# US 2023/0069145 A1 · Plant leaves-derived carbon material doped with two metals and preparation and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0069145 A1
- Document ID: US20230069145A1
- Status: Published application
- Kind: A1
- Application number: 17/811,221
- Filed: 2022-07-07
- Published: 2023-03-02
- Earliest claimed: 2021-08-25
- Assignees: Zhejiang University of Technology
- Applicants: Zhejiang University of Technology
- Inventors: Haimin Shen; Dong Lv
- Web page: https://patentgrep.com/patent/US20230069145A1

## CPC

- B01J 21/18: Carbon
- C07C 29/50: with molecular oxygen only
- B01J 23/06: of zinc, cadmium or mercury
- B01J 23/34: Manganese
- B01J 23/72: Copper
- B01J 23/745: Iron
- B01J 23/75: Cobalt
- B01J 23/755: Nickel
- B01J 37/0036: {Grinding}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/084: {Decomposition of carbon-containing compounds into carbon}
- C07C 27/12: with oxygen
- C07C 45/33: of CHx-moieties
- C07C 2521/18: Carbon
- C07C 2523/06: of zinc, cadmium or mercury
- C07C 2523/34: Manganese
- C07C 2523/72: Copper
- C07C 2523/745: Iron
- C07C 2523/75: Cobalt
- C07C 2523/755: Nickel
- C07C 2601/08: the ring being saturated
- C07C 2601/14: The ring being saturated
- C07C 2601/18: with a ring being at least seven-membered
- C07C 2601/20: the ring being twelve-membered
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

A plant leaves-derived carbon material doped with two metals and preparation and use thereof are provided, the carbon material prepared by carbonizing, in an inert atmosphere, plant leaves which have absorbed ions of two metals M1 and M2. The metal M1 is Co, Mn, or Fe. The metal M2 is Ni, Cu, or Zn. The carbon material can be used as an efficient, green, and safe catalyst for the selective oxidation of cycloalkanes to produce cycloalkanols and cycloalkanones, and enable an increased selectivity of the target products (thus less by-products), a low yield of cycloalkyl peroxides, reduced reaction temperature, low environmental impact, and safe production.

## Claims

### Claim 1

A plant leaves-derived carbon material doped with two metals, prepared by carbonizing, in an inert atmosphere, plant leaves which have absorbed ions of two metals M1 and M2,
wherein, the metal M1 is Co, Mn, or Fe, and the metal M2 is Ni, Cu, or Zn.

### Claim 2 (depends on 1)

A method for preparing the plant leaves-derived carbon material doped with two metals according to claim 1, the method comprising:
immersing a bottom of a branch with the plant leaves in an aqueous solution of metal salts of the metals M1 and M2 for a period of time, followed by removal of the leaves from the branch and washing with fresh water;
carbonizing the leaves in a nitrogen atmosphere, followed by cooling the carbonized leaves to room temperature and then grinding the carbonized leaves after being cooled to a powder; and
washing the powder by stirring the powder in a volume of a hydrochloric acid solution in order to remove inorganic salts therefrom, followed by suction filtration, washing until neutral with water, and drying.

### Claim 3 (depends on 2)

The method according to claim 2, wherein, the leaves are derived from at least one tree selected from the group consisting of Salix babylonica, Firmiana simplex, Magnolia denudata, Osmanthus, Viburnum odoratissimum, Ginkgo biloba, Populus L., and Metasequoia glyptostroboides.

### Claim 4 (depends on 2)

The method according to claim 2, wherein, M1 is Co (II), Mn (II), or Fe (II), and wherein, M2 is Ni (II), Cu (II), or Zn (II);
wherein, Co (II) is provided by any one of, or a mixture of any two or more at any ratio of, Co(CH3COO)2, Co(NO3)2, CoSO4, CoCl2, and their hydrates; Mn (II) is provided by any one of, or a mixture of any two or more at any ratio of, Mn(CH3COO)2, Mn(NO3)2, MnSO4, MnCl2, and their hydrates; Fe (II) is provided by any one of, or a mixture of any two or more at any ratio of, Fe(CH3COO)2, Fe(NO3)2, FeSO4, FeCl2, and their hydrates; Ni (II) is provided by any one of, or a mixture of any two or more at any ratio of, Ni(CH3COO)2, Ni(NO3)2, NiSO4, NiCl2, and their hydrates; Cu (II) is provided by any one of, or a mixture of any two or more at any ratio of, Cu(CH3COO)2, Cu(NO3)2, CuSO4, CuCl2, and their hydrates; and Zn (II) is provided by any one of, or a mixture of any two or more at any ratio of, Zn(CH3COO)2, Zn(NO3)2, ZnSO4, ZnCl2, and their hydrates.

### Claim 5 (depends on 2)

The method according to claim 2, wherein, the aqueous solution of metal salts of the metals M1 and M2 has a concentration of the salt of the metal M1 varying from 0.000001 to 0.001 mol/L, preferably 0.00001 to 0.001 mol/L, and a concentration of the salt of the metal M2 varying from 0.000001 to 0.001 mol/L, preferably 0.00001 to 0.001 mol/L.

### Claim 6 (depends on 2)

The method according to claim 2, wherein, the bottom of the branch with the plant leaves is immersed in the aqueous solution of metal salts of the metals M1 and M2 for 1.0 to 48.0 h, preferably 24.0 to 48.0 h; wherein, the leaves are carbonized at 300 to 1000° C. for 1.0 to 5.0 h; wherein, the hydrochloric acid solution used to wash the powder is at a concentration of 1.0 to 5.0 mol/L; and wherein, the powder is washed by stirring it in the hydrochloric acid solution for 4.0 to 12.0 h.

### Claim 7 (depends on 1)

Use of the plant leaves-derived carbon material doped with two metals according to claim 1 as a catalyst for the oxidation of a cycloalkane.

### Claim 8 (depends on 1, 7)

The use according to claim 7, comprising:
dispersing the carbon material according to claim 1 in the cycloalkane to form a mixture, followed by sealing;
heating the mixture with stirring to a reaction temperature, followed by introducing an oxidant thereinto and stirring for a period of time to allow an oxidation reaction to proceed; and
after completion of the reaction, cooling the reaction mixture to room temperature, followed by addition of triphenylphosphine and stirring at room temperature for 30 to 40 min to allow a peroxide formed during the oxidation reaction to be reduced.

### Claim 9 (depends on 8)

The use according to claim 8, wherein, the cycloalkane is any one of, or a mixture of any two or more at any ratio of, cyclopentane, cyclohexane, cycloheptane, cyclooctane, cyclononane, cyclodecane, and cyclododecane;
wherein, the oxidant is oxygen, air, or a mixture thereof at any ratio;
wherein, the oxidation reaction is conducted at a pressure of 0.1 to 2.0 MPa, preferably 0.5 to 2.0 MPa, and a temperature of 80 to 160° C., preferably 100 to 160° C., for 2.0 to 24.0 h, preferably 8.0 to 24.0 h, with a stirring speed of 600 to 1200 rpm;
and wherein, the ratio of the molar amount in mmol of the cycloalkane to the mass in mg of the carbon material is in a range of 5 to 20, preferably 8 to 12.

### Claim 10 (depends on 8)

The use according to claim 8, wherein, the triphenylphosphine is used in an amount of 2 to 4% by mole, with respect to the total amount of the cycloalkane.