# US 2023/0074156 A1 · Magnesium alloy for wheel and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0074156 A1
- Document ID: US20230074156A1
- Status: Published application
- Kind: A1
- Application number: 17/576,239
- Filed: 2022-01-14
- Published: 2023-03-09
- Earliest claimed: 2021-09-03
- Assignees: CITIC Dicastal Co., Ltd.
- Applicants: CITIC Dicastal Co., Ltd.
- Inventors: Lixin Huang; Zuo Xu; Meng Li; Tieqiang Chen; Hanqi Wu; Qingzhu Zhang
- Web page: https://patentgrep.com/patent/US20230074156A1

## CPC

- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- B21J 1/06: Heating or cooling methods or arrangements specially adapted for performing forging or pressing operations {(B21J5/063 takes precedence)}
- B21K 1/40: hubs
- C22C 1/03: using master alloys
- C22C 23/02: with aluminium as the next major constituent
- C22F 1/06: of magnesium or alloys based thereon
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B21J: FORGING; HAMMERING; PRESSING METAL; RIVETING; FORGE FURNACES (rolling of metal B21B; making particular products by forging or pressing B21K; cladding or plating B23K; finishing surfaces by hammering B23P9/04; compacting surfaces by blasting with particulate material B24C1/10; general features of presses, presses for consolidating scrap B30B; furnaces in general F27)
- B21K: MAKING FORGED OR PRESSED METAL PRODUCTS, e.g. HORSE-SHOES, RIVETS, BOLTS OR WHEELS (making particular articles by working sheet metal without essentially removing material B21D; processing wire B21F; making pins, needles or nails B21G; making particular articles by rolling B21H; forging machines, pressing machines, hammering machines, in general B21J; making chains B21L; plating B23K)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

The disclosure discloses a magnesium alloy for wheels, comprising in mass percentage: Al: 2-3.0 wt. %; Zn: 0.5-1.0 wt. %; Mn: 0.3-0.5 wt. %; Ce: 0.15-0.3 wt. %; La: 0.05-0.1 wt. %, the balance is Mg. The magnesium alloy of the present invention takes Al element and Mn element as main alloying elements, supplemented by trace Ce and La elements as alloying process, and the nano-scale Mn-rich precipitated phase obtained during homogenization and the segregation of rare earth elements Ce and La at the interface and grain boundary of Mn-rich precipitated phase are used to inhibit the coarsening during extrusion and forging, so as to improve the strength and plastic deformation ability of the alloy.

## Claims

### Claim 1

A magnesium alloy for wheels, comprising the mass percentage of: Al: 2-3.0 wt. %; Zn: 0.5-1.0 wt. %; Mn: 0.3-0.5 wt. %; Ce: 0.15-0.3 wt. %; La: 0.05-0.1 wt. %, the balance is Mg.

### Claim 2 (depends on 1)

The magnesium alloy for wheels according to claim 1, further comprising unavoidable impurities.

### Claim 3 (depends on 1)

A method for preparing a magnesium alloy for wheels according to claim 1, wherein the method comprises the following steps:
(1) batching, in mass percentage: Al: 2-3.0 wt. %; Zn: 0.5-1.0 wt. %; Mn: 0.3-0.5 wt. %; Ce: 0.15-0.3 wt. %; La: 0.05-0.1 wt. %, the balance is Mg for batching;
(2) smelting, putting the pure Mg ingot into a crucible of a smelting furnace, setting the furnace temperature at 700-730° C. and keeping it, adding pure Al block and pure Zn block preheated to 50-80° C. into the magnesium solution after melting, then raising the smelting temperature to 760° C., and adding the Al—Mn master alloy, Mg—Ce—La master alloy and Mg—Ce master alloy preheated to 50-80° C. into the magnesium solution respectively; then raising the smelting temperature to 780° C., keeping the temperature for 5-15 minutes, then stirring for 3-10 minutes, introducing high-purity Ar gas for refining and degassing, adjusting and controlling temperature at 710° C.-730° C., and keeping the temperature for 2-10 minutes;
(3) pouring, the pouring temperature is controlled above 680° C.;
(4) stress relief treatment, keeping the temperature at 280-320° C. for 8-12h, and then air cooling;
(5) extruding and deforming, heating the stress-relieved magnesium alloy to 250-380° C. within 30 minutes, then putting the magnesium alloy into a die for deformation processing; the extrusion speed being 1 m/min-8 m/min, and air cooling after deformation processing.

### Claim 4 (depends on 3)

The method for preparing a magnesium alloy for wheels according to claim 3, wherein the smelting process is carried out under the protection of a mixed gas of CO2 and SF6.

### Claim 5 (depends on 3)

The method for preparing a magnesium alloy for wheels according to claim 3, wherein after the smelting is completed, the surface scum needs to be removed and pour the solution into a die to obtain the magnesium alloy.

### Claim 6 (depends on 3)

The method for preparing a magnesium alloy for wheels according to claim 3, wherein, after the stress relief treatment, the process of cutting into blanks and peeling is also included before extrusion.

### Claim 7 (depends on 3)

The method for preparing a magnesium alloy for wheels according to claim 3, wherein the stirring in the smelting process comprises mechanical stirring and/or argon stirring.

### Claim 8 (depends on 3)

The method for preparing a magnesium alloy for wheels according to claim 3, wherein the Al—Mn master alloy is an Al-20Mn master alloy, the Mg—Ce—La master alloy is a Mg-15Ce-10La master alloy, and the Mg—Ce master alloy is a Mg-30Ce master alloy.

### Claim 9 (depends on 4)

The method for preparing a magnesium alloy for wheels according to claim 4, wherein the composition volume ratio of a mixed gas of CO2 and SF6 is 50-100:1.