# US 2023/0114065 A1 · Process for the preparation of polyacrylamides using an eco-friendly lubricant composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0114065 A1
- Document ID: US20230114065A1
- Status: Published application
- Kind: A1
- Application number: 17/906,941
- Filed: 2021-03-23
- Published: 2023-04-13
- Earliest claimed: 2020-04-01
- Assignees: S.P.C.M. SA
- Applicants: Spcm SA
- Inventors: Cédrick FAVERO; Thierry BESSENET; Frédéric DAGUERRE; Jing LING; Nicolas BOISSE
- Web page: https://patentgrep.com/patent/US20230114065A1

## CPC

- C08F 2/004: {by a prior coating on the reactor walls}
- C08F 220/56: Acrylamide; Methacrylamide
- C08F 220/34: Esters containing nitrogen {, e.g. N,N-dimethylaminoethyl (meth)acrylate}
- C08J 3/122: {Pulverisation by spraying}
- C10M 105/34: of monocarboxylic acids
- C10M 105/40: containing free hydroxy or carboxyl groups
- C10M 107/48: containing phosphorus
- C10M 111/04: at least one of them being a macromolecular organic compound
- C08J 2333/26: Homopolymers or copolymers of acrylamide or methacrylamide
- C10M 2207/2815: used as base material
- C10M 2207/2835: used as base material
- C10M 2225/0405: used as base material
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C10M: LUBRICATING COMPOSITIONS (well drilling compositions C09K8/02); USE OF CHEMICAL SUBSTANCES EITHER ALONE OR AS LUBRICATING INGREDIENTS IN A LUBRICATING COMPOSITION (mould release, i.e. separating, agents for metals B22C3/00, for plastics or substances in a plastic state, in general B29C33/56, for glass C03B40/02; textile lubricating compositions D06M11/00, D06M13/00, D06M15/00; immersion oils for microscopy G02B21/33)

## Abstract

Process for preparing water-soluble polymers in powder form by polymerization of water-soluble monoethylenically unsaturated monomers comprising the successive steps: a) Spraying on the inner wall of a polymerization vessel, the lubricant composition LC1: alkyl oleate/polyoxyethylene oleyl ether phosphate/sorbitan monolaurate, b) Polymerizing in aqueous solution in the presence of polymerization initiators at least one water-soluble monounsaturated ethylenic monomer, c) Discharging the polymer gel, d) Granulating the polymer gel thus obtained in a granulator, in presence of a lubricant composition LC2: alkyl oleate/polyxoyethylene oleyl ether phosphate/sorbitan monol aurate, e) Drying the polymer gel to obtain a polymer in powder form, f) Grinding and sifting the powder.

## Claims

### Claim 1

Process for preparing water-soluble polymers in powder form by polymerization of water-soluble monoethylenically unsaturated monomers comprising the successive steps:
a) Spraying on the inner wall of the polymerization vessel the lubricant composition LC1: alkyl oleate (25-40 weight %)/polyoxyethylene oleyl ether phosphate (50-65 weight %)/sorbitan monolaurate (5-15 weight %),
b) Polymerizing in aqueous solution, in the polymerization vessel, in the presence of polymerization initiators at an initiation temperature between −20° C. and 50° C., at least one water-soluble monounsaturated ethylenic monomer, the total mass concentration of monomer relative to the polymerization charge being between 10 and 60%,
c) Discharging the polymer gel from the polymerisation vessel,
d) Granulating the polymer gel thus obtained in a granulator, in presence of a lubricant composition LC2: alkyl oleate (15-35 weight %)/polyoxyethylene oleyl ether phosphate (15-45 weight %)/sorbitan monolaurate (35-55 weight %),
e) Drying the polymer gel to obtain a polymer in powder form,
f) Grinding and sifting the powder.

### Claim 2 (depends on 1)

Process for preparing water-soluble polymers in powder form according to claim 1 wherein water-soluble monoethylenically unsaturated monomers are nonionic and/or anionic and/or cationic:
Non-ionic monomers are selected from the group comprising acrylamide; methacrylamide; N-mono derivatives of acrylamide; N-mono derivatives of methacrylamide; N,N derivatives of acrylamide; N,N derivatives of methacrylamide; acrylic esters; and methacrylic esters, preferably acrylamide,
Anionic monomers are selected from the group comprising monomers having a carboxylic function and salts thereof including acrylic acid, methacrylic acid, itaconic acid; maleic acid, monomers having a sulfonic acid function and salts thereof; including acrylamide tertio butyl sulfonic acid (ATBS), monomers having a phosphonic acid function and salts thereof, preferably: acrylic acid, acrylamide tertio butyl sulfonic acid.
Cationic monomers are selected from the group comprising dimethylaminoethyl acrylate (DMAEA) quaternized or salified; dimethylaminoethyl methacrylate (DMAEMA) quaternized or salified; diallyldimethyl ammonium chloride (DADMAC); acrylamidopropyltrimethylammonium chloride (APTAC); methacrylamidopropyltrimethylammonium chloride (MAPTAC).

