# US 2023/0128739 A1 · Cmp process applied to a thin sic wafer for stress release and damage recovery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0128739 A1
- Document ID: US20230128739A1
- Status: Published application
- Kind: A1
- Application number: 17/962,090
- Filed: 2022-10-07
- Published: 2023-04-27
- Earliest claimed: 2021-10-26
- Assignees: STMicroelectronics S.r.l.
- Applicants: STMICROELECTRONICS S.r.l.
- Inventors: Agata GRASSO; Nicolo' PILUSO; Andrea SEVERINO; Brunella CAFRA
- Web page: https://patentgrep.com/patent/US20230128739A1

## CPC

- B24B 37/102: {the workpieces or work carriers being able to rotate freely due to a frictional contact with the lapping tool}
- H10P 52/402: {of semiconductor materials}
- B24B 37/015: Temperature control
- B24B 37/044: {characterised by the composition of the lapping agent}
- B24B 37/30: for single side lapping of plane surfaces
- H10P 90/123: {by grinding or lapping}
- H10P 90/124: {by processing the backside of the wafers}
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A Chemical Mechanical Polishing, CMP, process applied to a wafer of Silicon Carbide having a thickness of, or lower than, 200 μm, comprising the steps of: arranging the wafer on a supporting head of a CMP processing apparatus, the wafer having a front side and a back side opposite to one another, the front side housing at least one electronic component and being coupled to the supporting head; deliver a polishing slurry on the wafer, wherein the polishing slurry has a pH in the range 2-3; pressing the back side of the wafer against a polishing pad of the CMP apparatus exerting, by the supporting head, a pressure on the polishing pad in the range 5-20 kPa; setting a rotation of the polishing pad in the range 30-180 rpm, and setting a rotation of polishing head in the range 30-180 rpm; setting and maintaining a CMP process temperature equal to, or below, 50° C.

## Claims

### Claim 1

A method of executing a chemical mechanical polishing (CMP) process on a wafer of silicon carbide, comprising:
arranging the wafer on a supporting head of a CMP processing apparatus, the wafer having a front side and a back side opposite to one another, the front side housing at least one electronic component and being coupled to the supporting head;
delivering a polishing slurry on the wafer, wherein the polishing slurry has a pH value in a range between 2 and 3;
pressing the back side of the wafer against a polishing pad of the CMP apparatus by exerting, via the supporting head, a pressure on the polishing pad in a range between 5 kPa and 20 kPa;
setting a rotation speed of the polishing pad in a range between 30 rpm and 180 rpm, and setting a rotation speed of the polishing head in a range between 30 rpm and 180 rpm; and
setting and maintaining a CMP process temperature equal to or below 50° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein the flow rate of the polishing slurry is less than 100 ml/min.

### Claim 3 (depends on 1)

The method of claim 1, wherein the polishing slurry is alumina-based.

### Claim 4 (depends on 1)

The method of claim 1, wherein the CMP process is executed until a thickness of between 1 μm and 3 μm of material is removed from the back side of the wafer.

### Claim 5 (depends on 1)

The method of claim 1, wherein a direction of rotation of the polishing pad is set to be a same as a direction of rotation of the supporting head.

### Claim 6 (depends on 1)

The method of claim 1, wherein the rotation speed of the polishing pad is set in a range between 30 and 70 rpm, and the rotation speed of the polishing head is set in a range between 30 and 60 rpm.

### Claim 7

A chemical mechanical polishing (CMP) method, comprising:
pressing a surface of a silicon carbide wafer against a polishing pad; and
polishing the surface of the silicon carbide wafer by rotating the polishing pad with a polishing slurry and a polishing temperature,
wherein:
the polishing slurry has a pH value in a range between 2 and 3;
a pressure on the polishing pad is in a range between 5 kPa and 20 kPa;
a speed of the rotating the polishing pad is in a range between 30 rpm and 180 rpm; and
the polishing temperature is equal to or below than 50° C.

### Claim 8 (depends on 7)

The CMP method of claim 7, comprising rotating the silicon carbide wafer with a rotation speed in a range between 30 rpm and 180 rpm.

### Claim 9 (depends on 7)

The CMP method of claim 7, wherein the polishing slurry is delivered with a flow rate less than 100 ml/min.

### Claim 10 (depends on 7)

The CMP method of claim 7, wherein the polishing slurry is alumina-based.

### Claim 11 (depends on 7)

The CMP method of claim 7, wherein the polishing is executed until a thickness between 1 and 3 μm of material is removed from the surface of the silicon carbide wafer.

### Claim 12 (depends on 8)

The CMP method of claim 8, wherein a direction of rotation of the polishing pad is set to be a same as a direction of rotation of the silicon carbide wafer.

### Claim 13 (depends on 8)

The CMP method of claim 8, wherein a direction of rotation of the polishing pad is set to be opposite to a direction of rotation of the silicon carbide wafer.

### Claim 14 (depends on 8)

The CMP method of claim 8, wherein the rotation speed of the polishing pad is set in a range between 30 rpm and 70 rpm, and the rotation speed of the polishing head is set in a range between 30 rpm and 60 rpm.

### Claim 15

A method of executing a chemical mechanical polishing (CMP) process on a wafer of silicon carbide, comprising:
arranging the wafer on a supporting head of a CMP processing apparatus, the wafer having a front side and a back side opposite to one another, the front side housing at least one electronic component and being coupled to the supporting head;
delivering a polishing slurry on the wafer, the polishing slurry having a pH value in a range between 2 and 3;
pressing the back side of the wafer against a polishing pad of the CMP apparatus with a pressure on the polishing pad in a range between 5 kPa and 20 kPa;
setting a rotation speed of the polishing pad in a range between 30 rpm and 70 rpm, and setting a rotation speed of the polishing head in a range between 30 rpm and 60 rpm;
setting and maintaining a CMP process temperature in a range between 24° C. and 50° C.

### Claim 16 (depends on 15)

The method of claim 15, wherein the flow rate of the polishing slurry is less than 100 ml/min.

### Claim 17 (depends on 15)

The method of claim 15, wherein the polishing slurry is alumina-based.

### Claim 18 (depends on 15)

The method of claim 15, wherein the CMP process is executed until a thickness of between 1 μm and 3 μm of material is removed from the back side of the wafer.

### Claim 19 (depends on 15)

The method of claim 15, wherein a direction of rotation of the polishing pad is set to be a same as a direction of rotation of the supporting head.

### Claim 20 (depends on 15)

The method of claim 15, wherein a removal rate of the CMP process is set to be equal to or higher than 10 μm/hr.