# US 2023/0110950 A1 · Method for recycling coal liquefaction residue

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0110950 A1
- Document ID: US20230110950A1
- Status: Published application
- Kind: A1
- Application number: 17/806,914
- Filed: 2022-06-14
- Published: 2023-04-13
- Earliest claimed: 2021-10-13
- Assignees: University of Science and Technology Beijing
- Applicants: University of Science and Technology Beijing
- Inventors: Haibin Zuo; Yajie Wang
- Web page: https://patentgrep.com/patent/US20230110950A1

## CPC

- C10L 5/48: on industrial residues and waste materials {(C10L5/403, C10L5/406 take precedence)}
- C04B 33/04: Clay; Kaolin
- C04B 33/132: Waste materials; Refuse {; Residues} (C04B33/16 takes precedence)
- C04B 33/1355: {Incineration residues}
- C04B 33/32: Burning methods
- C04B 35/62695: {Granulation or pelletising (devices for shaping artificial aggregates from ceramic mixtures B28B1/004)}
- C10L 5/08: without the aid of extraneous binders
- C10L 5/361: {Briquettes}
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/349: Clays, e.g. bentonites, smectites such as montmorillonite, vermiculites or kaolines, e.g. illite, talc or sepiolite
- C04B 2235/447: Phosphates or phosphites, e.g. orthophosphate or hypophosphite
- C04B 2235/604: Pressing at temperatures other than sintering temperatures
- C04B 2235/6567: Treatment time
- C04B 2235/661: Multi-step sintering
- C04B 2235/781: Nanograined materials, i.e. having grain sizes below 100 nm
- C04B 2235/785: Submicron sized grains, i.e. from 0,1 to 1 micron
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- C10L 2270/08: for small applications, such as tools, lamp oil, welding
- C10L 2290/06: Heat exchange, direct or indirect
- C10L 2290/10: Recycling of a stream within the process or apparatus to reuse elsewhere therein
- C10L 2290/24: Mixing, stirring of fuel components
- C10L 2290/28: Cutting, disintegrating, shredding or grinding
- C10L 2290/30: Pressing, compressing or compacting
- C10L 2290/32: Molding or moulds
- C10L 2290/543: Distillation, fractionation or rectification for separating fractions, components or impurities during preparation or upgrading of a fuel
- Y02P 40/60: Production of ceramic materials or ceramic elements, e.g. substitution of clay or shale by alternative raw materials, e.g. ashes
- C10L: FUELS NOT OTHERWISE PROVIDED FOR; NATURAL GAS; SYNTHETIC NATURAL GAS OBTAINED BY PROCESSES NOT COVERED BY SUBCLASSES C10G OR C10K; LIQUIFIED PETROLEUM GAS; USE OF ADDITIVES TO FUELS OR FIRES; FIRE-LIGHTERS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed is a method for recycling a coal liquefaction residue. The method includes S1, drying a coal liquefaction residue and pulverizing to obtain a pulverized coal liquefaction residue; S2, subjecting the pulverized coal liquefaction residue to a solvothermal extraction in an autoclave to obtain an extract liquid and a residue; S3, distilling the extract liquid and recovering an organic solvent to obtain a solid extract.

## Claims

### Claim 1

A method for recycling a coal liquefaction residue, comprising:
drying a coal liquefaction residue and pulverizing the dried coal liquefaction residue to obtain a pulverized coal liquefaction residue, the coal liquefaction residue comprising a waste product generated by a direct coal liquefaction process;
subjecting the pulverized coal liquefaction residue to a solvothermal extraction in an autoclave to obtain an extract liquid and a residue; and
distilling the extract liquid and recovering an organic solvent to obtain a solid extract.

### Claim at position 2

2-10. (canceled)

### Claim 11 (depends on 1)

The method as claimed in claim 1, further comprising:
preparing a hot-pressed coal briquette using the solid extract as a binder; and
preparing a ceramsite using the residue obtained after subjecting the pulverized coal liquefaction residue to a solvothermal extraction in an autoclave as a raw material.

### Claim 12 (depends on 1)

The method as claimed in claim 1, wherein a solvent for the solvothermal extraction is N-methylpyrrolidone, and the solvothermal extraction is conducted at a temperature of 300-400° C. for 0.5-1.5 h.

### Claim 13 (depends on 1)

The method as claimed in claim 1, wherein the coal liquefaction residue is dried at a temperature of 80-120° C. and pulverized to a particle size of less than or equal to 0.2 mm.

### Claim 14 (depends on 1)

The method as claimed in claim 1, wherein the distilling is conducted at a temperature of 80-110° C. and a vacuum degree of less than or equal to 0.05 Mpa.

### Claim 15 (depends on 11)

The method as claimed in claim 11, wherein the preparation of the hot-pressed coal briquette comprises:
mixing amounts of the solid extract and raw coal to obtain a first mixture;
delivering the first mixture into a hot-pressing mold;
placing the hot-pressing mold in a high-temperature furnace;
heating the hot-pressing mold, and subjecting the first mixture to heat preservation and hot-pressing molding at a set pressure; and
cooling the hot-pressing mold to room temperature to obtain the hot-pressed coal briquette.

### Claim 16 (depends on 15)

The method as claimed in claim 15, wherein a weight ratio value of the solid extract to the raw coal is in the range of 5-25%, and the hot-pressing molding is conducted at a temperature of 250-500° C., and the heat preservation is conducted for 10-60 min.

### Claim 17 (depends on 15)

The method as claimed in claim 15, wherein the raw coal is selected from the group consisting of bituminous coal and anthracite.

### Claim 18 (depends on 11)

The method as claimed in claim 11, wherein the preparation of the ceramsite comprises:
mixing alumina, bentonite and the residue obtained after subjecting the pulverized coal liquefaction residue to a solvothermal extraction in an autoclave to obtain a second mixture; and
subjecting the second mixture to a granulation, a pre-heating, and a high-temperature sintering to obtain a finished ceramsite product.

### Claim 19 (depends on 18)

The method as claimed in claim 18, wherein the pre-heating is conducted at a temperature of 400-600° C. for 10-30 min, and the high-temperature sintering is conducted at a temperature of 900-1,200° C. for 10-60 min.