# US 2023/0069187 A1 · High-k gate dielectric and method forming same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0069187 A1
- Document ID: US20230069187A1
- Status: Published application
- Kind: A1
- Application number: 17/412,967
- Filed: 2021-08-26
- Published: 2023-03-02
- Earliest claimed: 2021-08-26
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Cheng-Hao Hou; Che-Hao Chang; Da-Yuan Lee; Chi On Chui
- Web page: https://patentgrep.com/patent/US20230069187A1

## CPC

- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 84/0177: {the gate conductors having different materials or different implants}
- H10D 84/0181: {Manufacturing their gate insulating layers}
- H10D 84/83135: {the IGFETs characterised by having different gate conductor materials or different gate conductor implants}
- H10D 84/8314: {the IGFETs characterised by having gate insulating layers with different properties}
- H10D 84/85: Complementary IGFETs, e.g. CMOS
- H10D 84/853: {comprising FinFETs}
- H10D 84/0193: {the components including FinFETs}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method includes depositing a first high-k dielectric layer over a first semiconductor region, performing a first annealing process on the first high-k dielectric layer, depositing a second high-k dielectric layer over the first high-k dielectric layer; and performing a second annealing process on the first high-k dielectric layer and the second high-k dielectric layer.

## Claims

### Claim 1

A method for forming a gate electrode, the method comprising:
depositing a first high-k dielectric layer over a first semiconductor region;
performing a first annealing process on the first high-k dielectric layer;
depositing a second high-k dielectric layer over the first high-k dielectric layer; and
performing a second annealing process on the first high-k dielectric layer and the second high-k dielectric layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein a first thickness of the first high-k dielectric layer is larger than a second thickness of the second high-k dielectric layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first annealing process and the second annealing process are the same.

### Claim 4 (depends on 3)

The method of claim 3, wherein during the performing the first annealing process and the second annealing process the temperature is ramped up to a first temperature that is in a range from 1000° C. to 1150° C.

### Claim 5 (depends on 4)

The method of claim 4, wherein during the performing the first annealing process and the second annealing process the first temperature is maintained for a duration from 1 ms to 30 ms.

### Claim 6 (depends on 1)

The method of claim 1, wherein after performing the first annealing process and the second annealing process the first high-k dielectric layer and the second high-k dielectric layer have a combined crystallinity that is higher than 70 percent.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first annealing process and the second annealing process are performed in an ambient environment that comprises nitrogen, argon, or a mixture thereof.

### Claim 8 (depends on 1)

The method of claim 1 further comprising:
depositing a first work function tuning layer over the second high-k dielectric layer;
selectively removing the first work function tuning layer from over a first, a third, and a fourth portion of the first semiconductor region;
depositing a second work function tuning layer over the first work function tuning layer and the second high-k dielectric layer;
selectively removing the second work function tuning layer from over the first, a second, and the third portion of the first semiconductor region;
depositing a third work function tuning layer over the first work function tuning layer, the second work function tuning layer, and the second high-k dielectric layer;
selectively removing the third work function tuning layer from over the first and the second portion of the first semiconductor region; and
depositing a fourth work function tuning layer over the first work function tuning layer, the third work function tuning layer, and the second high-k dielectric layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the first work function tuning layer comprises an n-type layer and the second work function tuning layer, the third work function tuning layer and the fourth work function tuning layer comprises a p-type layer.

### Claim 10

A method for forming a gate electrode, the method comprising:
depositing a first high-k dielectric layer over a first semiconductor region;
performing a first annealing process on the first high-k dielectric layer;
depositing a second high-k dielectric layer over the first high-k dielectric layer;
performing a second annealing process on the first high-k dielectric layer and the second high-k dielectric layer, wherein after the second annealing process the combined crystallinity of the first high-k dielectric layer and the second high-k dielectric layer is higher than 70 percent.

### Claim 11 (depends on 10)

The method of claim 10, wherein each of the first annealing process and the second annealing process comprise a preheat at a temperature that is in a range from 400° C. to 750° C.

### Claim 12 (depends on 10)

The method of claim 10, wherein the first annealing process and the second annealing process are microsecond anneals (μSSA).

### Claim 13 (depends on 10)

The method of claim 10, wherein during the first annealing process and the second annealing process the temperature is ramped up to a maximum temperature that is in a range from about 1000° C. to about 1150° C.

### Claim 14 (depends on 13)

The method of claim 13, wherein during the first annealing process and the second annealing process the maximum temperature is maintained for a duration that is in a range from 1 ms to 30 ms.

### Claim 15 (depends on 10)

The method of claim 10, wherein after each of the first annealing process and the second annealing process, a post heat temperature is maintained that is in a range from 500° C. to 700° C.

### Claim 16

A device comprising:
a first gate electrode, the first gate electrode comprising:
a first high-k dielectric layer;
a first p-type work function tuning metal contacting the first high-k dielectric layer; and
a first conductive material over the first p-type work function tuning metal; and
a second gate electrode, the second gate electrode comprising:
a second high-k dielectric layer;
a first n-type work function tuning metal contacting the second high-k dielectric layer;
a second p-type work function tuning metal contacting the first n-type work function tuning metal; and
a second conductive material over the second p-type work function tuning metal, wherein the crystallinity of the first high-k dielectric layer and the second high-k dielectric layer is higher than 70 percent.

### Claim 17 (depends on 16)

The device of claim 16 further comprising a third gate electrode, the third gate electrode comprising:
a third high-k dielectric layer;
a third p-type work function tuning metal contacting the third high-k dielectric layer;
a fourth p-type work function tuning metal contacting the third p-type work function tuning metal; and
a third conductive material over the fourth p-type work function tuning metal.

### Claim 18 (depends on 17)

The device of claim 17, wherein the first, the second, the third, and the fourth p-type work function tuning metal comprises the same material.

### Claim 19 (depends on 18)

The device of claim 18, wherein the first, the second, the third, and the fourth p-type work function tuning metal comprises titanium nitride and the first n-type work function tuning metal comprises titanium aluminum nitride.

### Claim 20 (depends on 19)

The device of claim 19, wherein a combined thickness of the third p-type work function tuning metal and the fourth p-type work function tuning metal is larger than a thickness of the first p-type work function tuning metal.