# US 2023/0118131 A1 · Low temperature carbon/bn/aluminum oxide coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0118131 A1
- Document ID: US20230118131A1
- Status: Published application
- Kind: A1
- Application number: 18/079,350
- Filed: 2022-12-12
- Published: 2023-04-20
- Earliest claimed: 2019-12-20
- Assignees: Richter Precision, Inc.
- Applicants: Richter Precision Inc.
- Inventors: Aghasi TOROSYAN; Hans E. RICHTER; Bikram S. KAMBOJ
- Web page: https://patentgrep.com/patent/US20230118131A1

## CPC

- C04B 35/583: based on boron nitride
- C04B 35/62222: {obtaining ceramic coatings (coating of mortars, concrete, artificial or natural stone or ceramics C04B41/45; laminated ceramic products B32B18/00; coating of glass C03C17/00, applying ceramic coatings on silicon for semi-conductor purposes H10W; coating metallic materials C23)}
- C04B 35/62635: {Mixing details}
- C04B 35/6264: {Mixing media, e.g. organic solvents}
- C23C 24/02: by application of pressure only
- C23C 24/04: Impact or kinetic deposition of particles
- C23C 24/045: {by trembling using impacting inert media}
- C23C 26/00: Coating not provided for in groups C23C2/00 - C23C24/00
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/386: Boron nitrides
- C04B 2235/425: Graphite
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/606: Drying
- C04B 2235/95: Products characterised by their size, e.g. microceramics
- C04B 2235/9669: Resistance against chemicals, e.g. against molten glass or molten salts
- C23C 24/00: Coating starting from inorganic powder (spraying of the coating material in molten state C23C4/00; solid state diffusion C23C8/00 - C23C12/00)
- F41A 21/22: Barrels which have undergone surface treatment, e.g. phosphating {(F41A21/44 takes precedence)}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- F41A: FUNCTIONAL FEATURES OR DETAILS COMMON TO BOTH SMALLARMS AND ORDNANCE, e.g. CANNONS; MOUNTINGS FOR SMALLARMS OR ORDNANCE

## Abstract

A method of forming an activated coating composition is disclosed. The method includes providing (a) boron nitride, (b) carbon, (c) aluminum oxide and (d) a liquid carrier. Each of the boron nitride, carbon and aluminum oxide are in particulate form. The coating composition is activated to form an activated coating composition. The activated coating composition includes active components having from about 60.0 wt% to about 90.0 wt% boron nitride, from about 16 wt% to about 24 wt% carbon and from about 4 wt% to about 6 wt% aluminum oxide. A coating method, coated substrate and activated coating composition are also disclosed.

## Claims

### Claim 1

A method of forming a coating composition, comprising:
providing (a) boron nitride, (b) carbon, (c) aluminum oxide and (d) a liquid carrier, each of the boron nitride, carbon and aluminum oxide being in particulate form; and
activating the coating composition to form an activated coating composition;
wherein the activated coating composition includes active components (a), (b) and (c) having from about 60.0 wt% to about 90.0 wt% boron nitride, from about 16 wt% to about 24 wt% carbon and from about 4 wt% to about 6 wt% aluminum oxide and forms a coating upon contact with a substrate.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the activating includes exposing the coating composition to a mechanical agitation.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the activating includes exposing the coating composition to a mechanical agitation including vibrating the coating composition.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the vibrating of the coating composition includes vibrating at a frequency from about 1 Hz to about 300 Hz.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the boron nitride includes hexagonal boron nitride.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the boron nitride has a particle size of from 0.1 to 50 micrometers.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the carbon includes graphite.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the graphite has a particle size of from 0.1 to 50 micrometers.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the aluminum oxide is devoid of forms of other than corundum.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the aluminum oxide has a particle size of from 0.1 to 50 micrometers.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the carrier includes toluene or ammonia.

### Claim 12 (depends on 1)

The method of claim 1, wherein the coating composition includes active components having from about 70.0 wt% to about 80.0 wt% boron nitride, from about 18 wt% to about 22 wt% carbon and from about 4.5 wt% to about 5.5 wt% aluminum oxide.

### Claim 13 (depends on 1)

The method of claim 1, wherein the coating composition includes (a) boron nitride, (b) carbon and (c) aluminum oxide in weight ratios (a):(b):(c) of from about 14 to about 18: from about 1 to about 8: from 0.3 to about 1.7.

### Claim 14

A method of coating a substrate, comprising:
providing an activated coating composition (a) boron nitride, (b) carbon and (c) aluminum oxide in (d) a liquid carrier; and
contacting a substrate surface at a low temperature with the activated coating composition to form a coated substrate;
wherein the activated coating composition includes active components (a), (b) and (c) having from about 60.0 wt% to about 90.0 wt% boron nitride, from about 16 wt% to about 24 wt% carbon and from about 4 wt% to about 6 wt% aluminum oxide.

### Claim 15 (depends on 14)

The method of claim 14, wherein the contacting includes applying the activated coating composition and drying the surface to form the coated substrate.

### Claim 16 (depends on 14)

The method of claim 14, wherein the contacting includes applying the activated coating composition and exposing the applied coating composition to a mechanical agitation to form the coated substrate.

### Claim 17 (depends on 14)

A coating formed from the process of claim 14, the coating having a coefficient of friction of 0.1 or less and a wear resistance having a distance to failure of greater than 500 meters.

### Claim 18 (depends on 14)

The coating according to claim 14, wherein the coating has a coating thickness of from about 0.1 to about 2.0 microns.

### Claim 19 (depends on 14)

The coating according to claim 14, wherein the coating includes a hardness of at least about 750 HV.

### Claim 20

An activated coating composition comprising (a) boron nitride, (b) carbon, (c) aluminum oxide and (d) a liquid carrier, wherein the activate composition has been activated with mechanical energy;
wherein the activated coating composition includes active components having from about 60.0 wt% to about 90.0 wt% boron nitride, from about 16 wt% to about 24 wt% carbon and from about 4 wt% to about 6 wt% aluminum oxide and forms a coating upon contact with a substrate.

### Claim 21 (depends on 20)

The activated coating composition accordingly to claim 20, wherein (a) is hexagonal boron nitride (h-BN), (b) is graphite and (c) aluminum oxide (Al2O3) in a liquid carrier.

### Claim 22 (depends on 20)

The activated coating composition according to claim 20, wherein the liquid carrier includes toluene or ammonia.