# US 2023/0069378 A1 · Optimized core particles for optical fiber preform and optical fiber preform thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0069378 A1
- Document ID: US20230069378A1
- Status: Published application
- Kind: A1
- Application number: 17/553,133
- Filed: 2021-12-16
- Published: 2023-03-02
- Earliest claimed: 2021-08-27
- Assignees: Sterlite Technologies Limited
- Applicants: Sterlite Technologies Limited
- Inventors: Nivedita Prasad; Chandan Saha
- Web page: https://patentgrep.com/patent/US20230069378A1

## CPC

- C03B 37/01282: {by pressing or sintering, e.g. hot-pressing}
- G02B 6/02: Optical fibres with cladding {with or without a coating}
- C03B 37/01205: {starting from tubes, rods, fibres or filaments (C03B37/014 takes precedence)}
- C03B 37/01248: {by collapsing without drawing}
- C03B 37/01268: {by casting}
- C03B 37/02763: {Fibres having axial variations, e.g. axially varying diameter, material or optical properties (rotational spin C03B37/02745)}
- C03C 13/046: {Multicomponent glass compositions}
- C03C 25/1061: {Inorganic coatings}
- C03B 2201/12: doped with fluorine (C03B2201/14 takes precedence)
- C03B 2201/32: doped with aluminium (C03B2201/36 takes precedence)
- C03B 2201/54: doped with beryllium, magnesium or alkaline earth metals
- C03C 2213/00: Glass fibres or filaments
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method for manufacturing of an optical fibre preform (100) using optimized core particles includes optimization of particles of calcium aluminum silicate powder (104), utilizing the optimized core particles, sintering the optimized core particles inside a fluorine doped glass tube (106) and drawing of an optical fibre. Particularly, the optimization of the particles of calcium aluminum silicate powder (104) facilitates formation of the optimized core particles and the optimized core particles are filled inside the fluorine doped glass tube (106). Moreover, sintering of the optimized core particles solidifies and adheres smoothly with the fluorine doped glass tube (106) for manufacturing of the optical fibre preform (100).

## Claims

### Claim 1

A method for manufacturing of an optical fibre preform using an optimized core particles comprising steps of:
optimization of particles of calcium aluminum silicate powder, wherein the optimization of the particles of calcium aluminum silicate powder facilitates formation of the optimized core particles;
utilizing the optimized core particles, wherein the optimized core particles are filled inside a fluorine doped glass tube, wherein the optimized core particles inside the fluorine doped glass tube facilitates manufacturing of the optical fibre preform;
sintering the optimized core particles inside the fluorine doped glass tube, wherein sintering solidifies the optimized core particles and adheres smoothly with the fluorine doped glass tube for manufacturing of the optical fibre preform; and
drawing an optical fibre, wherein the optical fibre is drawn by pulling the optical fibre preform.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the particles of calcium aluminum silicate powder forms a core section of the optical fibre preform.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the fluorine doped glass tube forms a cladding section of the optical fibre preform.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the optimized core particles has size in a range of about 30 microns to 50 microns.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the core section is characterized by low attenuation of about 0.1 decibel per kilometer.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein the optical fibre preform is manufactured by a powder-in-cylinder technique.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the powder-in-cylinder technique facilitates the optical fibre preform to form a plurality of solid preform rods of small diameter.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein sintering of the fluorine doped glass tube with the optimized core particles is performed at a temperature in range of about 1500 degree Celsius to 1600 degree Celsius.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the optimized core particles enables drawing of the optical fibre from the optical fibre preform with low transmission loss.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the fluorine doped glass tube has low viscosity.

### Claim 11

An optical fibre preform using optimized core particles comprising:
a core section defined along a longitudinal axis; and a cladding section circumferentially surrounding the core section.

### Claim 12 (depends on 11)

The optical fibre preform as claimed in claim 11, wherein the core section is formed by particles of calcium aluminum silicate powder.

### Claim 13 (depends on 11)

The optical fibre preform as claimed in claim 11, wherein the cladding section is formed by a fluorine doped glass tube.

### Claim 14 (depends on 11)

The optical fibre preform as claimed in claim 11, wherein a refractive index of the core section is greater than the refractive index of cladding section.

### Claim 15 (depends on 12)

The optical fibre preform as claimed in claim 12, wherein the particles of calcium aluminum silicate powder are optimized to facilitate formation of the optimized core particles.

### Claim 16 (depends on 15)

The optical fibre preform as claimed in claim 15, wherein size of the optimized core particles is in the range of about 30 microns to 50 microns.

### Claim 17 (depends on 15)

The optical fibre preform as claimed in claim 15, wherein the optimized core particles is performed at a temperature in range of about 1500 degree Celsius to 1600 degree Celsius.

### Claim 18 (depends on 11)

The optical fibre preform as claimed in claim 11, wherein the core section is characterized by low attenuation of about 0.1 decibel per kilometer.

### Claim 19 (depends on 11)

The optical fibre preform as claimed in claim 11, wherein the optical fibre preform is manufactured by using powder-in-cylinder technique.

### Claim 20 (depends on 19)

The optical fibre preform as claimed in claim 19, wherein the powder-in-cylinder technique facilitates the optical fibre preform to form a plurality of solid preform rods of small diameter.