# US 2023/0118309 A1 · Perovskite Optical Element and Manufacturing Method Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0118309 A1
- Document ID: US20230118309A1
- Status: Published application
- Kind: A1
- Application number: 17/547,434
- Filed: 2021-12-10
- Published: 2023-04-20
- Earliest claimed: 2021-10-14
- Assignees: National Dong Hwa University
- Applicants: National Dong Hwa University
- Inventors: DUC-HUY NGUYEN; JIA-YUAN SUN; CHIA-YAO LO; JIA-MING LIU; WAN-SHAO TSAI; MING-HUNG LI; SIN-JHANG YANG; CHENG-CHIA LIN; SHIEN-DER TZENG; YUAN-RON MA; MING-YI LIN; CHIEN-CHIH LAI
- Web page: https://patentgrep.com/patent/US20230118309A1

## CPC

- G02B 6/02395: {Glass optical fibre with a protective coating, e.g. two layer polymer coating deposited directly on a silica cladding surface during fibre manufacture (G02B6/02052, G02B6/02057, G02B6/024, G02B6/032, G02B6/105, G02B6/14 take precedence; coating on fibre gratings G02B6/02104; multilayer core or cladding G02B6/036; reinforcing splice joints G02B6/2558; optical cables, i.e. comprising protective structures external to the protective coating such as a jacket or plural coated optical fibres G02B6/44; coating of glass to obtain optical fibres C03C25/104)}
- H10K 50/182: {OLED comprising a fiber structure}
- C03C 25/105: Organic claddings
- C03C 25/328: Polyamides
- C03C 25/42: Coatings containing inorganic materials
- C03C 25/47: containing particles, fibres or flakes, e.g. in a continuous phase
- H10K 50/852: comprising a resonant cavity structure, e.g. Bragg reflector pair
- H10K 85/50: Organic perovskites; Hybrid organic-inorganic perovskites [HOIP], e.g. CH3NH3PbI3
- C03C 2218/111: by dipping, immersion
- H10K 50/844: Encapsulations
- Y02E 10/549: Organic PV cells
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A perovskite optical element includes a light guiding unit and a luminescent layer. The light guiding unit is configured to conduct light and serves as a resonant cavity. The luminescent layer is a thin film made of perovskite material and clads the light guiding unit. The luminescent layer is configured to be excited by an excitation module to emit light. The light is conducted and output by the light guiding unit. A manufacturing method of a perovskite optical element includes preparing a dip coating solution; dipping a single crystal optical fiber in the dip coating solution for one hour, removing the single crystal optical fiber out of the dip coating solution, and drying the single crystal optical fiber; and placing the single crystal optical fiber into a tube furnace, heating the crystal optical fiber, and introducing synthetic molecules into the tube furnace.

## Claims

### Claim 1

A perovskite optical element comprising:
a light guiding unit configured to conduct light and serve as a resonant cavity; and
a luminescent layer which is a thin film made of perovskite material and which dads the light guiding unit, wherein the luminescent layer is configured to be excited by an excitation module to emit light, and wherein the light is conducted and output by the light guiding unit.

### Claim 2 (depends on 1)

The perovskite optical element as claimed in claim 1, wherein the light guiding unit is a column structure of a section of a single crystal optical fiber, wherein the luminescent layer dads an outer periphery of the light guiding unit, and wherein a cross section of each of two ends of the light guiding unit is configured to connect with a light source or to output the light.

### Claim 3 (depends on 1)

The perovskite optical element as claimed in claim 1, wherein the perovskite material of the luminescent layer is methylammonium lead iodide.

### Claim 4 (depends on 1)

The perovskite optical element as claimed in claim 1, further comprising a protective layer covering an outer surface of the luminescent layer.

### Claim 5 (depends on 1)

The perovskite optical element as claimed in claim 1, wherein the excitation module is a pulse laser which emits a laser light entering the luminescent layer at an arbitrary angle.

### Claim 6 (depends on 1)

The perovskite optical element as claimed in claim 1, wherein the excitation module is a voltage source having an anode and a cathode, and wherein the anode and the cathode are in electrical connection with the luminescent layer.

### Claim 7

A manufacturing method of a perovskite optical element, comprising:
preparing a dip coating solution;
dipping a single crystal optical fiber in the dip coating solution for one hour, removing the single crystal optical fiber out of the dip coating solution, and drying the single crystal optical fiber; and
placing the single crystal optical fiber into a tube furnace, heating the crystal optical fiber, and introducing synthetic molecules into the tube furnace.

### Claim 8 (depends on 7)

The manufacturing method of the perovskite optical element as claimed in claim 7, wherein the dip coating solution is obtained from dissolving lead iodide in dimethylformamide, wherein lead iodide crystals are formed on an outer surface of the single crystal optical fiber, wherein the synthetic molecules are methylammonium iodide, and wherein the lead iodide crystals on the single crystal optical fiber synthesize with the synthetic molecules after heating, forming a thin film of methylammonium lead iodide.

### Claim 9 (depends on 7)

The manufacturing method of the perovskite optical element as claimed in claim 7, wherein two ends of the tube furnace are sealed and an intermediate portion of the tube furnace is heated, and wherein an inert gas and the synthetic molecules are introduced into an interior space of the tube furnace.

### Claim 10 (depends on 9)

The manufacturing method of the perovskite optical element as claimed in claim 9, wherein after the single crystal optical fiber is placed into the tube furnace, the tube furnace is evacuated to a pressure range of 0.01-5 Torr, and the tube furnace is then gradually heated to a temperature range of 100-130° C., wherein the inert gas is filled into the tube furnace simultaneously to increase the pressure to 5-20 Torr, wherein the synthetic molecules are added to proceed with a reaction, and during the reaction, the tube furnace is maintained at the temperature range of 100-130° C. and the pressure range of 0.01-5 Torr for 1-5 hours.