- Applicants: ExxonMobil Chemical Patents Inc.
- Inventors: Xiao-Dong Pan; Alan A. Galuska; Feng Li; Nieves Hernandez, JR.
- Web page: https://patentgrep.com/patent/US20230130953A1

## CPC

- B60C 1/0016: {Compositions of the tread}
- C08L 9/06: Copolymers with styrene
- C08F 212/08: Styrene
- C08F 236/06: Butadiene
- C08G 61/08: of carbocyclic compounds containing one or more carbon-to-carbon double bonds in the ring
- C08K 3/04: Carbon
- C08K 3/36: Silica
- C08L 65/00: Compositions of macromolecular compounds obtained by reactions forming a carbon-to-carbon link in the main chain (C08L7/00 - C08L57/00, C08L61/00 take precedence); Compositions of derivatives of such polymers
- B60C 2011/0033: {Thickness of the tread}
- B60C 2200/04: for road vehicles, e.g. passenger cars
- C08F 2500/32: Glass transition temperature [Tg]
- C08G 2261/11: Homopolymers
- C08G 2261/132: branched or hyperbranched
- C08G 2261/216: Cis-trans isomerism
- C08G 2261/3321: derived from cyclopentene
- C08G 2261/418: Ring opening metathesis polymerisation [ROMP]
- C08G 2261/60: Glass transition temperature
- C08G 2261/63: Viscosity
- C08G 2261/76: crosslinking
- Y02T 10/86: Optimisation of rolling resistance, e.g. weight reduction
- B60C: VEHICLE TYRES; TYRE INFLATION; TYRE CHANGING; CONNECTING VALVES TO INFLATABLE ELASTIC BODIES IN GENERAL; DEVICES OR ARRANGEMENTS RELATED TO TYRES
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

A rubber compound suitable for passenger tires may comprise: 40 to 70 parts by weight per hundred parts by weight rubber (phr) of a long chain branched cyclopentene ring-opening rubber (LCB-CPR) having a glass transition temperature (Tg) of −120° C. to −80° C., a g′vis of 0.50 to 0.91, and a ratio of cis to trans of 40:60 to 5:95, 30 phr to 60 phr of a styrene-butadiene rubber (SBR), wherein the SBR has a glass transition temperature (Tg) of −60° C. to −5° C., 50 phr to 110 phr of a reinforcing filler, and 20 phr to 50 phr of a process oil.

## Claims

### Claim 1

A rubber compound for passenger tires comprising:
40 to 70 parts by weight per hundred parts by weight rubber (phr) of a long chain branched cyclopentene ring-opening rubber (LCB-CPR) having a glass transition temperature (Tg) of −120° C. to −80° C., a g′vis of 0.50 to 0.91, and a ratio of cis to trans of 40:60 to 5:95,
30 phr to 60 phr of a styrene-butadiene rubber (SBR), wherein the SBR has a glass transition temperature (Tg) of −60° C. to −5° C.,
50 phr to 110 phr of a reinforcing filler, and
20 phr to 50 phr of a process oil.

### Claim 2 (depends on 1)

The rubber compound of claim 1, wherein the LCB-CPR has a weight average molecular weight (Mw) of 1 kDa to 1,000 kDa.

### Claim 3 (depends on 1)

The rubber compound of claim 1, wherein the LCB-CPR has a melting temperature of 10° C. to 20° C.

### Claim 4 (depends on 1)

The rubber compound of claim 1, wherein the long chain branched cyclopentene ring-opening rubber (CPR) has an Mw divided by Mn of 1 to 10.

### Claim 5 (depends on 1)

The rubber compound of claim 1, wherein the SBR has a Mooney viscosity (ML(1+4) at 100° C.) of 40 MU to 50 MU.

### Claim 6 (depends on 1)

The rubber compound of claim 1, wherein the reinforcing filler comprises carbon black, silica, or a mixture thereof.

### Claim 7 (depends on 1)

The rubber compound of claim 1, wherein the rubber compound has a cross-linking density (MH-ML) after curing at 160° C., 0.5° for 45 minutes of 10 dN.M to 25 dN.M.

### Claim 8 (depends on 1)

The rubber compound of claim 1, wherein the rubber compound has a wet skid resistance (tan δ at −8° C., strain at 0.20%) of 0.1 to 0.7.

### Claim 9 (depends on 1)

The rubber compound of claim 1, wherein the rubber compound has a wear loss (tan δ at 60° C., strain at 2.0%) of 0.1 to 0.45.

### Claim 10 (depends on 1)

The rubber compound of claim 1, wherein the rubber compound has a tire handling (G′ at 60° C., strain at 2.0%) of 4 MPa to 10 MPa.

### Claim 11 (depends on 1)

The rubber compound of claim 1, wherein the rubber compound has a DIN abrasion volume loss of 40 mm3 to 130 mm3.

### Claim 12 (depends on 1)

The rubber compound of claim 1 further comprising:
0.1 phr to 15 phr of a vulcanizing agent and/or a crosslinking agent, wherein optionally the rubber compound is at least partially crosslinked.

### Claim 13

A method comprising:
compounding: 40 to 70 parts by weight per hundred parts by weight rubber (phr) of a long chain branched cyclopentene ring-opening rubber (LCB-CPR) having a glass transition temperature (Tg) of −120° C. to −80° C., a g′vis of 0.50 to 0.91, and a ratio of cis-to-trans of 40:60 to 5:95; 30 phr to 60 phr of a styrene-butadiene rubber (SBR), wherein the SBR has a glass transition temperature (Tg) of −60° C. to −5° C.; 50 phr to 110 phr of a reinforcing filler; and 20 phr to 50 phr of a process oil to form a rubber compound.

### Claim 14 (depends on 13)

The method of claim 13, wherein the rubber compound further comprises 0.1 phr to 15 phr of a vulcanizing agent and/or a crosslinking agent, and wherein the method further comprises:
at least partially crosslinking the rubber compound.

### Claim 15 (depends on 13)

The method of claim 13 further comprising:
molding the rubber compound into a passenger tire tread, wherein the tire tread has a depth of 15/32 of an inch or less.

### Claim 16

A passenger tire tread comprising: a rubber compound that comprises:
40 to 70 parts by weight per hundred parts by weight rubber (phr) of a cyclopentene ring-opening rubber (CPR) having a glass transition temperature (Tg) of −120° C. to −80° C., and a ratio of cis to trans of 40:60 to 5:95,
30 phr to 60 phr of a styrene-butadiene rubber (SBR), wherein the SBR has a glass transition temperature (Tg) of −60° C. to −5° C.,
50 phr to 110 phr of a reinforcing filler, and
20 phr to 50 phr of a process oil.

### Claim 17 (depends on 16)

The passenger tire tread of claim 16, wherein the rubber compound is at least partially crosslinked.

### Claim 18 (depends on 16)

The passenger tire tread of claim 16, wherein the tire tread has a depth of 15/32 of an inch or less.

### Claim 19 (depends on 16)

The passenger tire tread of claim 16, wherein the rubber compound is at least partially crosslinked and has a depth of 15/32 of an inch or less.