# US 2023/0086290 A1 · Graphene reinforced aluminum matrix composite with high electrical conductivity and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0086290 A1
- Document ID: US20230086290A1
- Status: Published application
- Kind: A1
- Application number: 17/843,235
- Filed: 2022-06-17
- Published: 2023-03-23
- Earliest claimed: 2021-08-11
- Assignees: Wuhan Research Institute of Materials Protection
- Applicants: Wuhan Research Institute of Materials Protection
- Inventors: Haitao Duan; Yinhua Li; Jiesong Tu; Jian Li; Xingeng Li; Zhibin Fan; Dan Jia; Shengpeng Zhan; Tian Yang; Yunhu Ding; Lixin Ma
- Web page: https://patentgrep.com/patent/US20230086290A1

## CPC

- C23C 18/31: Coating with metals
- C23C 18/1639: {Substrates other than metallic, e.g. inorganic or organic or non-conductive}
- C23C 18/1691: {Cooling, e g. forced or controlled cooling}
- C23C 18/1692: {Heat-treatment}
- C23C 18/52: using reducing agents for coating with metallic material not provided for in a single one of groups C23C18/32 - C23C18/50
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A graphene reinforced aluminum matrix composite with high electrical conductivity and a preparation method thereof. The method includes: obtaining aluminum coated graphene powder by plating aluminum on a graphene surface, melting aluminum block into aluminum liquid, heating a mold to be lower than an aluminum melting point, alternately pouring the aluminum liquid and the aluminum coated graphene powder into the mold for layered casting to obtain a sandwich structure; extruding the sandwich structure into a rectangular test block and then heating to 500˜600° C., performing heat preservation for a preset time and performing forging treatment, and performing longitudinal cold deformation under inert gas to obtain the graphene reinforced aluminum matrix composite. The method can solve a problem that poor wettability of graphene and aluminum matrix, the graphene is evenly dispersed in the aluminum matrix, which can improve strength of the aluminum matrix and keep its high electrical conductivity.

## Claims

### Claim 1

A preparation method of a graphene reinforced aluminum matrix composite, comprising:
preparation of raw materials, comprising: drying graphene, aluminum powder and aluminum block in a drying oven to remove moisture;
obtaining aluminum coated graphene powder by plating the aluminum powder on a surface of the graphene through electroless plating;
melting the aluminum block into aluminum liquid in a crucible furnace and injecting first inert gas for protection;
heating a forming device to a temperature lower than a melting point of aluminum;
alternately pouring the aluminum liquid into the forming mold of the forming device to form an aluminum liquid solidification layer and laying a layer of the aluminum coated graphene powder on the aluminum liquid solidification layer to form an aluminum coated graphene powder layer until the forming mold is fully filled, thereby forming a sandwich structure with a first layer and a last layer both being the aluminum liquid solidification layers;
extruding the sandwich structure into a rectangular test block by using a press;
heating the rectangular test block to a temperature in a range of 500° C. to 600° C. in a heating furnace and performing heat preservation for a preset time, and performing forging treatment on the rectangular test block to obtain a forged rectangular test block;
after cooling the forged rectangular test block to room temperature, performing longitudinal cold deformation on the forged rectangular test block to obtain a deformed rectangular test block; and
performing annealing treatment on the deformed rectangular test block under a protection of second inert gas to obtain the graphene reinforced aluminum matrix composite.

### Claim 2 (depends on 1)

The preparation method of the graphene reinforced aluminum matrix composite according to claim 1, wherein the plating the aluminum powder on a surface of the graphene through electroless plating, comprises:
after the graphene is coarsened, sensitized and activated, plating the aluminum powder on the surface of the graphene through the electroless plating in an aluminum liquid at room temperature.

### Claim 3 (depends on 1)

The preparation method of the graphene reinforced aluminum matrix composite according to claim 1, wherein a heating temperature of the crucible furnace is in a range of 700° C. to 800° C.

### Claim 4 (depends on 1)

The preparation method of the graphene reinforced aluminum matrix composite according to claim 1, wherein each of the first inert gas and the second inert gas is one of argon gas and helium gas.

### Claim 5 (depends on 1)

The preparation method of the graphene reinforced aluminum matrix composite according to claim 1, wherein a heating temperature of the forming device is in a range of 250° C. to 350° C.

### Claim 6 (depends on 1)

The preparation method of the graphene reinforced aluminum matrix composite according to claim 1, wherein a number of the aluminum coated graphene powder layer of the sandwich structure is greater than or equal to 2, content of the aluminum coated graphene powder layers are evenly distributed according to a total content, a thickness of the aluminum coated graphene powder layer is less than 10 μm, and a thickness of the aluminum liquid solidification layer is less than 3 mm.

### Claim 7 (depends on 1)

The preparation method of the graphene reinforced aluminum matrix composite according to claim 1, wherein the preset time is in a range of 25 min to 35 min, and a forging direction of the forging treatment is crisscross.

### Claim 8 (depends on 1)

The preparation method of the graphene reinforced aluminum matrix composite according to claim 1, wherein a deformation amount of the longitudinal cold deformation of the forged rectangular test block is in a range of 40% to 60%.

### Claim 9 (depends on 1)

The preparation method of the graphene reinforced aluminum matrix composite according to claim 1, wherein a temperature of the annealing treatment is in a range of 200° C. to 300° C., and a time in a furnace during the annealing treatment is in a range of 30 min to 60 min.

### Claim 10 (depends on 1)

A graphene reinforced aluminum matrix composite, prepared by the preparation method according to claim 1.

### Claim 11 (depends on 10)

The graphene reinforced aluminum matrix composite according to claim 10, wherein the plating the aluminum powder on a surface of the graphene through electroless plating, comprises:
after the graphene is coarsened, sensitized and activated, plating the aluminum powder on the surface of the graphene through the electroless plating in an aluminum liquid at room temperature.

### Claim 12 (depends on 10)

The graphene reinforced aluminum matrix composite according to claim 10, wherein a heating temperature of the crucible furnace is in a range of 700° C. to 800° C.

### Claim 13 (depends on 10)

The graphene reinforced aluminum matrix composite according to claim 10, wherein each of the first inert gas and the second inert gas is one of argon gas and helium gas.

### Claim 14 (depends on 10)

The graphene reinforced aluminum matrix composite according to claim 10, wherein a heating temperature of the forming device is in a range of 250° C. to 350° C.

### Claim 15 (depends on 10)

The graphene reinforced aluminum matrix composite according to claim 10, wherein a number of the aluminum coated graphene powder layer of the sandwich structure is greater than or equal to 2, content of the aluminum coated graphene powder layers are evenly distributed according to a total content, a thickness of the aluminum coated graphene powder layer is less than 10 μm, and a thickness of the aluminum liquid solidification layer is less than 3 mm.

### Claim 16 (depends on 10)

The graphene reinforced aluminum matrix composite according to claim 10, wherein the preset time is in a range of 25 min to 35 min, and a forging direction of the forging treatment is crisscross.

### Claim 17 (depends on 10)

The graphene reinforced aluminum matrix composite according to claim 10, wherein a deformation amount of the longitudinal cold deformation of the forged rectangular test block is in a range of 40% to 60%.

### Claim 18 (depends on 10)

The graphene reinforced aluminum matrix composite according to claim 10, wherein a temperature of the annealing treatment is in a range of 200° C. to 300° C., and a time in a furnace during the annealing treatment is in a range of 30 min to 60 min.