# US 2023/0089728 A1 · Polyphenylene ether resin modified with benzoxazine, method for producing the same, and substrate material for circuit board

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0089728 A1
- Document ID: US20230089728A1
- Status: Published application
- Kind: A1
- Application number: 17/871,982
- Filed: 2022-07-24
- Published: 2023-03-23
- Earliest claimed: 2021-09-13
- Assignees: Nan Ya Plastics Corporation
- Applicants: Nan Ya Plastics Corporation
- Inventors: TE-CHAO LIAO; HUNG-YI CHANG; YU-TING LIU; CHIEN-KAI WEI; Chi-Lin Chen
- Web page: https://patentgrep.com/patent/US20230089728A1

## CPC

- C08G 65/485: {Polyphenylene oxides}
- C08K 5/357: Six-membered rings
- C08G 2650/04: End-capping
- C08G 2650/12: Depolymerisation, e.g. to reform the monomer
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A polyphenylene ether resin modified with benzoxazine, a method for producing the same, and a substrate material for a circuit board are provided. The polyphenylene ether resin modified with the benzoxazine has a structural formula as follows: in which R represents a chemical group that is located between two hydroxyphenyl functional groups of a bisphenol compound, and n is an integer between 3 and 25, inclusive.

## Claims

### Claim 1

A method for producing a polyphenylene ether resin, comprising:
providing a high molecular mass polyphenylene ether resin material that has a first number average molecular mass;
performing a cracking process which includes: cracking the high molecular mass polyphenylene ether resin material to form a low molecular mass polyphenylene ether resin material that has a second number average molecular mass and is modified with a bisphenol functional group, wherein the second number average molecular mass is less than the first number average molecular mass;
performing a nitration process which includes: carrying out a nitration reaction of the low molecular mass polyphenylene ether resin material, so that two ends of a polymer chain of the low molecular mass polyphenylene ether resin material are respectively modified with two nitro functional groups;
performing a hydrogenation process which includes: carrying out a hydrogenation reaction of the low molecular mass polyphenylene ether resin material that contains the polymer chain having the two ends respectively modified with the two nitro functional groups, so as to form a low molecular mass polyphenylene ether resin material that contains a polymer chain having two ends respectively modified with two amino functional groups; and
performing a cyclization process which includes: carrying out a cyclization reaction of the low molecular mass polyphenylene ether resin material, which contains the polymer chain having the two ends respectively modified with the two amino functional groups, with a phenol material and a polyoxymethylene material, so that a low molecular mass polyphenylene ether resin material that contains a polymer chain having two ends respectively modified with benzoxazine (BX) is formed and has a structural formula as follows:
wherein R represents a chemical group that is located between two hydroxyphenyl functional groups of a bisphenol compound, and n is an integer between 3 and 25, inclusive.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the first number average molecular mass (Mn) of the high molecular mass polyphenylene ether resin material is not less than 18,000, and the second number average molecular mass of the low molecular mass polyphenylene ether resin material is not greater than 12,000.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the cracking process includes: reacting the bisphenol compound with the high molecular mass polyphenylene ether resin material having the first number average molecular mass in a presence of peroxide, so that the high molecular mass polyphenylene ether resin material is cracked to form the low molecular mass polyphenylene ether resin material having the second number average molecular mass, and wherein a side of the polymer chain of the low molecular mass polyphenylene ether resin material is modified with the bisphenol functional group.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the bisphenol compound is at least one material selected from a group consisting of 4,4′-biphenol, bisphenol A, bisphenol B, bisphenol S, bisphenol fluorene, 4,4′-ethylene bisphenol, 4,4′-dihydroxydiphenylmethane, 3,5,3′,5′-tetramethyl-4,4′-dihydroxybiphenyl, and 2,2-bis (4-hydroxy-3,5-dimethylphenyl) propane, and wherein a material type of the peroxide is at least one selected from a group consisting of azobisisobutyronitrile, benzyl peroxide, and dicumyl peroxide.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the nitration process includes: carrying out the nitration reaction of a 4-halonitrobenzene material with the low molecular mass polyphenylene ether resin material that is cracked and modified with the bisphenol functional group in an alkaline environment, so that the two ends of the polymer chain of the low molecular mass polyphenylene ether resin material are respectively modified with the two nitro functional groups.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the nitration process allows the nitration reaction of the low molecular mass polyphenylene ether resin material to be carried out in the alkaline environment, the alkaline environment having a pH value between 8 and 14.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the hydrogenation process includes: carrying out the hydrogenation reaction of a hydrogenation solvent with the low molecular mass polyphenylene ether resin material that contains the polymer chain having the two ends respectively modified with the two nitro functional groups, and wherein a material type of the hydrogenation solvent is at least one material selected from a group consisting of dimethylacetamide, tetrahydrofuran, toluene, and isopropanol.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the hydrogenation solvent is prepared by mixing 80 to 100 parts by weight of the dimethylacetamide, the tetrahydrofuran or the toluene with 0 to 20 parts by weight of the isopropanol.

### Claim 9 (depends on 1)

The method according to claim 1, wherein in the cyclization process, the cyclization reaction is carried out in an environment of a cyclization solvent, and the cyclization solvent is at least one material selected from a group consisting of toluene and ethanol.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the cyclization solvent is prepared by mixing 60 to 100 parts by weight of the toluene with 0 to 40 parts by weight of the ethanol.

### Claim 11

A polyphenylene ether resin modified with benzoxazine, which is suitable for use as a substrate material for a circuit board, comprising a structural formula as follows:
wherein R represents a chemical group that is located between two hydroxyphenyl functional groups of a bisphenol compound, and n is an integer between 3 and 25, inclusive.

### Claim 12 (depends on 11)

A substrate material for a circuit board, comprising at least 20 wt % of the polyphenylene ether resin modified with the benzoxazine as claimed in claim 11, wherein the substrate material for the circuit board has a dielectric constant (Dk) that is between 3.5 and 4.0, a dielectric dissipation factor (Df) that is between 0.002 and 0.01, and a glass transition temperature that is not less than 230° C.