxy group, or an epoxy curing agent.

### Claim 17

(canceled)

### Claim 18

(canceled)

### Claim 19 (depends on 1)

The heat-curable powder coating composition according to claim 1, wherein component E comprises at least one basic catalyst promoting a ring-opening reaction of an epoxy resin at 70-100° C.

### Claim 20

(canceled)

### Claim 21 (depends on 1)

The heat-curable powder coating composition according to claim 1, wherein a total amount of component A, component B and component C added is 100 wt%;
component D is added in an amount of 0.1-50 wt% of the total amount of component A, component B and component C;
component E is added in an amount of 0.05-30 wt% of the total amount of component A, component B and component C.

### Claim 22

(canceled)

### Claim 23

(canceled)

### Claim 24

(canceled)

### Claim 25

(canceled)

### Claim 26 (depends on 1)

A preparation method of the heat-curable powder coating composition according to claim 1, comprising:
1) dividing component D into component F and component G with the same or different weights;
2) mixing component, A, component B, component C, component E and component F together to obtain a first premix;
3) mixing-extruding the first premix, and cooling to ambient temperature to obtain an extrudate;
4) pulverizing the extrudate after cooling to obtain a first powder particle;
5) pulverizing component G to obtain a second powder particle; and
6) mixing the first powder particle and the second powder particle, and pulverizing to obtain a powder coating composition as a final product.

### Claim 27 (depends on 26)

The preparation method of the heat-curable powder coating composition according to claim 26, wherein an amount of component F used is 1-35 wt% of a total amount of component A, component B and component C; and an amount of component G used is 1-35 wt% of the total amount of component A, component B and component C.

### Claim 28

(canceled)

### Claim 29

(canceled)