### Claim 3 (depends on 1)

Process for preparing water-soluble polymers in powder form according to claims 1 wherein the alkyloleate of lubricant compositions LC1 and/or LC2, is selected form the group: methyl oleate, ethyl oleate, propyl oleate;
isopropyl oleate, butyl oleate, isobutyl oleate, amyl oleate, ethylhexyl oleate.

### Claim 4 (depends on 1)

Process for preparing water-soluble polymers in powder form according to claim 1 wherein the polyoxyethylene group of the polyxoyethylene oleyl ether phosphate of lubricant compositions LC1 and/or LC2, contains between 2 and 50 oxyethylene moieties.

### Claim 5 (depends on 1)

Process for preparing water-soluble polymers in powder form according to claim 1 wherein in step a) of the process 0.01 to 0.8 weight % of the lubricant composition LC1 is sprayed based on the weight of the polymerization charge.

### Claim 6 (depends on 1)

Process for preparing water-soluble polymers in powder form according to claim 1 wherein in step d) of the process 0.01 to 1.2 weight % of the lubricant composition LC2 based on the weight of the polymerization charge is sprayed on the polymer in the cutting chamber of the granulator.

### Claim 7

(canceled)

### Claim 8 (depends on 2)

The process for preparing water-soluble polymers in powder form according to claim 2 wherein the water-soluble monoethylenically unsaturated monomers comprise anionic monomers selected from acrylic acid, acrylamide tertio butyl sulfonic acid (ATBS), and alkaline or alkaline earth or ammonium salts thereof

### Claim 9 (depends on 2)

Process for preparing water-soluble polymers in powder form according to claim 2 wherein the alkyloleate of lubricant compositions LC1 and/or LC2, is selected form the group: methyl oleate, ethyl oleate, propyl oleate; isopropyl oleate, butyl oleate, isobutyl oleate, amyl oleate, ethylhexyl oleate.

### Claim 10 (depends on 2)

Process for preparing water-soluble polymers in powder form according to claim 2 wherein the polyoxyethylene group of the polyxoyethylene oleyl ether phosphate of lubricant compositions LC1 and/or LC2, contains between 2 and 50 oxyethylene moieties.

### Claim 11 (depends on 3)

Process for preparing water-soluble polymers in powder form according to claim 3 wherein the polyoxyethylene group of the polyxoyethylene oleyl ether phosphate of lubricant compositions LC1 and/or LC2, contains between 2 and 50 oxyethylene moieties.

### Claim 12 (depends on 8)

Process for preparing water-soluble polymers in powder form according to claim 8 wherein the polyoxyethylene group of the polyxoyethylene oleyl ether phosphate of lubricant compositions LC1 and/or LC2, contains between 2 and 50 oxyethylene moieties.

### Claim 13 (depends on 9)

Process for preparing water-soluble polymers in powder form according to claim 9 wherein the polyoxyethylene group of the polyxoyethylene oleyl ether phosphate of lubricant compositions LC1 and/or LC2, contains between 2 and 50 oxyethylene moieties.

### Claim 14 (depends on 2)

Process for preparing water-soluble polymers in powder form according to claim 2 wherein in step a) of the process 0.01 to 0.8 weight % of the lubricant composition LC1 is sprayed based on the weight of the polymerization charge.

### Claim 15 (depends on 3)

Process for preparing water-soluble polymers in powder form according to claim 3 wherein in step a) of the process 0.01 to 0.8 weight % of the lubricant composition LC1 is sprayed based on the weight of the polymerization charge.

### Claim 16 (depends on 4)

Process for preparing water-soluble polymers in powder form according to claim 4 wherein in step a) of the process 0.01 to 0.8 weight % of the lubricant composition LC1 is sprayed based on the weight of the polymerization charge.

### Claim 17 (depends on 8)

Process for preparing water-soluble polymers in powder form according to claim 8 wherein in step a) of the process 0.01 to 0.8 weight % of the lubricant composition LC1 is sprayed based on the weight of the polymerization charge.

### Claim 18 (depends on 2)

Process for preparing water-soluble polymers in powder form according to claim 2 wherein in step d) of the process 0.01 to 1.2 weight % of the lubricant composition LC2 based on the weight of the polymerization charge is sprayed on the polymer in the cutting chamber of the granulator.

### Claim 19 (depends on 3)

Process for preparing water-soluble polymers in powder form according to claim 3 wherein in step d) of the process 0.01 to 1.2 weight % of the lubricant composition LC2 based on the weight of the polymerization charge is sprayed on the polymer in the cutting chamber of the granulator.

### Claim 20 (depends on 4)

Process for preparing water-soluble polymers in powder form according to claim 4 wherein in step d) of the process 0.01 to 1.2 weight % of the lubricant composition LC2 based on the weight of the polymerization charge is sprayed on the polymer in the cutting chamber of the granulator.

### Claim 21 (depends on 5)

Process for preparing water-soluble polymers in powder form according to claim 5 wherein in step d) of the process 0.01 to 1.2 weight % of the lubricant composition LC2 based on the weight of the polymerization charge is sprayed on the polymer in the cutting chamber of the granulator.